Tribological, electrochemical and in vitro biocompatibility properties of SiC reinforced composite coatings

被引:37
作者
Das, Mitun [1 ]
Balla, Vamsi Krishna [1 ]
Kumar, T. S. Sampath [2 ]
Bandyopadhyay, Amit [3 ]
Manna, Indranil [1 ,4 ]
机构
[1] Cent Glass & Ceram Res Inst, CSIR, Bioceram & Coating Div, 196 Raja SC Mullick Rd, Kolkata 700032, India
[2] Indian Inst Technol Madras, Dept Met & Mat Engn, Madras 60036, Tamil Nadu, India
[3] Washington State Univ, Sch Mech & Mat Engn, WM Keck Biomed Mat Res Lab, Pullman, WA 99164 USA
[4] IITK, Kanpur 208016, Uttar Pradesh, India
关键词
Laser processing; Composite coatings; Wear resistance; Biocompatibility; SILICON-CARBIDE; WEAR PROPERTIES; TITANIUM; METAL; WATER; FRICTION; ALLOYS; CYTOCOMPATIBILITY; MICROSTRUCTURE; ALUMINA;
D O I
10.1016/j.matdes.2016.01.143
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In this work, laser engineered net shaping (LENS (TM)) technique was used to create SiC reinforced titanium matrix composite (TMC) on titanium surface. These composite coatings developed by injecting SiC powder into titanium melt pool, created using a high-power laser. The laser parameters strongly influenced the dissolution of SiC particles leading to formation of TiSi2, Ti5Si3, and TiC phases along with residual SiC in the composite layers. A graded microstructure, with high concentration of secondary phases on top compared to the bottom region was formed. The reinforcing ceramic phases in the TMC coatings enhanced the wear resistance of titanium by about 100 times. The wear resistance of the composite coatings in physiological environment found to increase with increase in the laser power and concentration of SiC particles injected into the melt pool. These composite coatings also showed better corrosion resistance than Ti. In vitro biocompatibility studies performed using osteoblast (MG63) and fibroblast cells (NIH3T3) demonstrated non-toxic nature of these composite coatings. It is envisioned that such coatings may find applications in articulating surfaces of load-bearing implants to enhance their in vivo lifetime with reduced metal ion release. (C) 2016 Elsevier Ltd. All rights reserved.
引用
收藏
页码:510 / 517
页数:8
相关论文
共 36 条
[31]  
Willmann G, 2001, ADV ENG MATER, V3, P135, DOI 10.1002/1527-2648(200103)3:3<135::AID-ADEM135>3.0.CO
[32]  
2-B
[33]   Formation of tribochemical layer of ceramics sliding in water and its role for low friction [J].
Xu, JG ;
Kato, K .
WEAR, 2000, 245 (1-2) :61-75
[34]   Surface characteristic and cell response of CVD SiC coating for carbon/carbon composites used for hip arthroplasty [J].
Zhang Lei-Lei ;
Li He-Jun ;
Lu Jin-Hua ;
Li Ke-Zhi ;
Cao Sheng ;
Zhao Xue-Ni ;
He Zi-Bo .
SURFACE AND INTERFACE ANALYSIS, 2012, 44 (10) :1319-1323
[35]   Friction and wear properties of CrN coatings sliding against Si3N4 balls in water and air [J].
Zhou, Fei ;
Chen, Kangmin ;
Wang, Meiling ;
Xu, Xiaojing ;
Meng, Hua ;
Yu, Min ;
Dai, Zhendong .
WEAR, 2008, 265 (7-8) :1029-1037
[36]   Friction and wear properties of duplex MAO/CrN coatings sliding against Si3N4 ceramic balls in air, water and oil [J].
Zhou, Fei ;
Wang, Yuan ;
Liu, Feng ;
Meng, Yuedong ;
Dai, Zhendong .
WEAR, 2009, 267 (9-10) :1581-1588