摘要
In the FRIMA salt project in Harlingen (The Netherlands) rock salts of different degrees of purity are produced following the specifications of the clients. The salt plant is fed by solution mining of two caverns, which are located at depths down to 3,050 m. Consequently; they are currently the deepest caverns in the world. The depths of the cavities cause unusual temperature/pressure conditions. There were several factors that in the first phase of sump leaching induced a crystallisation of gypsum in the production annulus of one cavern. To avoid precipitations on the tubing walls it is necessary to distinguish between unchangeable parameters, such as the mineralogical/chemical composition of the salt horizons, and variables, which can be influenced during the leaching process, such as the composition of the solution which is used for the leaching, and the injection pressure which influences the flow rate of the fluids. This paper gives a brief introduction of the technical data of the FRIMA Zoutindustrie project. Afterwards, the processes that induce the gypsum crystallisation are discussed in context with the geochemical fundamentals of the ternary system NaCl-CaSO4-H2O.
引用
收藏
页码:265 / 270
页数:6
相关论文
共 50 条
  • [21] Thermoluminescence emission, excitation and stimulation spectra of CaSO4:Dy and CaSO4:Tm
    Lewandowski, AC
    Barkyoumb, JH
    Mathur, VK
    RADIATION PROTECTION DOSIMETRY, 1996, 65 (1-4) : 281 - 286
  • [22] The thermal behaviour of γ-CaSO4
    Ballirano, Paolo
    Melis, Elisa
    PHYSICS AND CHEMISTRY OF MINERALS, 2009, 36 (06) : 319 - 327
  • [23] Kinetics Study on the Effect of NaCl on the CaSO4 Dissolution Behavior
    Song, Jingyao
    Shi, Peiyang
    Wang, Yeguang
    Jiang, Maofa
    5TH ANNUAL INTERNATIONAL CONFERENCE ON MATERIAL SCIENCE AND ENVIRONMENTAL ENGINEERING (MSEE2017), 2018, 301
  • [24] Recombination luminescence in CaSO4
    Salikhodzha, Zh. M.
    Nurakhmetov, T. N.
    Akilbekov, A. T.
    Zhunusbekov, A. M.
    Kainarbay, A. Zh.
    Sadykova, B. M.
    Daurenbekov, D. H.
    Zhangylysov, K. B.
    RADIATION MEASUREMENTS, 2019, 125 : 19 - 24
  • [25] Thermal Stabilisation of CaSO4
    Tsoumeleas, C.I.
    Katsioti, M.
    Georgali, B.
    Marinos, J.
    World Cement, 2000, 31 (11): : 57 - 61
  • [26] Thermal stabilization of CaSO4
    Tsomeleas, C.I.
    Katsioti, M.
    Georgali, B.
    Marinos, J.
    World Cement, 2000, 31 (11):
  • [27] CASO4 POLYMORPHIC MODIFICATIONS
    BUSHUEV, NN
    FROLOVA, NG
    NOSOV, VN
    KARMYSHOV, VF
    ZHURNAL NEORGANICHESKOI KHIMII, 1978, 23 (12): : 3383 - 3384
  • [28] The thermal behaviour of γ-CaSO4
    Paolo Ballirano
    Elisa Melis
    Physics and Chemistry of Minerals, 2009, 36 : 319 - 327
  • [29] 脱硫石膏制备γ-CaSO4晶须及Ⅱ-CaSO4晶须
    马文静
    陈学青
    郜丽丽
    李雲
    郭宏飞
    李治水
    曹吉林
    高校化学工程学报, 2021, 35 (03) : 520 - 528
  • [30] Induction times induced in an RO system by antiscalants delaying CaSO4 precipitation
    Hasson, D
    Drak, A
    Semiat, R
    DESALINATION, 2003, 157 (1-3) : 193 - 207