Solid state amorphization and nanocrystallization of a Ti−50.0 Ni(at.%) alloy

被引:0
作者
Gyu-Bong Cho
Yeon-Ho Kim
Shin-Goo Hur
Cheol-Am Yu
Tae-Hyun Nam
机构
[1] Gyeongsang National University,Division of Materials Engineering and ERI
来源
Metals and Materials International | 2006年 / 12卷
关键词
Ti−Ni shape memory alloy; cold working; amorphous; crystallization; shear band;
D O I
暂无
中图分类号
学科分类号
摘要
Amorphization and crystallization behavior of an equiatomic Ti−Ni alloy have been investigated by means of differential scanning calorimetry, X-ray diffraction, optical microscopy and transmission electron microscopy. Amorphous phases were induced by cold working, and their morphologies changed from domain like shape to band shape with increasing the amount of cold working. Volume fraction of amorphous phase increased from 17 to 43% with increasing working ratio from 30 to 70%. With increasing the amount of cold rolling from 30 to 70%, the crystallization temperature increased from 552 to 539 K and enthalpy changes associated with crystallization increased from 170 to 447 J/mol. The average grain size of the 40% cold rolled alloy increased from 27 to 80 nm with increasing annealing temperature from 573 to 673 K.
引用
收藏
页码:173 / 179
页数:6
相关论文
共 50 条
  • [1] Grant D. M.(1995)undefined Acta metall. mater. 43 1045-1045
  • [2] Green S. M.(1992)undefined Mater. Sci. Forum. 88–90 75-75
  • [3] Wood J. V.(1990)undefined J. Mater. Res. 5 1414-1414
  • [4] Daroczi L.(2002)undefined Mat. Sci. Forum 386–388 597-597
  • [5] Beke D. L.(1998)undefined Met. Mater.-Int. 4 61-61
  • [6] Koike J.(1996)undefined Phil. Mag. Lett. 74 137-137
  • [7] Parkin D. M.(2005)undefined Smart Mater. Struct. 14 239-239
  • [8] Nastasi M.(1990)undefined Phil. Mag. Lett. 62 257-257
  • [9] Crone W. C.(2001)undefined Mater. Trans. 42 1987-1987
  • [10] Yahya A. N.(1997)undefined Acta mater. 45 2197-2197