Prediction of swelling of 18Cr10NiTi austenitic steel over a wide range of displacement rates

被引:37
作者
Kalchenko, A. S. [2 ]
Bryk, V. V. [2 ]
Lazarev, N. P. [2 ]
Neklyudov, I. M. [2 ]
Voyevodin, V. N. [2 ]
Garner, F. A. [1 ]
机构
[1] Radiat Effects Consulting, Richland, WA 99354 USA
[2] Kharkov Phys & Technol Inst, Natl Sci Ctr, UA-61108 Kharkov, Ukraine
关键词
MICROSTRUCTURAL EVOLUTION; FAST-REACTOR; IRRADIATION; ALLOYS; BN-350; TEMPERATURE; PERFORMANCE; METALS; DPA;
D O I
10.1016/j.jnucmat.2010.01.010
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The internal components of pressurized water reactors of Russian types WWER-440 and WWER-1000 are constructed of annealed 18Cr10NiTi steel, a close analog to AISI 321. Void swelling of the internals is a concern for plant life extension and predictive equations are required to assess the potential of swelling in critical components such as the baffle ring or reflection shield that surrounds the WWER core. The only previously available swelling data for this steel were derived at higher than PWR-relevant displacement rates in the BOR-60 fast reactor. The swelling equation previously developed from these data does not incorporate the effect of displacement rate on swelling. Using heavy-ion irradiation at very high dpa rates (10(-2) and 10(-3) dpa s(-1)) and doses (5-100 dpa) and coupling the results to available neutron data a swelling equation has been developed that specifically incorporates the effect of dpa rate on void swelling. Experimental results allow description of the swelling peak, the incubation period and the steady-state swelling rate over a wide range of irradiation temperature. For the first time it appears possible to describe both ion and neutron data on this steel within the framework of a single empirical model. Swelling maps constructed from this model permit forecasting of the behavior of the steel in WWERs under the required irradiation conditions, not only at already attained exposure doses, but more importantly to higher dose levels that will be reached following plant life extension. (C) 2010 Elsevier B.V. All rights reserved.
引用
收藏
页码:114 / 121
页数:8
相关论文
共 35 条
[11]  
Garner F.A., 1976, ASTM STP, V611, P208
[12]  
Garner F.A., 1983, P INT C DIM STAB MEC, VII, P41
[13]  
Garner F. A., 1994, Materials Science and Technology: A Comprehensive Treatment, V10, P419
[15]  
GARNER FA, 1993, PROCEEDINGS OF THE SIXTH INTERNATIONAL SYMPOSIUM ON ENVIRONMENTAL DEGRADATION OF MATERIALS IN NUCLEAR POWER SYSTEMS - WATER REACTORS, P783
[16]   Comparison of swelling and irradiation creep behavior of fcc-austenitic and bcc-ferritic/martensitic alloys at high neutron exposure [J].
Garner, FA ;
Toloczko, MB ;
Sencer, BH .
JOURNAL OF NUCLEAR MATERIALS, 2000, 276 (01) :123-142
[17]  
GARNER FA, 2006, FONT 6 S CONTR MAT I, P637
[18]  
GARNER FA, 2006, FONT 6 S CONTR MAT I, P625
[19]   Vold swelling of AISI 321 analog stainless steel irradiated at low dpa rates in the BN-350 reactor [J].
Maksimkin, O. P. ;
Tsai, K. V. ;
Turubarova, L. G. ;
Doronina, T. ;
Garner, F. A. .
JOURNAL OF NUCLEAR MATERIALS, 2007, 367 (990-994) :990-994
[20]   Characterization of 08Cr16Ni11Mo3 stainless steel irradiated in the BN-350 reactor [J].
Maksimkin, OP ;
Tsai, KV ;
Turubarova, LG ;
Doronina, T ;
Garner, FA .
JOURNAL OF NUCLEAR MATERIALS, 2004, 329 :625-629