Durability of PEFCs at high humidity conditions

被引:339
作者
Xie, J
Wood, DL
Wayne, DM
Zawodzinski, TA
Atanassov, P
Borup, RL
机构
[1] Los Alamos Natl Lab, Elect & Electrochem Mat & Devices Grp, Los Alamos, NM 87545 USA
[2] Pit Disposit Sci & Technol Grp, Los Alamos, NM 87545 USA
[3] Univ New Mexico, Dept Chem & Nucl Engn, Albuquerque, NM 87131 USA
关键词
D O I
10.1149/1.1830355
中图分类号
O646 [电化学、电解、磁化学];
学科分类号
081704 ;
摘要
This work addresses issues of long-term durability of hydrogen-air polymer electrolyte fuel cells (PEFCs). The chromium in a Pt3Cr binary alloy catalyst has been found to migrate from cathode to anode during the course of life testing when operating within the oversaturated, or high-humidity, gas feed regime (one or both inlet feeds with a dew point equal to or higher than cell operating temperature! above 1 A/cm(2) current density. Other major factors such as membrane degradation, dissolution of catalyst-layer recast ionomer, catalyst oxidation, and catalyst agglomeration/growth have been identified as simultaneous, gradual processes that can lead to long-term PEFC failure. In situ cyclic voltammetry measurement of electrochemically active catalyst surface area shows a continuous decrease, revealing that catalyst agglomeration and/or growth may be a major cause of membrane electrode assembly degradation during middle-term life tests (i.e., operation times up to about 2000 h) under high-humidity conditions. Membrane and/or recast ionomer degradation was confirmed by the presence of fluoride and sulfate anions in the cathode outlet water. Scanning and transmission electron microscopy observation of a tested MEA suggest the loss of carbon-supported catalyst clusters and possible dissolution of recast Nafion ionomer. (C) 2004 The Electrochemical Society.
引用
收藏
页码:A104 / A113
页数:10
相关论文
共 31 条
[1]   Preparation of cross-sectional samples of proton exchange membrane fuel cells by ultramicrotomy for TEM [J].
Blom, DA ;
Dunlap, JR ;
Nolan, TA ;
Allard, LF .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2003, 150 (04) :A414-A418
[2]   Kinetic model of platinum dissolution in PEMFCs [J].
Darling, RM ;
Meyers, JP .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2003, 150 (11) :A1523-A1527
[3]  
ENDOTH E, 2002, ELECTROCHEMICAL SOC
[4]  
GOTTESFELD S, 1998, ADV ELECTROCHEMCIAL, V5, P242
[5]   Dry layer preparation and characterisation of polymer electrolyte fuel cell components [J].
Gülzow, E ;
Schulze, M ;
Wagner, N ;
Kaz, T ;
Reissner, R ;
Steinhilber, G ;
Schneider, A .
JOURNAL OF POWER SOURCES, 2000, 86 (1-2) :352-362
[6]   Study of ionic conductivity profiles of the air cathode of a PEMFC by AC impedance spectroscopy [J].
Guo, QZ ;
Cayetano, M ;
Tsou, YM ;
De Castro, ES ;
White, RE .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2003, 150 (11) :A1440-A1449
[7]   Development of a high-performance PEFC module operated by reformed gas [J].
Isono, T ;
Suzuki, S ;
Kaneko, M ;
Akiyama, Y ;
Miyake, Y ;
Yonezu, I .
JOURNAL OF POWER SOURCES, 2000, 86 (1-2) :269-273
[8]  
KINOSHITA K, 1988, CARBON ELECTROCHEMIC, P86
[9]  
KINOSHITA K, 1977, MOD ASPECT ELECTROC, V12, P183
[10]  
LaConti A.B., 2003, HDB FUEL CELLS FUNDA, V3