Mechanism and kinetics of the isothermal thermodegradation of ethylene-propylene-diene (EPDM) elastomers

被引:53
作者
Gamlin, CD [1 ]
Dutta, NK [1 ]
Choudhury, NR [1 ]
机构
[1] Univ S Australia, ARC Special Res Ctr, Ian Wark Res Inst, Mawson Lakes, SA 5095, Australia
关键词
EPDM elastomer; isothermal degradation; kinetics of degradation; activation energy; polyolefins; thermogravimetric analysis;
D O I
10.1016/S0141-3910(03)00036-3
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
The thermal degradation behavior of a range of ethylene-propylene-diene (EPDM) elastomers, covering the whole range of composition, has been examined under isothermal conditions between 410 and 44 degreesC using thermogravimetric analysis. The kinetic parameters of degradation for the polymers have been evaluated using different mathematical models based on different proposed mechanisms of degradation. The experimental data were fitted to the models using non-linear regression analysis technique based on Marquardt-Levenberg algorithm. It appears that the degradation of EPDMs follows the Avrami-Erofeev two-dimensional nucleation model or a random chain-scission mechanism. No observable trend was found between the ethylene content of EPDM and the activation energy of degradation. (C) 2003 Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:525 / 531
页数:7
相关论文
共 41 条
[21]   EFFECT OF COMPATIBILISER, CURING SEQUENCE AND AGING ON THE THERMAL-STABILITY OF SILICONE-RUBBER, EPDM RUBBER AND THEIR BLENDS [J].
KOLE, S ;
CHAKI, TK ;
BHOWMICK, AK ;
TRIPATHY, DK .
POLYMER DEGRADATION AND STABILITY, 1993, 41 (01) :109-116
[22]  
KOMAR J, 1994, POLYM DEGRAD STABIL, V43, P209
[23]   Effect of long-term corona on non-ceramic outdoor insulator housing materials [J].
Moreno, VM ;
Gorur, RS .
IEEE TRANSACTIONS ON DIELECTRICS AND ELECTRICAL INSULATION, 2001, 8 (01) :117-128
[24]  
NG WL, 1975, AUST J CHEM, V28, P1169, DOI 10.1071/CH9751169
[25]  
Noordermeer JWM, 1997, CELL POLYM, V16, P331
[26]   EVA-EPDM BLENDS AS CABLE INSULANT [J].
RAY, I ;
KHASTGIR, D .
JOURNAL OF APPLIED POLYMER SCIENCE, 1994, 53 (03) :297-307
[27]   PYROLYSIS OF LINEAR COPOLYMERS OF ETHYLENE AND PROPYLENE [J].
STRAUS, S ;
WALL, LA .
JOURNAL OF RESEARCH OF THE NATIONAL BUREAU OF STANDARDS, 1961, A 65 (03) :221-+
[28]   Application of sepiolite to prevent bleeding and blooming for EPDM rubber composition [J].
Sugiura, M ;
Horii, M ;
Hayashi, H ;
Sasayama, M .
APPLIED CLAY SCIENCE, 1996, 11 (2-4) :89-97
[29]   ENVIRONMENTALLY DURABLE ELASTOMER MATERIALS FOR WINDSHIELD WIPER BLADES [J].
THEODORE, AN ;
SAMUS, MA ;
KILLGOAR, PC .
INDUSTRIAL & ENGINEERING CHEMISTRY RESEARCH, 1992, 31 (12) :2759-2764
[30]   Influence of engine coolant composition on the electrochemical degradation behavior of EPDM radiator hoses [J].
Vroomen, GLM ;
Lievens, SS ;
Maes, JP .
ENGINE COOLANT TESTING: FOURTH VOLUME, 1999, 1335 :183-195