Acid leaching of vanadium from roasted residue of stone coal

被引:31
作者
Zhu Yang-ge [1 ]
Zhang Guo-fan [1 ]
Feng Qi-ming [1 ]
Lu Yi-ping [1 ]
Ou Le-ming [1 ]
Huang Si-jie [1 ]
机构
[1] Cent S Univ, Sch Resources Proc & Bioengn, Changsha 410083, Hunan, Peoples R China
来源
TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA | 2010年 / 20卷
关键词
stone coal; roasting; acid leaching; vanadium;
D O I
10.1016/S1003-6326(10)60022-2
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Through leaching from residue directly and leaching after a roasting treatment, respectively, the experimental research on sulfuric leaching of vanadium from residue of stone coal that came from power generation was conducted. Factors which influence the leaching of vanadium such as concentration of sulfuric acid, leaching temperature, leaching time and liquid-to-solid ratio were investigated in both processes. In the process of direct leaching, to achieve a leaching rate of 74.49%, H2SO4 concentration of up to 5.4%, leaching temperature of 90 degrees C and leaching time of 8 h were necessary reaction factors. The results show that after a roasting treatment at the optimum condition of 950 degrees C at 1 h, 76.88% vanadium can be leached under the experimental condition of 0.45% of H2SO4, 30 degrees C for 1 h with a liquid-to-solid ratio of 2 mL/g. Leaching after an oxidation roasting treatment is an efficient way to leach vanadium from the residue of stone coal, which has some advantages, such as high recovery, low economic cost and less impurities in leaching solution.
引用
收藏
页码:S107 / S111
页数:5
相关论文
共 50 条
[41]   Recovery of sulfuric acid from a stone coal acid leaching solution by diffusion dialysis [J].
Wang, Kui ;
Zhang, Yimin ;
Huang, Jing ;
Liu, Tao ;
Wang, Jingpeng .
HYDROMETALLURGY, 2017, 173 :9-14
[42]   A mechanism of calcium fluoride-enhanced vanadium leaching from stone coal [J].
Wang, Fei ;
Zhang, Yimin ;
Liu, Tao ;
Huang, Jing ;
Zhao, Jie ;
Zhang, Guobin ;
Liu, Juan .
INTERNATIONAL JOURNAL OF MINERAL PROCESSING, 2015, 145 :87-93
[43]   Leaching of vanadium from chromium residue [J].
Yang, Kang ;
Zhang, Xiaoyun ;
Tian, Xueda ;
Yang, Yonglong ;
Chen, Yanbo .
HYDROMETALLURGY, 2010, 103 (1-4) :7-11
[44]   Leaching vanadium from extracted vanadium residue of vanadium titanomagnetite [J].
Deng, Zhigan ;
Wei, Chang ;
Li, Xingbin ;
Li, Cunxiong ;
Xu, Hongsheng ;
Li, Minting .
MANUFACTURE ENGINEERING AND ENVIRONMENT ENGINEERING, VOLS 1 AND 2, 2014, 84 :1193-1199
[45]   Effect of simulated acid rain on leaching and transformation of vanadium in paddy soils from stone coal smelting area [J].
Xiao, Xiyuan ;
Jiang, Zhichao ;
Guo, Zhaohui ;
Wang, Mingwei ;
Zhu, Huiwen ;
Han, Xiaoqing .
PROCESS SAFETY AND ENVIRONMENTAL PROTECTION, 2017, 109 :697-703
[46]   Separation of impurities aluminum and iron during pressure acid leaching of vanadium from stone [J].
Xue, Nan-nan ;
Zhang, Yi-min ;
Huang, Jing ;
Liu, Tao ;
Wang, Lu-yao .
JOURNAL OF CLEANER PRODUCTION, 2017, 166 :1265-1273
[47]   Mechanisms of aid-leaching reagent calcium fluoride in the extracting vanadium processes from stone coal [J].
Wang, Fei ;
Zhang, Yi-Min ;
Huang, Jing ;
Liu, Tao ;
Wang, Yi ;
Yang, Xiao ;
Zhao, Jie .
RARE METALS, 2013, 32 (01) :57-62
[48]   Mechanisms of aid-leaching reagent calcium fluoride in the extracting vanadium processes from stone coal [J].
Fei Wang ;
Yi-Min Zhang ;
Jing Huang ;
Tao Liu ;
Yi Wang ;
Xiao Yang ;
Jie Zhao .
Rare Metals, 2013, 32 :57-62
[49]   Mechanisms of aid-leaching reagent calcium fluoride in the extracting vanadium processes from stone coal [J].
Fei Wang ;
Yi-Min Zhang ;
Jing Huang ;
Tao Liu ;
Yi Wang ;
Xiao Yang ;
Jie Zhao .
RareMetals, 2013, 32 (01) :57-62
[50]   Enhanced vanadium bioleaching from stone coal employing Aspergillus niger : Optimization of stone coal pretreatment method [J].
Dong, Yingbo ;
Zan, Jinyu ;
Lin, Hai .
MINERALS ENGINEERING, 2024, 215