Advances in pressureless densification of boron carbide

被引:65
作者
Speyer, RF [1 ]
Lee, H
机构
[1] Georgia Inst Technol, Sch Mat Sci & Engn, Atlanta, GA 30332 USA
[2] USAF, Inst Technol, Dept Aeronaut & Astronaut, Wright Patterson AFB, OH 45433 USA
关键词
D O I
10.1023/B:JMSC.0000041698.23052.b9
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The coarsening processes which occur concurrently with the sintering of B4C were deduced using differential dilatometry, weight loss and grain size measurements. B2O3 coatings on B4C particles stalled the onset of densification until these coatings decomposed away at 1840degreesC. Oxide gaseous species formed in this process were postulated to be one conduit of particle coarsening. At higher temperatures, the volatilization of B4C itself were interpreted to be the second vapor phase coarsening mechanism, starting at temperatures above 2000degreesC. Carbon additions or soaking the compact in a hydrogen-containing atmosphere at 1350degreesC removed the oxide coatings at temperatures below those in which sintering or coarsening occurred. Accelerating densification above 2130degreesC was attributed to nonstoichiometric volatilization, leaving carbon behind to facilitate activated sintering. (C) 2004 Kluwer Academic Publishers.
引用
收藏
页码:6017 / 6021
页数:5
相关论文
共 11 条
  • [1] [Anonymous], 1996, Sintering theory and practice
  • [2] MICROSTRUCTURAL COARSENING DURING SINTERING OF BORON-CARBIDE
    DOLE, SL
    PROCHAZKA, S
    DOREMUS, RH
    [J]. JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1989, 72 (06) : 958 - 966
  • [3] STRUCTURE AND SINGLE-PHASE REGIME OF BORON CARBIDES
    EMIN, D
    [J]. PHYSICAL REVIEW B, 1988, 38 (09): : 6041 - 6055
  • [4] KANNO Y, 1987, NIPPON SERAM KYO GAK, V95, P1137, DOI 10.2109/jcersj1950.95.1107_1137
  • [5] PRESSURELESS SINTERING AND RELATED REACTION PHENOMENA OF AL2O3-DOPED B4C
    LEE, CH
    KIM, CH
    [J]. JOURNAL OF MATERIALS SCIENCE, 1992, 27 (23) : 6335 - 6340
  • [6] Pressureless sintering of boron carbide
    Lee, H
    Speyer, RF
    [J]. JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2003, 86 (09) : 1468 - 1473
  • [7] Sintering of boron carbide heat-treated with hydrogen
    Lee, H
    Speyer, RF
    Hackenberger, WS
    [J]. JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2002, 85 (08) : 2131 - 2133
  • [8] Schwetz K. A., 1980, U.S. Patent, Patent No. [4,195,066, 4195066, US 4195066]
  • [9] Skorokhod V, 1996, J MATER SCI LETT, V15, P1337, DOI 10.1007/BF00240800
  • [10] Thevenot F., 1990, Journal of the European Ceramic Society, V6, P205, DOI 10.1016/0955-2219(90)90048-K