Mechanical characterisation of carbon fibre-PEEK manufactured by laser-assisted automated-tape-placement and autoclave

被引:192
作者
Comer, A. J. [1 ]
Ray, D. [1 ]
Obande, W. O. [1 ]
Jones, D. [1 ]
Lyons, J. [1 ]
Rosca, I. [1 ]
O'Higgins, R. M. [1 ]
McCarthy, M. A. [1 ]
机构
[1] Univ Limerick, Mech Aeronaut & Biomed Engn Dept, MSSI, Irish Ctr Composites Res IComp, Limerick, Ireland
关键词
Automation; Thermoplastic resin; Carbon fibre; Mechanical properties; COOLING RATE INFLUENCES; THERMOPLASTIC COMPOSITES; FIBRE/PEEK COMPOSITES; FRACTURE-TOUGHNESS; WELD STRENGTH; CONSOLIDATION; CRYSTALLINITY; PARAMETERS;
D O I
10.1016/j.compositesa.2014.10.003
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Obtaining autoclave-level mechanical properties using in-situ consolidation of thermoplastic composites by Automated Tape Placement (ATP) is challenging. However, relatively recent availability of high quality ATP grade pre-preg material and tape heads equipped with more efficient heat sources (e.g. lasers) offers an opportunity to achieve improved mechanical properties and deposition rates. In the present study, carbon fibre-PEEK laminates, manufactured by laser-assisted ATP (LATP) and autoclave, are compared. Analysis of the through-thickness temperature distribution during LATP processing using thermocouples indicates that LATP cooling rates are extremely rapid and suggests full through-thickness melting of the pre-preg tape may not occur. Inadequate crystallinity, in conjunction with voids, compromised mechanical properties compared to autoclaved laminates but was beneficial in terms of the toughness of LATP laminates. Optimisation of pre-preg properties and processing parameters is required to realise the full potential of the LATP process in terms of mechanical properties, energy requirements, cost and deposition rates. (C) 2014 Elsevier Ltd. All rights reserved.
引用
收藏
页码:10 / 20
页数:11
相关论文
共 39 条
[1]  
[Anonymous], 1997, BRIT STAND AER SER
[2]  
ASTMD6484, 2015, STANDARD TEST METHOD
[3]  
Brecher C, 2010, JEC COMPOS MAG, P56
[4]  
Cano R.J., 2001, P STRUCT SPEC M
[5]  
Chen J, 2013, 1 INT S AUT COMP MAN
[6]   IMPROVED THERMOPLASTIC TAPE WINDING USING LASER OR DIRECT-FLAME HEATING [J].
FUNCK, R ;
NEITZEL, M .
COMPOSITES MANUFACTURING, 1995, 6 (3-4) :189-192
[7]   Cooling rate influences in carbon fibre/PEEK composites. Part II: interlaminar fracture toughness [J].
Gao, SL ;
Kim, JK .
COMPOSITES PART A-APPLIED SCIENCE AND MANUFACTURING, 2001, 32 (06) :763-774
[8]   Cooling rate influences in carbon fibre/PEEK composites. Part 1. Crystallinity and interface adhesion [J].
Gao, SL ;
Kim, JK .
COMPOSITES PART A-APPLIED SCIENCE AND MANUFACTURING, 2000, 31 (06) :517-530
[9]  
Grouve W., 2012, THESIS U TWENTE
[10]   On crystallisation and fracture toughness of poly(phenylene sulphide) under tape placement conditions [J].
Grouve, W. J. B. ;
Poel, G. Vanden ;
Warnet, L. L. ;
Akkerman, R. .
PLASTICS RUBBER AND COMPOSITES, 2013, 42 (07) :282-288