Deuterium trapping and surface modification of polycrystalline tungsten exposed to a high-flux plasma at high fluences

被引:41
作者
Zibrov, M. [1 ,2 ,3 ,4 ,5 ]
Balden, M. [1 ]
Morgan, T. W. [2 ]
Mayer, M. [1 ]
机构
[1] Max Planck Inst Plasma Phys, Boltzmannstr 2, D-85748 Garching, Germany
[2] DIFFER Dutch Inst Fundamental Energy Res, Zaale 20, NL-5612 AJ Eindhoven, Netherlands
[3] Univ Ghent, Dept Appl Phys, Sint Pietersnieuwstr 41, B-9000 Ghent, Belgium
[4] Tech Univ Munich, Phys Dept E28, James Franck Str 1, D-85748 Garching, Germany
[5] Natl Res Nucl Univ, MEPhI Moscow Engn Phys Inst, Kashirskoe Shosse 31, Moscow 115409, Russia
关键词
tungsten; deuterium retention; surface modifications; blistering; high fluences; ORIENTATION DEPENDENCE; LOW-ENERGY; RETENTION; MORPHOLOGY; FILMS;
D O I
10.1088/1741-4326/aa5898
中图分类号
O35 [流体力学]; O53 [等离子体物理学];
学科分类号
070204 ; 080103 ; 080704 ;
摘要
Deuterium (D) retention and surface modifications of hot-rolled polycrystalline tungsten (W) exposed to a low-energy (similar to 40 eV D-1), high-flux (2-5 x 10(23) D m(-2) s(-1)) D plasma at temperatures of similar to 380 K and similar to 1140 K to fluences up to 1.2 x 10(28) D m(-2) have been examined by using nuclear reaction analysis, thermal desorption spectroscopy, and scanning electron microscopy. The samples exposed at similar to 380 K exhibited various types of surface modifications: dome-shaped blister-like structures, stepped flat-topped protrusions, and various types of nanostructures. It was observed that a large fraction of the surface was covered with blisters and protrusions, but their average size and the number density showed almost no fluence dependence. The D depth distributions and total D inventories also barely changed with increasing fluence at similar to 380 K. A substantial amount of D was retained in the subsurface region, and thickness correlated with the depth where the cavities of blisters and protrusions were located. It is therefore suggested that defects appearing during creation of blisters and protrusions govern the D trapping in the investigated fluence range. In addition, a large number of small cracks was observed on the exposed surfaces, which can serve as fast D release channels towards the surface, resulting in a reduction of the effective D influx into the W bulk. On the samples exposed at similar to 1140 K no blisters and protrusions were found. However, wave-like and faceted terrace-like structures were formed instead. The concentrations of trapped D were very low (<10(-5) at. fr.) after the exposure at similar to 1140 K.
引用
收藏
页数:9
相关论文
共 36 条
[1]   Temperature dependence of surface morphology and deuterium retention in polycrystalline ITER-grade tungsten exposed to low-energy, high-flux D plasma [J].
Alimov, V. Kh. ;
Tyburska-Pueschel, B. ;
Lindig, S. ;
Hatano, Y. ;
Balden, M. ;
Roth, J. ;
Isobe, K. ;
Matsuyama, M. ;
Yamanishi, T. .
JOURNAL OF NUCLEAR MATERIALS, 2012, 420 (1-3) :519-524
[2]   Deuterium retention and morphological modifications of the surface in five grades of tungsten after deuterium plasma exposure [J].
Balden, M. ;
Manhard, A. ;
Elgeti, S. .
JOURNAL OF NUCLEAR MATERIALS, 2014, 452 (1-3) :248-256
[3]   Influence of tungsten microstructure and ion flux on deuterium plasma-induced surface modifications and deuterium retention [J].
Buzi, L. ;
De Temmerman, G. ;
Unterberg, B. ;
Reinhart, M. ;
Dittmar, T. ;
Matveev, D. ;
Linsmeier, Ch. ;
Breuer, U. ;
Kreter, A. ;
Van Oost, G. .
JOURNAL OF NUCLEAR MATERIALS, 2015, 463 :320-324
[4]   ELM simulation experiments on Pilot-PSI using simultaneous high flux plasma and transient heat/particle source [J].
De Temmerman, G. ;
Zielinski, J. J. ;
van Diepen, S. ;
Marot, L. ;
Price, M. .
NUCLEAR FUSION, 2011, 51 (07)
[5]   Retention in tungsten resulting from extremely high fluence plasma exposure [J].
Doerner, R. P. ;
Baldwin, M. J. ;
Lynch, T. C. ;
Yu, J. H. .
NUCLEAR MATERIALS AND ENERGY, 2016, 9 :89-92
[6]  
ELEVELD H, 1992, J NUCL MATER, V191, P433
[7]   Suppression of hydrogen-induced blistering of tungsten by pre-irradiation at low temperature [J].
Gao, L. ;
von Toussaint, U. ;
Jacob, W. ;
Balden, M. ;
Manhard, A. .
NUCLEAR FUSION, 2014, 54 (12)
[8]   Mechanism for orientation dependence of blisters on W surface exposed to D plasma at low temperature [J].
Jia, Y. Z. ;
Liu, W. ;
Xu, B. ;
Luo, G. -N. ;
Qu, S. L. ;
Morgan, T. W. ;
De Temmerman, G. .
JOURNAL OF NUCLEAR MATERIALS, 2016, 477 :165-171
[9]   Nanostructures and pinholes on W surfaces exposed to high flux D plasma at high temperatures [J].
Jia, Y. Z. ;
Liu, W. ;
Xu, B. ;
Luo, G. -N. ;
Li, C. ;
Fu, B. Q. ;
De Temmerman, G. .
JOURNAL OF NUCLEAR MATERIALS, 2015, 463 :312-315
[10]  
Jia Y. Z., 2015, J NUCL MAT