An investigation on the durability properties of RAP-containing roller compacted concrete pavement

被引:12
作者
Abut, Yavuz [1 ]
Yildirim, Salih Taner [2 ]
机构
[1] Kocaeli Metropolitan Municipal, Construct Mat Lab, Dept Transportat, Karabas Mah Salim Dervisoglu Cad 80, TR-41040 Kocaeli, Turkey
[2] Kocaeli Univ, Dept Civil Engn, Fac Engn, Kocaeli, Turkey
关键词
Roller compacted concrete (RCC); reclaimed asphalt pavement (RAP); freeze thaw resistance; durability properties; waste management; ASPHALT PAVEMENT; MECHANICAL-PROPERTIES; ASH; RESISTANCE;
D O I
10.1080/19648189.2019.1679672
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
Use of recycled aggregate in concrete-mix provides many advantages for waste management; more efficient energy and natural resource use, ecological protection, and lower CO2 emissions. This study investigated the use of either 15% or 20% Reclaimed Asphalt Pavement (RAP) by weight in the production of Roller Compacted Concrete (RCC), replacing with coarse aggregate, and the effect on drying deformation and freeze-thaw resistance. After the freeze-thaw cycle, a flexural test was applied to the specimens to investigate the effect of freeze-thaw resistance on the flexural strength of specimens. Drying deformation of the control mixture was found to be 0.05% (500 microstrain) at the end of the 112th day and 600 microstrain in the mixtures containing 15% and 20% RAP. Weight loss was recorded as 2% in all mixtures. An average of 73% of the durability factor was determined in all mixtures at the end of 300 cycles. This study shows that if RAP-containing materials are used up to 20% in the RCC mixture, no significant difference in terms of freeze-thaw resistance occurs. When the effect of the freeze-thaw cycle on flexural strength was investigated, a reducing effect of about 7% in control mixtures and 17?22% in the RAP-containing mixtures was found.
引用
收藏
页码:802 / 818
页数:17
相关论文
共 48 条
[21]  
Hazaree C. V., 2007, THESIS IOWA STATE U
[22]  
HUTCHINSON RL, 1987, CONCRETE INT, V9, P55
[23]  
Jingfu K., 2008, Materials and Structures, V42, P1117, DOI [DOI 10.1617/S11527-008-9447-X, DOI 10.1617/s11527-008-9447-x]
[24]  
Khayat K. H., 2014, R363 NUTC MISS U SCI, P9
[25]  
Khunthongkeaw J, 2003, ACI MATER J, V100, P3
[26]  
Kuzu T., 1990, Proceedings of annual symposium of JCI, V12, P697
[27]  
Liu T. C., 1995, P INT S ROLL COMP CO, V2, P1189
[28]  
LIU TC, 1991, DURABILITY OF CONCRETE, VOLS 1 AND 2, P155
[29]  
Lowe J., 1988, P RCC SPEC C, V1, P1
[30]   The microstructure of dry concrete products [J].
Marchand, J ;
Hornain, H ;
Diamond, S ;
Pigeon, M ;
Guiraud, H .
CEMENT AND CONCRETE RESEARCH, 1996, 26 (03) :427-438