The manufacture and fatigue cracking resistance of grit free aluminide diffusion coatings

被引:2
|
作者
Warnes, BM
Purvis, AL
Schilbe, JE
机构
[1] Howmet Res Corp, Whitehall, MI 49461 USA
[2] Howmet Thermatech Coatings, Whitehall, MI 49461 USA
来源
关键词
chemical vapor deposition; platinum aluminide; fatigue testing;
D O I
10.1016/S0257-8972(02)00598-4
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Abrasive blasting is an inexpensive and effective means of cleaning superalloy castings, and of roughening the surface of these castings prior to platinum electroplating or overlay coating deposition. However, during the blasting operations, some of the abrasive grit particles become embedded in the surface of the superalloy and this embedded grit can result in detrimental effects on the mechanical properties of gas turbine components. A research program was conducted to evaluate the use of molten caustic immersion to eliminate entrapped grit particles, and to determine the effects of entrapped grit removal on the Thermo-Mechanical Fatigue (TMF) crack resistance of aluminide diffusion coatings. Using aggressive TMF testing conditions, the average life of the samples increased by 47% using the molten caustic immersion to remove the embedded grit particles. The research program is described, the results are presented and discussed and all possible conclusions are summarized. (C) 2002 Elsevier Science B.V. All rights reserved.
引用
收藏
页码:100 / 105
页数:6
相关论文
共 50 条
  • [31] Corrosion resistance of reactive element aluminide diffusion coatings on a nickel-based superalloy and an austenitic stainless steel
    Department of Materials Science and Engineering, University of Toronto, Toronto, Ont., Canada
    不详
    Steel Res. Int., 2007, 1 (58-62):
  • [32] Enhancing steam oxidation resistance of ferritic steels through formation of nickel aluminide diffusion coatings at low temperatures
    Xiang, Z. D.
    Rose, S. R.
    Datta, P. K.
    MANUFACTURING SCIENCE AND ENGINEERING, PTS 1-5, 2010, 97-101 : 1373 - +
  • [33] Corrosion resistance of reactive element aluminide diffusion coatings on a nickel-based superalloy and an austenitic stainless steel
    Elsawy, Abdel Raouf
    Soda, Hiroshi
    McLean, Alexander
    STEEL RESEARCH INTERNATIONAL, 2007, 78 (01) : 58 - 62
  • [34] Thermal cyclic resistance and long term inter-diffusion properties of slurry aluminide coatings modified with Si
    Aguero, Alina
    Ostergard, Maria Jose Landeira
    Hansson, Anette N.
    Gutierrez, Marcos
    RESULTS IN SURFACES AND INTERFACES, 2022, 6
  • [35] Determination of the fatigue behavior of aluminide coatings by means of the impact testing method
    David, C.
    Anthymidis, K. G.
    Agrianidis, P.
    Tsipas, D. N.
    ADVANCES IN FRACTURE AND DAMAGE MECHANICS VI, 2007, 348-349 : 645 - +
  • [36] Resistance of Aluminide Coatings on Austenitic Stainless Steel in a Nitriding Atmosphere
    Wierzbowska, Karolina
    Kochmanska, Agnieszka Elzbieta
    Kochmanski, Pawel
    MATERIALS, 2022, 15 (01)
  • [37] FATIGUE CRACKING IN MATERIALS WITH BRITTLE SURFACE-COATINGS
    SURESH, S
    SUGIMURA, Y
    OGAWA, T
    SCRIPTA METALLURGICA ET MATERIALIA, 1993, 29 (02): : 237 - 242
  • [38] Long term oxidation resistance and thermal stability of Ni-aluminide/Fe-aluminide duplex diffusion coatings formed on ferritic steels at low temperatures
    Xiang, Z. D.
    Rose, S. R.
    Datta, P. K.
    INTERMETALLICS, 2009, 17 (06) : 387 - 393
  • [39] Cyclic oxidation of diffusion aluminide coatings on cobalt base super alloys
    Warnes, BM
    DuShane, NS
    Cockerill, JE
    SURFACE & COATINGS TECHNOLOGY, 2001, 148 (2-3): : 163 - 170
  • [40] SPONTANEOUS FORMATION OF DIFFUSION BARRIERS IN ALUMINIDE COATINGS ON NICKEL-ALLOYS
    FITZER, E
    MAURER, HJ
    ARCHIV FUR DAS EISENHUTTENWESEN, 1978, 49 (02): : 95 - 100