Segmented block copolymers of natural rubber and propylene glycol toluene diisocyanate oligomers

被引:23
作者
Paul, CJ
Nair, MRG
Neelakantan, NR
Koshy, P
机构
[1] Mahatma Gandhi Univ, Sch Chem Sci, Kottayam 686560, Kerala, India
[2] Indian Inst Technol, Div Chem Engn, Madras 600036, Tamil Nadu, India
[3] Reg Res Lab, Instrumentat & Electron Microscopy Div, Trivandrum 695019, Kerala, India
关键词
D O I
10.1002/pen.10205
中图分类号
TQ [化学工业];
学科分类号
0817 ;
摘要
Segmented block copolymers were synthesized from hydroxyl terminated liquid natural rubber (HTNR) and polyurethane oligomers based on 1,2-propylene glycol and toluene diisocyanate (TDI) by one-shot and two-shot processes in solution. They were completely phase segregated. Structural features were characterized by infrared and nuclear magnetic resonance spectroscopies. The two-phase morphology was deducted from thermal analysis and dynamic mechanical analysis (DMA). The soft segment glass transition temperature was about -64 degrees C and the hard segment glass transition was between 70 degrees C and 100 degrees C depending on the polyurethane content. The two-phase morphology was corroborated by a two-stage thermal decomposition of the products. The morphology consisted of a heterogeneous dispersion of beads in a continuous matrix. The large size and the nature of the beads suggest that they are independent of the block copolymer structure and are formed by the agglomeration of the polyurethane homopolymers, which remain unbonded to the rubber chains during chain extension. At lower hard segment contents the materials behaved like quasi-elastomers, and at higher hard segment contents, they were like tough plastics. At intermediate compositions they behaved as rigid elastomers. Variations in hardness and tear strength were consistent with this behavior.
引用
收藏
页码:440 / 451
页数:12
相关论文
共 34 条
[11]  
MADHUSUDANAN PM, 1975, J THERMAL ANAL, V8, P311
[12]  
Mampel KL, 1940, Z PHYS CHEM A-CHEM T, V187, P43
[13]  
MEVLIDA V, 1990, POLIMERI ZAGREB, V11, P15
[14]  
OAN AT, 1990, POLLIMO, V14, P608
[15]  
OAN AT, 1990, POLLIMO, V14, P497
[16]  
OERTEL G, POLYURETHANE HDB, P85
[17]  
PAUL CJ, 1992, J NAT RUBBER RES, V5, P199
[18]   STUDY OF THE EFFECT OF SOFT-SEGMENT LENGTH AND CONCENTRATION ON PROPERTIES OF POLYETHERURETHANES .1. THE EFFECT ON PHYSICAL AND MORPHOLOGICAL PROPERTIES [J].
PETROVIC, ZS ;
BUDINSKISIMENDIC, J .
RUBBER CHEMISTRY AND TECHNOLOGY, 1985, 58 (04) :685-700
[19]   SEGMENTED BLOCK COPOLYMERS BASED ON LIQUID NATURAL-RUBBER [J].
RAVINDRAN, T ;
NAYAR, MRG ;
FRANCIS, DJ .
JOURNAL OF APPLIED POLYMER SCIENCE, 1991, 42 (02) :325-333
[20]   PRODUCTION OF HYDROXYL-TERMINATED LIQUID NATURAL-RUBBER - MECHANISM OF PHOTOCHEMICAL DEPOLYMERIZATION AND HYDROXYLATION [J].
RAVINDRAN, T ;
NAYAR, MRG ;
FRANCIS, DJ .
JOURNAL OF APPLIED POLYMER SCIENCE, 1988, 35 (05) :1227-1239