Effect of surface finishing of a Zr-based bulk metallic glass on its corrosion behaviour

被引:73
作者
Gebert, A. [1 ]
Gostin, P. F. [1 ]
Schultz, L. [1 ]
机构
[1] Leibniz Inst Solid State & Mat Res IFW Dresden, D-01171 Dresden, Germany
关键词
Zirconium; Alloy; AES; Amorphous structures; Passivity; Pitting corrosion; ZR65AL7.5NI10CU17.5 AMORPHOUS ALLOY; ELECTROCHEMICAL-BEHAVIOR; POLARIZATION BEHAVIOR; MECHANICAL-PROPERTIES; LOCALIZED CORROSION; PITTING CORROSION; ZIRCONIUM; NB; MICROSTRUCTURE; HYDROGEN;
D O I
10.1016/j.corsci.2010.01.027
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Zr-based metallic glasses passivate spontaneously, but exhibit also a certain pitting susceptibility. On the example of the Zr59Ti3Cu20Al10Ni8 alloy studied in 0.01 M Na2SO4 + x M NaCl (x = 0-0.1) electrolytes it is demonstrated that the surface finishing state and the pre-exposure conditions can significantly influence the free corrosion and anodic polarisation behaviour. Mechanical fine-polishing procedures can lead to extremely smooth topographies but also to Cu enrichment at the surface. This yields a pronounced Cu dissolution at low anodic polarisation prior to stable passivity and increases the pitting initiation susceptibility as compared to mechanically ground surface states. (C) 2010 Elsevier Ltd. All rights reserved.
引用
收藏
页码:1711 / 1720
页数:10
相关论文
共 48 条
[1]   Influence of the degree of polishing of alloy AA 5083 on its behaviour against localised alkaline corrosion [J].
Aballe, A ;
Bethencourt, M ;
Botana, FJ ;
Marcos, M ;
Sánchez-Amaya, M .
CORROSION SCIENCE, 2004, 46 (08) :1909-1920
[2]   An auger electron spectroscopic study of the corrosion behavior of an amorphous Zr40Cu60 alloy [J].
Asami, K ;
Kikuchi, M ;
Hashimoto, K .
CORROSION SCIENCE, 1997, 39 (01) :95-106
[3]   Chip formation, cutting forces, and tool wear in turning of Zr-based bulk metallic glass [J].
Bakkal, M ;
Shih, AJ ;
Scattergood, RO .
INTERNATIONAL JOURNAL OF MACHINE TOOLS & MANUFACTURE, 2004, 44 (09) :915-925
[4]   ACID CORROSION OF AMORPHOUS AND CRYSTALLINE CU-ZR ALLOYS [J].
BALA, H ;
SZYMURA, S .
APPLIED SURFACE SCIENCE, 1988, 35 (01) :41-51
[5]   Characterization of oxide layers on amorphous Zr-based alloys by Auger electron spectroscopy with sputter depth profiling [J].
Baunack, S ;
Mudali, UK ;
Gebert, A .
APPLIED SURFACE SCIENCE, 2005, 252 (01) :162-166
[6]   The influence of surface condition on the localized corrosion of 316L stainless steel orthopaedic implants [J].
Beddoes, J ;
Bucci, K .
JOURNAL OF MATERIALS SCIENCE-MATERIALS IN MEDICINE, 1999, 10 (07) :389-394
[7]   Fabrication and characterization of metallic glasses with a specific microstructure for micro-electro-mechanical system applications [J].
Chen, X. H. ;
Zhang, X. C. ;
Zhang, Y. ;
Chen, G. L. .
JOURNAL OF NON-CRYSTALLINE SOLIDS, 2008, 354 (28) :3308-3316
[8]   Influence of surface polishing on the electrochemical behavior of titanium [J].
Cheng, XL ;
Roscoe, SG .
ELECTROCHEMICAL AND SOLID STATE LETTERS, 2005, 8 (09) :B38-B41
[9]   Work-hardenable ductile bulk metallic glass [J].
Das, J ;
Tang, MB ;
Kim, KB ;
Theissmann, R ;
Baier, F ;
Wang, WH ;
Eckert, J .
PHYSICAL REVIEW LETTERS, 2005, 94 (20)
[10]   Potentiodynamic polarization studies on amorphous Zr46.75Ti8.25CU7.5Ni1.0Be27.5, Zr65CU17.5Ni10Al7.5, Zr67Ni33 and Ti60Ni40 in aqueous HNO3 solutions [J].
Dhawan, A. ;
Sachdev, K. ;
RoychowdItury, S. ;
De, P. K. ;
Sharma, S. K. .
JOURNAL OF NON-CRYSTALLINE SOLIDS, 2007, 353 (27) :2619-2623