Tailoring the magnetic properties and microstructure of Alnico 8 magnets by various Ti contents and processing conditions

被引:14
作者
Rehman, Sajjad Ur [1 ,2 ]
Wei, Chen [3 ]
Zhang, Ruibiao [2 ]
Liu, Haihua [1 ]
Li, Shaoxiong [1 ]
Zhong, Minglong [1 ]
Yang, Munan [1 ]
Jiang, Qingzheng [1 ]
Wang, Jun [3 ]
Zhong, Zhenchen [1 ]
机构
[1] Jiangxi Univ Sci & Technol, Coll Rare Earths, Jiangxi Key Lab Rare Earth Magnet Mat & Devices, Ganzhou 341000, Peoples R China
[2] Zhejiang Tiantong Elect Informat Mat Res Inst Co L, Hangzhou 314400, Zhejiang, Peoples R China
[3] Northwestern Polytech Univ, State Key Lab Solidificat Proc, Xi'an 710072, Shaanxi, Peoples R China
关键词
Magnetic properties; Permanent magnets; Interaction mechanism; Ferromagnetic phase; PERMANENT-MAGNETS; ALLOYS; DECOMPOSITION; COERCIVITY; ANISOTROPY; EVOLUTION; TITANIUM; PHASE;
D O I
10.1016/j.intermet.2022.107486
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Shape anisotropy, developed as a result of spinodal decomposition (SD) is the basis for the hysteresis behavior of Alnico magnets. The SD process is sensitive to processing conditions and constituent elements. In this paper, the development of spinodal structure and its effects on magnetic properties and serviceability of Alnico 8 alloys are investigated. The Ti-content is varied between 2.5 and 7.5 wt%. The magnets are fabricated by conventional casting, homogenization, magnetic field annealing and tempering treatments. The magnetic properties of intrinsic coercivity, Hcj = 30 kA/m, remanence, Br = 0.53 T and maximum energy density, (BH)max = 6.03 kJ/m3 for 2.5 wt% Ti are increased to Hcj = 150 kA/m, Br = 0.0.88 T and (BH)max = 29.3 kJ/m3 for 6.5 wt% Ti alloy. These magnetic properties are 100% reversible up to 800 K. Furthermore, an alloy with 5.5 wt% Ti is directionally solidified and magnetic properties of Br = 1.01 T and (BH)max = 58.9 kJ/m3 are obtained. The evolution of mosaic nano structure, the mechanism of magnetic hardening and the interactions of various phases have been investigated.
引用
收藏
页数:7
相关论文
共 49 条
  • [1] Influence of Ti content on magnetic and microstructural properties of Fe-28Cr-15Co-3.5Mo permanent magnets
    Ahmad, Z
    Ul Haq, A
    Husain, SW
    Ali, A
    Abbas, T
    [J]. JOURNAL OF MAGNETISM AND MAGNETIC MATERIALS, 2003, 257 (2-3) : 397 - 402
  • [2] Synthesis, magnetic and microstructural properties of Alnico magnets with additives
    Ahmad, Zubair
    Liu, Zhongwu
    ul Haq, A.
    [J]. JOURNAL OF MAGNETISM AND MAGNETIC MATERIALS, 2017, 428 : 125 - 131
  • [3] Microstructural and Magnetic Properties of a Fe-Co-Ni-Al-Ti-Cu Alloy
    Akbar, S.
    Ahmad, Z.
    Farooque, M.
    [J]. ADVANCED MATERIALS XI, 2010, 442 : 236 - 241
  • [4] Novel pre-alloyed powder processing of modified alnico 8: Correlation of microstructure and magnetic properties
    Anderson, I. E.
    Kassen, A. G.
    White, E. M. H.
    Zhou, L.
    Tang, W.
    Palasyuk, A.
    Dennis, K. W.
    McCallum, R. W.
    Kramer, M. J.
    [J]. JOURNAL OF APPLIED PHYSICS, 2015, 117 (17)
  • [5] Buschow K.H.J., 1988, HDB FERROMAGNETIC MA
  • [6] Origin of recoil hysteresis loops in Sm-Co/Fe exchange-spring magnets
    Choi, Y.
    Jiang, J. S.
    Pearson, J. E.
    Bader, S. D.
    Liu, J. P.
    [J]. APPLIED PHYSICS LETTERS, 2007, 91 (02)
  • [7] Current progress and future challenges in rare-earth-free permanent magnets
    Cui, Jun
    Kramer, Matthew
    Zhou, Lin
    Liu, Fei
    Gabay, Alexander
    Hadjipanayis, George
    Balasubramanian, Balamurugan
    Sellmyer, David
    [J]. ACTA MATERIALIA, 2018, 158 : 118 - 137
  • [8] De Vos K.J., 1966, Journal of Applied Physics, V37, P1100
  • [9] Assessment of the Fe-Ni-Al system
    Eleno, Luiz
    Frisk, Karin
    Schneider, Andre
    [J]. INTERMETALLICS, 2006, 14 (10-11) : 1276 - 1290
  • [10] On the Formation and Evolution of Cu-Ni-Rich Bridges of Alnico Alloys With Thermomagnetic Treatment
    Fan, M.
    Liu, Y.
    Jha, Rajesh
    Dulikravich, George S.
    Schwartz, J.
    Koch, C. C.
    [J]. IEEE TRANSACTIONS ON MAGNETICS, 2016, 52 (08)