Thermoelectric Properties of Zn Doped BiCuSeO

被引:0
作者
Sayan Das
Anbalagan Ramakrishnan
Moumin Rudra
Kuei-Hsien Chen
T. P. Sinha
Dinesh Kumar Misra
Ramesh Chandra Mallik
机构
[1] Indian Institute of Science,Thermoelectric Materials and Devices Laboratory, Department of Physics
[2] Institute of Atomic and Molecular Sciences,Department of Physics
[3] Academia Sinica,Advanced Materials and Devices
[4] Bose Institute,undefined
[5] CSIR-National Physical Laboratory,undefined
来源
Journal of Electronic Materials | 2019年 / 48卷
关键词
Seebeck coefficient; electrical resistivity; thermal conductivity; small polaron;
D O I
暂无
中图分类号
学科分类号
摘要
Layered oxychalcogenide BiCuSeO is a promising thermoelectric material due to its ultra-low thermal conductivity and moderate Seebeck coefficient. The doping of monovalent/divalent elements at the Bi site helps in reducing the electrical resistivity. In this report, Bi1−xZnxCuSeO (x = 0.0, 0.02, 0.04, 0.06, 0.08, and 0.1) was prepared by the solid state synthesis to elucidate the Zn doping effect at the Bi site. Zinc oxide was used as a precursor to dope Zn at the Bi site. The X-ray diffraction patterns were matched with BiCuSeO with no additional peak, which confirms the crystal structure and phase purity of the samples. X-ray photo electron spectroscopy of the Bi0.90Zn0.10CuSeO sample indicated a coexistence of Bi+3 and Bi+4 oxidation states. The electrical resistivity and Seebeck coefficient of the samples decreased with increase in the doping concentration because of increasing carrier concentration. The electrical resistivity of all the doped samples showed a transition from a metallic to semiconducting nature around 473 K. The Seebeck coefficient of the samples with x = 0.06, 0.08 and 0.1 showed a very weak temperature dependence above 523 K, which is a signature of small polaron hopping. The highest power factor of 0.35 mW/m K2 was obtained for x = 0.02 at 773 K. The impedance spectroscopy of the Bi0.90Zn0.10CuSeO sample confirmed the hopping conductivity and also the increase in the mobility of the charge carrier with temperature. The total thermal conductivity was dominated by the lattice thermal conductivity. The highest zT of 0.48 at 773 K has been obtained for x = 0.02, mainly due to the increment in the power factor.
引用
收藏
页码:3631 / 3642
页数:11
相关论文
共 245 条
  • [21] Kim J(2010)undefined Powder Technol. 203 243-undefined
  • [22] Cho S(2018)undefined J. Phys. D Appl. Phys. 51 35501-undefined
  • [23] Zhao LD(1993)undefined Phys. B Phys. Condens. Matter 192 55-undefined
  • [24] He J(2017)undefined Appl. Surf. Sci. 418 238-undefined
  • [25] Berardan D(1959)undefined J. Inorg. Nucl. Chem. 9 113-undefined
  • [26] Lin Y(2016)undefined Phys. Chem. Chem. Phys. 18 19158-undefined
  • [27] Li JF(2009)undefined Solid State Sci. 11 2065-undefined
  • [28] Nan CW(2016)undefined Acta Mater. 102 88-undefined
  • [29] Dragoe N(1995)undefined Chem. Phys. 191 321-undefined
  • [30] Lee C(1979)undefined Phys. Rev. B 20 2255-undefined