Consolidation of titanium carbide with zirconium carbide by Spark Plasma Sintering

被引:9
作者
Li, Ying [1 ]
Katsui, Hirokazu [1 ]
Goto, Takashi [1 ]
机构
[1] Tohoku Univ, Inst Mat Res, Sendai, Miyagi 9808577, Japan
来源
ADVANCED CERAMICS AND NOVEL PROCESSING | 2014年 / 616卷
关键词
spark plasma sintering; solid solution; TI(C; N) CERMET TOOLS; MO-NI CERMETS; MECHANICAL-PROPERTIES; FRACTURE-TOUGHNESS; WC; MICROSTRUCTURE; ZRC;
D O I
10.4028/www.scientific.net/KEM.616.52
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Titanium carbide (TiC) was consolidated with 20 mol% zirconium carbide (ZrC) by spark plasma sintering in the temperature range of 1773-2473 K, and the phase formation, microstructure, relative density and mechanical properties were investigated. The composite consisted of Ti-rich (Ti, Zr)C and Zr-rich (Zr, Ti) C solid solutions at 1773-2373 K, and was single-phase (Ti, Zr) C at 2473 K. The relative density of the composite was over 98% above 2073 K. The composite prepared at 2273 K exhibited the maximum H-V of 29.7 GPa with the K-IC of 3.76 MPa m(1/2).
引用
收藏
页码:52 / 55
页数:4
相关论文
共 12 条
[1]  
[Anonymous], 2000, CRC MAT SCI ENG HDB, DOI DOI 10.1201/9781420038408
[2]   A CRITICAL-EVALUATION OF INDENTATION TECHNIQUES FOR MEASURING FRACTURE-TOUGHNESS .1. DIRECT CRACK MEASUREMENTS [J].
ANSTIS, GR ;
CHANTIKUL, P ;
LAWN, BR ;
MARSHALL, DB .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1981, 64 (09) :533-538
[3]   Densification and mechanical properties of TiC by SPS-effects of holding time, sintering temperature and pressure condition [J].
Cheng, Lixia ;
Xie, Zhipeng ;
Liu, Guanwei ;
Liu, Wei ;
Xue, Weijiang .
JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2012, 32 (12) :3399-3406
[4]   MICROSTRUCTURAL EVOLUTION DURING THE SINTERING OF TIC-MO-NI CERMETS [J].
CHUN, DI ;
KIM, DY ;
EUN, KY .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1993, 76 (08) :2049-2052
[5]   HOT-PRESSING OF SIC-TIC COMPOSITES [J].
ENDO, H ;
UEKI, M ;
KUBO, H .
JOURNAL OF MATERIALS SCIENCE, 1990, 25 (05) :2503-2506
[6]   Migration of intergranular liquid films and formation of core-shell grains in sintered TiC-Ni bonded to WC-Ni [J].
Ko, JY ;
Park, SY ;
Yoon, DY ;
Kang, SJL .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2004, 87 (12) :2262-2267
[7]  
Koc R, 1997, J AM CERAM SOC, V80, P952, DOI 10.1111/j.1151-2916.1997.tb02926.x
[8]   Effect of group IV elements on the cutting characteristics of Ti(C,N) cermet tools and reliability analysis [J].
Kwon, WT ;
Park, JS ;
Kang, SH .
JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2005, 166 (01) :9-14
[9]   Effect of WC and group IV carbides on the cutting performance of Ti(C,N) cermet tools [J].
Kwon, WT ;
Park, JS ;
Kim, SW ;
Kang, SH .
INTERNATIONAL JOURNAL OF MACHINE TOOLS & MANUFACTURE, 2004, 44 (04) :341-346
[10]   Reactive sintering of ZrC-TiC composites [J].
Yung, Der-Liang ;
Kollo, Lauri ;
Hussainova, Irina ;
Zikin, Arkadi .
ENGINEERING MATERIALS AND TRIBOLOGY, 2013, 527 :20-25