Washout resistance of self-protected underwater concrete in freshwater and seawater

被引:34
作者
Nasr, Ahmed A. [1 ]
Chen, Songgui [2 ]
Jin, Feng [1 ]
机构
[1] Tsinghua Univ, State Key Lab Hydrosci & Engn, Beijing 100084, Peoples R China
[2] Tianjin Res Inst Water & Transport Engn, Xingang 2nd Rd, Tianjin, Peoples R China
基金
中国国家自然科学基金;
关键词
Self-protected underwater concrete (SPUC); Underwater protective agent (UPA); Washout; pH value test; Freshwater & Seawater; Aggregate segregation; COMPACTING CONCRETE; RHEOLOGICAL PROPERTIES; BOND STRENGTH; SLUMP FLOW; SUPERPLASTICIZER; PERFORMANCE; DOSAGE; TIME;
D O I
10.1016/j.conbuildmat.2021.123186
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
In this paper, the washout resistance of an innovative self-protected underwater concrete (SPUC) was tested under the influence of an underwater protective agent (UPA) in freshwater and seawater during the static case of water flow. The pervious methods of underwater concrete have been carried performed by incorporating the anti-washout admixtures (AWAs) into the proportions of concrete mix in order to make the mixture coherent during the placing of underwater concrete, but the UPA technique depends on changing the characteristics of the water to make it suitable for receiving fresh self-compacted concrete (SCC) without leakage into water. An experimental program consisted of 20 mixes was conducted by using 4 tests: non-dispersion test (US Army Corp CRD C61), slump, and slump flow (SF), and pH value test to investigate the behavior of concrete during placing the concrete underwater. These experiments were implemented based on five parameters: UPA concentration, W/C ratio, superplasticizer (SP) content, fine aggregate (FA) ratio, and water environment. Test results showed that the washout was decreased by increasing the UPA concentration. Mass losses also were increased by increasing the W/C ratio or SP and decreased by increasing the fine aggregate ratio. Besides, seawater showed higher resistance to washout than freshwater. On the other hand, the pH test was shown to be compatible with the results of the CRD C61 test. However, freshwater specimens achieved higher pH values than seawater because freshwater was more alkaline. Furthermore, the relationship between D loss of mass and D pH tests was induced between UPA and UPA-free. Finally, it was concluded that the recommendations relating to the SPUC proportions should be concluded in the technical guideline on SPUC. (c) 2021 Elsevier Ltd. All rights reserved.
引用
收藏
页数:11
相关论文
共 40 条
[1]  
A.U.C.R. Committee, 1991, RECOMMENDATIONS DESI
[2]   Performance evaluation of asphalt concrete mixes under varying replacement percentages of natural sand [J].
Albayati, Amjad H. ;
Abdulsattar, Harith .
RESULTS IN ENGINEERING, 2020, 7
[3]   Mechanisms of strength loss in underwater concrete [J].
Assaad, Joseph J. ;
Issa, Camille A. .
MATERIALS AND STRUCTURES, 2013, 46 (10) :1613-1629
[4]  
Assaad JJ, 2013, ACI STRUCT J, V110, P511
[5]   Bond strength of epoxy-coated bars in underwater concrete [J].
Assaad, Joseph J. ;
Issa, Camille A. .
CONSTRUCTION AND BUILDING MATERIALS, 2012, 30 :667-674
[6]  
ASTM C, 2002, Annual Book of ASTM Standards, V4
[7]   Dosage effect of superplasticizer on self-compacting concrete: correlation between rheology and strength [J].
Benaicha, M. ;
Hafidi Alaoui, A. ;
Jalbaud, O. ;
Burtschell, Y. .
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2019, 8 (02) :2063-2069
[8]  
Bowles O., 1956, Limestone and dolomite
[9]   Additivity effect on properties of cemented coal fly ash backfill containing water-reducing admixtures [J].
Cavusoglu, Ibrahim ;
Yilmaz, Erol ;
Yilmaz, Ali Osman .
CONSTRUCTION AND BUILDING MATERIALS, 2021, 267
[10]  
Daou Y., 2011, SALMAN, V153, P162