Rheology, mechanical properties and thermal degradation kinetics of polypropylene (PP) and polylactic acid (PLA) blends

被引:36
作者
Rajan, Krishna Prasad [1 ]
Thomas, Selvin P. [1 ,2 ]
Gopanna, Aravinthan [2 ]
Al-Ghamdi, Ahmed [1 ]
Chavali, Murthy [3 ]
机构
[1] Royal Commiss Yanbu Coll & Inst, Yanbu Ind Coll, Dept Chem Engn Technol, POB 30436, Yanbu Ind City 41912, Saudi Arabia
[2] Royal Commiss Yanbu Coll & Inst, Yanbu Res Ctr, Adv Mat Lab, POB 30436, Yanbu Ind City 41912, Saudi Arabia
[3] MCETRC, Guntur 522201, Andhra Pradesh, India
关键词
capillary; rheometry; thermal degradation; non-isothermal methods; polymer blends; kinetic models; apparent activation energy; L-LACTIC ACID; POLY(LACTIC ACID); SELECTIVE DEPOLYMERIZATION; ISOCONVERSIONAL METHOD; PYROLYSIS KINETICS; BARRIER PROPERTIES; POLYMER MELTS; ACTIVATION; COMPATIBILIZATION; L; L-LACTIDE;
D O I
10.1088/2053-1591/aad1d3
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The blending of immiscible polymers and their compatibilization leads to materials with tailor-made properties suitable for wide range of applications. Polypropylene (PP) and polylactic acid (PLA) were blended in different weight ratios and the optimized blend was compatibilized with maleic anhydride grafted PP (MA-g-PP) in varying amounts from 0 to 5 wt%. Rheological studies performed using a capillary rheometer showed the pseudo plastic behavior of the blends and from the shear viscosity data, it was observed that 3 wt% of the compatibilizer effectively compatibilized the selected blend. Mechanical properties further confirmed this finding. Thermogravimetric analysis revealed a two-stage degradation mechanism for the blends, corresponding to each component in the blend system. The apparent activation energy (E a ) values for the thermal degradation were calculated using Kissinger method, Horowitz and Metzger method, Kissinger-Akahira-Sunose equation, Friedman model and Ozawa-Flynn and Wall method. Coats-Redfern method was used to elucidate the mechanism of thermal degradation of the chosen blend system. The E-a values for PLA component of the blend increased with increase in compatibilizer addition up to 3 wt% and then decreased, whereas, it decreased for PP fraction up to a compatibilizer level of 3 wt% and then increased.
引用
收藏
页数:18
相关论文
共 74 条
[1]   Thermal degradation behaviors of polyethylene and polypropylene. Part I: Pyrolysis kinetics and mechanisms [J].
Aboulkas, A. ;
El Harfi, K. ;
El Bouadili, A. .
ENERGY CONVERSION AND MANAGEMENT, 2010, 51 (07) :1363-1369
[2]  
Akahira T., 1971, RES REPORT CHIBA I T, V16, P22
[3]   Thermal degradation of poly[(R)-3-hydroxybutyrate], poly[ε-caprolactone], and poly[(S)-lactide] [J].
Aoyagi, Y ;
Yamashita, K ;
Doi, Y .
POLYMER DEGRADATION AND STABILITY, 2002, 76 (01) :53-59
[4]   Tuning the processability, morphology and biodegradability of clay incorporated PLA/LLDPE blends via selective localization of nanoclay induced by melt mixing sequence [J].
As'habi, L. ;
Jafari, S. H. ;
Khonakdar, H. A. ;
Boldt, R. ;
Wagenknecht, U. ;
Heinrich, G. .
EXPRESS POLYMER LETTERS, 2013, 7 (01) :21-39
[5]   Effect of water on the oxygen barrier properties of poly(ethylene terephthalate) and polylactide films [J].
Auras, R ;
Harte, B ;
Selke, S .
JOURNAL OF APPLIED POLYMER SCIENCE, 2004, 92 (03) :1790-1803
[6]   Mechanical, physical, and barrier properties of poly(lactide) films [J].
Auras, RA ;
Harte, B ;
Selke, S ;
Hernandez, R .
JOURNAL OF PLASTIC FILM & SHEETING, 2003, 19 (02) :123-135
[7]  
Babanalbandi A, 1999, POLYM INT
[8]   Extensional viscosity for polymer melts measured in the filament stretching rheometer [J].
Bach, A ;
Rasmussen, HK ;
Hassager, O .
JOURNAL OF RHEOLOGY, 2003, 47 (02) :429-441
[9]  
Bai Z-F, 2015, INT C MAT SCI APPL I, P282
[10]   Rheology, Morphology, Crystallization Behaviors, Mechanical and Thermal Properties of Poly(lactic acid)/Polypropylene/Maleic Anhydride-Grafted Polypropylene Blends [J].
Bai, Zhifei ;
Dou, Qiang .
JOURNAL OF POLYMERS AND THE ENVIRONMENT, 2018, 26 (03) :959-969