Effects of water and hydrogen on early stage oxidation of high purity titanium

被引:0
作者
Mizuno, Y [1 ]
Tanaka, A [1 ]
Tonda, H [1 ]
Takakuwa, Y [1 ]
Takahiro, K [1 ]
Ishikawa, K [1 ]
Takano, T [1 ]
Ikeuch, T [1 ]
Okada, T [1 ]
Yamaguchi, S [1 ]
Homma, T [1 ]
机构
[1] Nippon Valqua Ind Ltd, Shinjuku Ku, Tokyo 1630406, Japan
来源
HIGH TEMPERATURE CORROSION AND MATERIALS CHEMISTRY | 2000年 / 99卷 / 38期
关键词
oxide layer; titanium; high purity material; hydrogen; ERDA; XPS;
D O I
暂无
中图分类号
O646 [电化学、电解、磁化学];
学科分类号
081704 ;
摘要
Study has been made of the effects of hydrogen to early stage oxidation on a titanium surface under different treatments. Characterization of oxide layers was performed by using AES and XPS. Some influence of hydrogen on the titanium oxidation during the surface treatments was established by obtaining depth profiles of hydrogen with ERDA. The depth profiles showed extremely high-density of hydrogen in the surfaces, especially depending on MCP and BP treatments, In the samples of titanium hydrides, the deformed valence band spectra of energy states between 3 and 13 eV consistent with hydride formation were observed by XPS. To estimate surface chemical affinity of gas species, TDS was applied to each titanium surface. The TD spectra of H-2 and H2O showed significant differences among three kinds of solvents; water, alcohol and carbon tetrachloride. It has been suggested that mechanical and chemical processes of the surface treatment play an important role at an early stage of titanium surface oxidation.
引用
收藏
页码:153 / 165
页数:13
相关论文
共 50 条
  • [41] High temperature oxidation of titanium-silicon alloys
    Vojtech, D
    Bártová, B
    Kubatík, T
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2003, 361 (1-2): : 50 - 57
  • [42] Role of niobium in the high-temperature oxidation of titanium
    Valenza, Thomas C.
    Weber, Peter K.
    Marquis, Emmanuelle A.
    CORROSION SCIENCE, 2023, 225
  • [43] Role of gold in high temperature oxidation of titanium alloy
    Zhang, ZX
    Dong, H
    Bell, T
    SURFACE ENGINEERING, 2005, 21 (01) : 76 - 79
  • [44] Effects of titanium on a ferritic steel oxidation at 950°C
    Issartel, C
    Buscail, H
    Caudron, E
    Cueff, R
    Riffard, F
    El Messki, S
    Karimi, N
    Antoni, L
    HIGH TEMPERATURE CORROSION AND PROTECTION OF MATERIALS 6, PRT 1 AND 2, PROCEEDINGS, 2004, 461-464 : 69 - 76
  • [45] The oxidation of calcium implanted titanium in water: A depth profiling study
    Armitage, D. A.
    Mihoc, R.
    Tate, T. J.
    McPhail, D. S.
    Chater, R.
    Hobkirk, J. A.
    Shinawi, L.
    Jones, F. H.
    APPLIED SURFACE SCIENCE, 2007, 253 (08) : 4085 - 4093
  • [46] The effect of hydrogen on the early stages of oxidation of a magnesium alloy
    McCarroll, I. E.
    Haley, D.
    Thomas, S.
    Meier, M. S.
    Bagot, P. A. J.
    Moody, M. P.
    Birbilis, N.
    Cairney, J. M.
    CORROSION SCIENCE, 2020, 165
  • [47] Design of a methane processing system producing high-purity hydrogen
    Tan, Oezguer
    Masalaci, Emre
    Oensan, Z. Ilsen
    Avci, Ahmet K.
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2008, 33 (20) : 5516 - 5526
  • [48] Hydrogen isotopic evidence for early oxidation of silicate Earth
    Pahlevan, Kaveh
    Schaefer, Laura
    Hirschmann, Marc M.
    EARTH AND PLANETARY SCIENCE LETTERS, 2019, 526
  • [49] Effects of Hydrogen Contents on Oxidation Behavior of Alloy 690TT and Associated Boron Accumulation within Oxides in High-Temperature Water
    Jeon, Soon-Hyeok
    Song, Geun Dong
    Hur, Do Haeng
    SCANNING, 2018,
  • [50] The corrosion behavior of commercial purity titanium after double glow plasma hydrogen-free carburizing
    Zhang, GH
    Liu, XL
    Zhang, PZ
    Liu, YP
    Pan, JD
    Xu, Z
    ISTM/2005: 6TH INTERNATIONAL SYMPOSIUM ON TEST AND MEASUREMENT, VOLS 1-9, CONFERENCE PROCEEDINGS, 2005, : 9071 - 9074