The formation of nanotubes and nanocoils of molybdenum disulphide

被引:29
|
作者
Lavayen, V.
Mirabal, N.
O'Dwyer, C. [1 ]
Ana, M. A. Santa
Benavente, E.
Torres, C. M. Sotomayor
Gonzalez, G.
机构
[1] Natl Univ Ireland Univ Coll Cork, Tyndall Natl Inst, Cork, Ireland
[2] Univ Chile, Fac Sci, Dept Chem, Santiago, Chile
[3] Univ Tecnol Metropolitana, Dept Chem, Santiago, Chile
基金
爱尔兰科学基金会;
关键词
chalcogenides; transmission electron microscopy; molybdenum; nanotubes nanostructures;
D O I
10.1016/j.apsusc.2006.12.019
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
This work reports the successful realization of MoS2 nanotubes by a novel intercalation chemistry and hydrothermal treatment. An inorganic-organic precursor of hexadecylamine (HDA) and molybdenum disulphide (MoS2) were used in synthesizing the nanocomposite comprising laminar MoS2 with HDA intercalated in the interlaminar spacing. The formation of MoS2 nanotubes occurred during hydrothermal treatment (HT) by a self-organized rolling mechanism. The nanotubes were observed to have dimensions 2-12 mu m in length and inner diameters typically in the range of 25-100 nm. We also report the formation of amorphous nanocoils of MoS2 obtained during similar procedures. (c) 2006 Elsevier B.V. All rights reserved.
引用
收藏
页码:5185 / 5190
页数:6
相关论文
共 50 条
  • [1] MOLYBDENUM DISULPHIDE DEPOSITS - THEIR FORMATION AND CHARACTERISTICS ON STEEL BALLS
    BLACK, AL
    DUNSTER, RW
    SANDERS, JV
    WEAR, 1966, 9 (06) : 462 - &
  • [2] The synthesis, structure and properties of single-wall molybdenum disulphide nanotubes
    Mihailovic, D
    Mrzel, A
    Remskar, M
    Demsar, J
    Ceh, M
    Skraba, Z
    Jesih, A
    ELECTRONIC PROPERTIES OF MOLECULAR NANOSTRUCTURES, 2001, 591 : 478 - 482
  • [3] MOLYBDENUM DISULPHIDE DEPOSITS - THEIR FORMATION AND CHARACTERISTICS ON AUTOMOTIVE ENGINE PARTS
    BLACK, AL
    DUNSTER, RW
    SANDERS, JV
    MCTAGGAR.FK
    WEAR, 1967, 10 (01) : 17 - &
  • [4] INFLUENCE OF SUBSTRATE HARDNESS ON FORMATION AND ENDURANCE OF MOLYBDENUM DISULPHIDE FILMS
    LANCASTER, JK
    WEAR, 1967, 10 (02) : 103 - +
  • [5] Amorphous carbon nanotubes-molybdenum disulphide: A potential material for energy storage
    Jain, Kritika
    Bhowmick, P.
    Das, B.
    Sarkar, J.
    Gain, A.
    Ghorai, U. K.
    Chattopadhyay, K. K.
    Banerjee, D.
    MATERIALS TODAY COMMUNICATIONS, 2022, 33
  • [6] MOLYBDENUM DISULPHIDE FOR TRACTORS
    不详
    INDUSTRIAL LUBRICATION AND TRIBOLOGY, 1969, 21 (01) : 18 - &
  • [7] Formation of Nanotubes and Nanocoils by Spontaneous Self-Rolling of Aluminum (001)/(111) Bilayer
    Jijun Lao
    Dorel Moldovan
    JOM, 2013, 65 : 168 - 174
  • [8] Formation of Nanotubes and Nanocoils by Spontaneous Self-Rolling of Aluminum (001)/(111) Bilayer
    Lao, Jijun
    Moldovan, Dorel
    JOM, 2013, 65 (02) : 168 - 174
  • [9] MOLYBDENUM DISULPHIDE IN METAL CUTTING
    CRUMP, WJJ
    INDUSTRIAL LUBRICATION AND TRIBOLOGY, 1971, 23 (02) : 67 - &
  • [10] Chemical diffusion in molybdenum disulphide
    Potoczek, M.
    Przybylski, K.
    Rekas, M.
    JOURNAL OF PHYSICS AND CHEMISTRY OF SOLIDS, 2007, 68 (04) : 564 - 569