Activation energies during glass transition and fragility of the As30Te64Ga6 chalcogenide glass

被引:10
|
作者
Hassan, R. M. [1 ]
Neffati, R. [2 ,3 ]
Abd-Elnaiem, A. M. [4 ]
Dahshan, A. [2 ,5 ]
机构
[1] Abyan Univ, Fac Educ Zingiber, Phys Dept, Abyan, Yemen
[2] King Khalid Univ, Fac Sci, Dept Phys, POB 9004, Abha, Saudi Arabia
[3] Univ Tunis El Manar, Lab Phys Matiere Condensee, Dept Phys, Fac Sci Tunis, Campus Univ, Tunis 1060, Tunisia
[4] Assiut Univ, Fac Sci, Phys Dept, Assiut 71516, Egypt
[5] Port Said Univ, Fac Sci, Dept Phys, Port Said, Egypt
关键词
DSC; iso-conversional methods; glass transition; chalcogenides; fragility; THERMOELECTRIC PROPERTIES; HEATING RATE; TEMPERATURE; KINETICS; LIQUIDS; SE; CRYSTALLIZATION; CALORIMETRY; RELAXATION; WATER;
D O I
10.1088/1402-4896/abff86
中图分类号
O4 [物理学];
学科分类号
0702 ;
摘要
Glass transition features of chalcogenides are important for the broad and increasing industrial applications of these glassy semiconductors. Hence, differential scanning calorimetry was applied at different scanning rates on As30Te64Ga6 prepared by conventional melt quenching technique in order to study their glass transition and fragility. The Kauzmann temperature was estimated to about 136 K while its glass transition is about 397 K at 10 K min(-1). Different experimental evaluation methods gave the same fragility index m = 25 or D = 71 which is typical of a strong liquid corresponding to the prepared glass. Four iso-conversional methods were then applied to monitor the change in the activation energy for the temperature range corresponding to the transition from glass to liquid. All methods give a small monotonic decrease of the activation energy during transition from 108 to 99 kJ mol(-1) confirming the strong character.
引用
收藏
页数:8
相关论文
共 50 条
  • [1] The activation energy and fragility index of the glass transition in Se76Te21Sb3 chalcogenide glass
    Soltan, A. S.
    Abu-Sehly, A. A.
    Joraid, A. A.
    Alamri, S. N.
    THERMOCHIMICA ACTA, 2013, 574 : 73 - 78
  • [2] The activation energy and fragility index of the glass transition in Se76Te21Sb3 chalcogenide glass
    Soltan, A. S.
    Abu-Sehly, A. A.
    Joraid, A. A.
    Alamri, S. N.
    3RD INTERNATIONAL ADVANCES IN APPLIED PHYSICS AND MATERIALS SCIENCE CONGRESS, 2013, 1569 : 442 - 445
  • [3] Kinetics of the glass transition in AS22S78 chalcogenide glass: Activation energy and fragility index
    Abu-Sehly, A. A.
    MATERIALS CHEMISTRY AND PHYSICS, 2011, 125 (03) : 672 - 677
  • [4] Glass transition and crystallization study of Te additive Se - Bi chalcogenide glass
    Farid, A. S.
    Atyia, H. E.
    JOURNAL OF NON-CRYSTALLINE SOLIDS, 2015, 408 : 123 - 129
  • [5] Kinetics of the glass transition in Se72Te23Sb5 chalcogenide glass: Variation of the activation energy
    Elabbar, Abdalla A.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2009, 476 (1-2) : 125 - 129
  • [6] Glass transition and crystallization of Se 95 Te 5 chalcogenide glassy semiconductor
    Atayeva, S. U.
    Isayev, A. I.
    Mekhtiyeva, S. I.
    Garibova, S. N.
    Alekberov, R. I.
    Mammadov, F. N.
    CHALCOGENIDE LETTERS, 2024, 21 (04): : 355 - 363
  • [7] Glass transition and crystallization study of chalcogenide Se70Te15In15 glass
    Tripathi, S. K.
    Patial, Balbir Singh
    Thakur, Nagesh
    JOURNAL OF THERMAL ANALYSIS AND CALORIMETRY, 2012, 107 (01) : 31 - 38
  • [8] COMPOSITIONAL TRENDS OF THE GLASS TRANSITION AND CRYSTALLIZATION IN Te20Se80-xSbx CHALCOGENIDE GLASSES
    Elabbar, A. A.
    CHALCOGENIDE LETTERS, 2014, 11 (12): : 651 - 659
  • [9] Influence of silver introduction on glass-transition and crystallization processes in As40Se30Te30 glass
    Vigi, Robert
    Bosak, Ondrej
    Strbac, Dragana
    Strbac, Goran
    JOURNAL OF THERMAL ANALYSIS AND CALORIMETRY, 2024, : 895 - 910
  • [10] The activation energies at glass transition temperatures and dynamic fragility of (Se90Te10)100-x Inx glassy alloys
    Abd-Elrahman, M. I.
    Sayed, M.
    Abu El-Fadl, A.
    Abu-Sehly, A. A.
    Hafiz, M. M.
    THERMOCHIMICA ACTA, 2019, 672 : 86 - 92