EFFECT OF DIAMOND INTERLAYER ON THE TRIBOLOGICAL PROPERTIES OF TiAlN FILM SLIDING AGAINST CARBON STEEL

被引:4
作者
Lei, X. L. [1 ]
He, Y. [1 ]
Sun, F. H. [2 ]
机构
[1] East China Univ Sci & Technol, Sch Mech & Power Engn, Shanghai 200237, Peoples R China
[2] Shanghai Jiao Tong Univ, Sch Mech Engn, Shanghai 200240, Peoples R China
基金
美国国家科学基金会; 中国博士后科学基金;
关键词
Tribology; diamond film; carbon steel; TiAlN; interlayer; WC-CO ALLOYS; CUTTING PERFORMANCE; COATINGS; TOOLS; WEAR; PRETREATMENT; DEPOSITION; FRICTION; TIN;
D O I
10.1142/S0218625X1950001X
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
In this study, the effect of diamond interlayer on the tribological properties of titanium aluminum nitride (TiAlN) film sliding against medium carbon steel is investigated in dry rotary friction tests, by evaluating the coefficients of friction (COFs), wear rates, worn surfaces and element transitions of the contacted surfaces in the cemented carbide (WC-Co)-steel, TiAlN-steel, microcrystalline diamond (MCD)-steel, TiAlN/MCD-steel, micro- and nano-crystalline diamond (MNCD)-steel and TiAlN/MNCD-steel contacting pairs. It is found that compared with the TiAlN monolayer, the TiAlN/MCD bilayer film shows 57% higher COF, while the COF of TiAlN/MNCD multilayer inversely drops as much as 54%, due to the distinguished surface diamond grain morphologies of the MCD and MNCD interlayers as well as the copied effect of the TiAlN layer with relatively small thickness. Meanwhile, the diamond interlayer can provide robust load support for the top TiAlN layer, induce the wear mechanism transform from the abrasive wear to adhesive wear, and result in the mild wear of TiAlN/MCD and TiAlN/MNCD multilayers compared to the TiAlN monolayer. Moreover, the softer TiAlN top layer on MCD and MNCD interlayers can effectively improve the storage capacity of element oxygen and worn steel ball debris as well as accelerating the surface chemical reactions to form a smoother continuous ionic metal oxides tribo film in the contacted zones due to its good self-lubricating property. Among all the hard coatings discussed when sliding against medium carbon steel, the TiAlN/MNCD coating shows the lowest COF and mild wear, due to the robust load support capacity of the beneath MNCD layer as well as the good self-lubricated and tribo film formation capacity of the top TiAlN layer, which shows broad application potential in carbon steel machining.
引用
收藏
页数:9
相关论文
共 27 条
[21]   Tribological properties and deformation mechanism of TiAlN coating sliding with various counterbodies [J].
Ramadoss, Radhika ;
Kumar, N. ;
Pandian, R. ;
Dash, S. ;
Ravindran, T. R. ;
Arivuoli, D. ;
Tyagi, A. K. .
TRIBOLOGY INTERNATIONAL, 2013, 66 :143-149
[22]  
Silva R., 2011, WEAR, V9, P2459
[23]   Wear studies of (Ti-Al)N coatings deposited by reactive magnetron sputtering [J].
Singh, K ;
Limaye, PK ;
Soni, NL ;
Grover, AK ;
Agrawal, RG ;
Suri, AK .
WEAR, 2005, 258 (11-12) :1813-1824
[24]   Tribological properties and cutting performance of boron and silicon doped diamond films on Co-cemented tungsten carbide inserts [J].
Wang, Liang ;
Lei, Xuelin ;
Shen, Bin ;
Sun, Fanghong ;
Zhang, Zhiming .
DIAMOND AND RELATED MATERIALS, 2013, 33 :54-62
[25]   Deposition of diamond/β-SiC/cobalt suicide composite interlayers to improve adhesion of diamond coating on WC-Co substrates by DC-Plasma Assisted HFCVD [J].
Wang, Tao ;
Xiang, Li ;
Shi, Wei ;
Jiang, Xin .
SURFACE & COATINGS TECHNOLOGY, 2011, 205 (8-9) :3027-3034
[26]   Grain size dependent mechanical properties of nanocrystalline diamond films grown by hot-filament CVD [J].
Wiora, M. ;
Bruehne, K. ;
Floeter, A. ;
Gluche, P. ;
Willey, T. M. ;
Kucheyev, S. O. ;
Van Buuren, A. W. ;
Hamza, A. V. ;
Biener, J. ;
Fecht, H. -J. .
DIAMOND AND RELATED MATERIALS, 2009, 18 (5-8) :927-930
[27]   Pre-treatment for diamond coatings on free-shape WC-Co tools [J].
Zhang, ZM ;
He, XC ;
Shen, HS ;
Sun, FH ;
Chen, M ;
Wan, YZ .
DIAMOND AND RELATED MATERIALS, 2000, 9 (9-10) :1749-1752