Effects of Cu contents in Pb-free solder alloys on interfacial reactions and bump reliability of Pb-free solder bumps on electroless Ni-P under-bump metallurgy

被引:32
作者
Jeon, YD [1 ]
Paik, KW [1 ]
Ostmann, A [1 ]
Reichl, H [1 ]
机构
[1] Korea Adv Inst Sci & Technol, Dept Mat Sci & Engn, Taejon 305701, South Korea
关键词
Cu content; Pb-free solder; interfacial reactions; electroless Ni-P; under-bump metallurgy (UBM);
D O I
10.1007/s11664-005-0183-5
中图分类号
TM [电工技术]; TN [电子技术、通信技术];
学科分类号
0808 ; 0809 ;
摘要
Using the screen-printed solder-bumping technique on the electroless plated Ni-P under-bump metallurgy (UBM) is potentially a good method because of cost effectiveness. As SnAgCu Pb-free solders become popular, demands for understanding of interfacial reactions between electroless Ni-P UBMs and Cu-containing Pb-free solder bumps are increasing. It was found that typical Ni-Sn reactions between the electroless Ni-P UBM and Sn-based solders were substantially changed by adding small amounts of Cu in Sn-based Pb-free solder alloys. In Cu-containing solder bumps, the (Cu,Ni)(6)Sn-5 phase formed during initial reflow, followed by (Ni,Cu)(3)Sn-4 phase formation during further reflow and aging. The Sn3.5Ag solder bumps showed a much faster electroless Ni-P UBM consumption rate than Cu-containing solder bumps: Sn4.0Ag0.5Cu and Sn0.7Cu. The initial formation of the (Cu,Ni)(6)Sn-5 phase in SnAgCu and SnCu solders significantly reduced the consumption of the Ni-P UBM. The more Cu-containing solder showed slower consumption rate of the Ni-P UBM than the less Cu-containing solder below 300degreesC heat treatments. The growth rate of the (Cu,Ni)(6)Sn-5 intermetallic compound (IMC) should be determined by substitution of Ni atoms into the Cu sublattice in the solid (Cu,Ni)(6)Sn-5 IMC. The Cu contents in solder alloys only affected the total amount of the (Cu,Ni)(6)Sn-5 IMC. More Cu-containing solders were recommended to reduce consumption of the Ni-based UBM. In addition, bump shear strength and failure analysis were performed using bump shear test.
引用
收藏
页码:80 / 90
页数:11
相关论文
共 21 条
[1]   Electromigration effect upon the Sn-0.7 wt% Cu/Ni and Sn-3.5 wt% Ag/Ni interfacial reactions [J].
Chen, CM ;
Chen, SW .
JOURNAL OF APPLIED PHYSICS, 2001, 90 (03) :1208-1214
[2]  
CHONAN Y, 2001, P 7 INT S JWS KOB, P1311
[3]   INTERSTITIAL DIFFUSION OF COPPER IN TIN [J].
DYSON, BF ;
ANTHONY, TR ;
TURNBULL, D .
JOURNAL OF APPLIED PHYSICS, 1967, 38 (08) :3408-&
[4]   Strong effect of Cu concentration on the reaction between lead-free microelectronic solders and Ni [J].
Ho, CE ;
Lin, YL ;
Kao, CR .
CHEMISTRY OF MATERIALS, 2002, 14 (03) :949-+
[5]   Morphology of interfacial reaction between lead-free solders and electroless Ni-P under bump metallization [J].
Jang, JW ;
Frear, DR ;
Lee, TY ;
Tu, KN .
JOURNAL OF APPLIED PHYSICS, 2000, 88 (11) :6359-6363
[6]   Under bump metallurgy study for Pb-free bumping [J].
Jang, SY ;
Wolf, J ;
Paik, KW .
JOURNAL OF ELECTRONIC MATERIALS, 2002, 31 (05) :478-487
[7]   A study on interfacial reactions between electroless Ni-P under bump metallization and 95.5Sn-4.0Ag-0.5Cu alloy [J].
Jeon, YD ;
Nieland, S ;
Ostmann, A ;
Reichl, H ;
Paik, KW .
JOURNAL OF ELECTRONIC MATERIALS, 2003, 32 (06) :548-557
[8]  
Kang SK, 2001, ELEC COMP C, P448, DOI 10.1109/ECTC.2001.927766
[9]  
Lee KY, 2001, ELEC COMP C, P478, DOI 10.1109/ECTC.2001.927770
[10]  
Lide DR, 1995, CRC HDB CHEM PHYSICS, P6