Crack Propagation Behavior of SNCM439 Steels in High-pressure Hydrogen Gas

被引:2
作者
Arashima, Hironobu [1 ]
Masada, Satoru [1 ]
Isobe, Shigehito [2 ]
Hashimoto, Naoyuki [2 ]
机构
[1] Japan Steel Works M&E Inc, 4 Chatsucho, Muroran, Hokkaido 0518505, Japan
[2] Hokkaido Univ, Kita Ku, N13,W8, Sapporo, Hokkaido 0608628, Japan
关键词
low-alloy steel; high-pressure hydrogen gas; hydrogen embrittlement; stress intensity factor; rising load test; crack initiation; INITIATION;
D O I
10.2355/isijinternational.ISIJINT-2022-017
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
To investigate the effect of high-pressure hydrogen gas on the fracture of high-strength low-alloy steels, rising load tests were conducted on JIS SNCM439 steel in high-pressure (20 MPa) hydrogen gas at room temperature (20-25 degrees C), and its hydrogen-induced crack initiation behavior was investigated. The load-crack opening displacement curve obtained for rising load tests in hydrogen began to deviate from that obtained in air at very low loads, indicating that the stress intensity factor at crack initiation was significantly smaller in hydrogen. Scanning electron microscopy observations of the fractured surfaces of the specimens unloaded during the middle of the rising load test confirmed that hydrogen-induced cracks had already occurred at a load lower than the deviation point. The stretch zone that appeared in the rising load test in air was not observed for the test in hydrogen, and the hydrogen-induced cracks were found to directly initiate from the tip of the fatigue pre-crack. The hydrogen-induced cracks were initiated at almost the same stress intensity factor value as that at which the stretch zone was observed in air, indicating that plastic slip and the resulting hydrogen ingress from the new surface were the causes of the hydrogen embrittlement. In addition, it was shown that the stress intensity factor for crack initiation in hydrogen increased and the effect of hydrogen decreased with the increase in loading rate, inferring that dislocation migration and hydrogen penetration into the steel are key factors for hydrogen embrittlement.
引用
收藏
页码:1540 / 1547
页数:8
相关论文
共 50 条
  • [41] Influence of hydrogen on plasticity around the crack tip in high strength steels
    de Assis, Kioshy S.
    Lage, Marcella Araujo
    Guttemberg, Geraldo
    dos Santos, Fabricio Pinheiro
    Mattos, Oscar R.
    ENGINEERING FRACTURE MECHANICS, 2017, 176 : 116 - 125
  • [42] Evaluation of the cementite morphology influence on the hydrogen induced crack nucleation and propagation path in carbon steels
    Karimi, Shabnam
    Taji, Iman
    Hajilou, Tarlan
    Barnoush, Afrooz
    Johnsen, Roy
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2022, 47 (30) : 14121 - 14129
  • [43] Review and Assessment of the Effect of Hydrogen Gas Pressure on the Embrittlement of Steels in Gaseous Hydrogen Environment
    Michler, Thorsten
    Wackermann, Ken
    Schweizer, Frank
    METALS, 2021, 11 (04)
  • [44] The Use of Crack-Tip Opening Displacement for Testing of the Hydrogen Embrittlement of High-Strength Steels
    W. Dietzel
    Materials Science, 2004, 40 : 749 - 755
  • [45] Mechanical Properties of X70 Welded Joint in High-Pressure Natural Gas/Hydrogen Mixtures
    Huang, Gai
    Zheng, Jinyang
    Meng, Bo
    Hua, Zhengli
    Lu, Qunjie
    Li, Xiongying
    Xu, Ping
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2020, 29 (03) : 1589 - 1599
  • [46] Evaluation and Analytical Method for Hydrogen Embrittlement Ⅱ:Material Testing in High Pressure Hydrogen Gas
    Koide K.
    Zairyo/Journal of the Society of Materials Science, Japan, 2022, 71 (04) : 408 - 413
  • [47] Mechanical Properties of X70 Welded Joint in High-Pressure Natural Gas/Hydrogen Mixtures
    Gai Huang
    Jinyang Zheng
    Bo Meng
    Zhengli Hua
    Qunjie Lu
    Xiongying Li
    Ping Xu
    Journal of Materials Engineering and Performance, 2020, 29 : 1589 - 1599
  • [48] Hydrogen absorption to low alloy steels in high pressure gaseous hydrogen environments
    Omura, Tomohiko
    Nakamura, Jun
    Kobayashi, Kenji
    Zairyo to Kankyo/ Corrosion Engineering, 2014, 63 (10): : 528 - 534
  • [49] DETACLAD™ CHARACTERIZATION FOR HIGH-TEMPERATURE AND HIGH-PRESSURE HYDROGEN SERVICE
    Sarrat, Olivier
    Prothe, Curtis
    Delahanty, Tim
    PROCEEDINGS OF ASME 2022 PRESSURE VESSELS AND PIPING CONFERENCE, PVP2022, VOL 4B, 2022,
  • [50] IMPACT OF HYDROGEN CONCENTRATION DISTRIBUTION IN HYDROGEN-BLENDED GAS ON FATIGUE CRACK GROWTH RATE OF PIPELINE STEELS
    Zheng, Tingsen
    Chen, Nian-Zhong
    PROCEEDINGS OF ASME 2024 43RD INTERNATIONAL CONFERENCE ON OCEAN, OFFSHORE AND ARCTIC ENGINEERING, OMAE2024, VOL 2, 2024,