Effect of Fe-rich intermetallics on the wear behavior of eutectic Al-Si piston alloy (LM13)

被引:53
作者
Abouei, V. [1 ]
Saghafian, H. [1 ]
Shabestari, S. G. [1 ]
Zarghami, M. [2 ]
机构
[1] Iran Univ Sci & Technol, Sch Met & Mat Engn, Ctr Excellence Adv Mat Proc, Tehran 1684613114, Iran
[2] Supplying Automot Parts Co, Tehran, Iran
关键词
ALUMINUM-ALLOY; IRON; SOLIDIFICATION; PARAMETERS; PHASES; CAST;
D O I
10.1016/j.matdes.2010.02.015
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In the present study, the effect of Fe-rich intermetallics has been investigated on the wear behavior of eutectic Al-Si alloy (LM13). Dry sliding wear tests have been conducted using a pin-on-disk machine under different normal loads of 18, 51, 74 and 100 N at a constant sliding speed of 0.3 m/s. Addition of 1.2% Fe to the LM13 alloy leads to the formation of the flake like 8-intermetallic compounds. These hard compounds initiate micro cracks and can reduce the wear resistance of the alloy. The addition of Mn converts the flake like beta-intermetallic compounds to the star-like alpha-intermetallics and decreases the detrimental effect of iron. Applying high cooling rate during solidification of the alloy containing Fe and Mn, resulted to the formation of finer alpha-intermetallic compounds and improved the wear behavior of the alloy to a great extent. (c) 2010 Elsevier Ltd. All rights reserved.
引用
收藏
页码:3518 / 3524
页数:7
相关论文
共 29 条
  • [1] An investigation of the wear behaviour of 0.2%C dual phase steels
    Abouei, V.
    Saghafian, H.
    Kheirandish, Sh.
    Ranjbar, Kh.
    [J]. JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2008, 203 (1-3) : 107 - 112
  • [2] Effect of microstructure on the oxidative wear behavior of plain carbon steel
    Abouei, V.
    Saghafian, H.
    Kheirandish, Sh.
    [J]. WEAR, 2007, 262 (9-10) : 1225 - 1231
  • [3] *AM SOC MET, 1992, ASM HDB, V18
  • [4] Influence of Sr and Mn additions on intermetallic compound morphologies in Al-Si-Cu-Fe cast alloys
    Ashtari, P
    Tezuka, H
    Sato, T
    [J]. MATERIALS TRANSACTIONS, 2003, 44 (12) : 2611 - 2616
  • [5] Belov N.A., 2002, IRON ALUMINUM ALLOYS
  • [6] Effect of cooling rate on the solidification behaviour of Al-Fe-Si alloys
    Dutta, B
    Rettenmayr, M
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2000, 283 (1-2): : 218 - 224
  • [7] EYRE TS, 1976, TRIBOL INT, V9, P1
  • [8] Gruzleski J.E., 1990, TREATMENT LIQUID ALU, P1
  • [9] Study on wear properties of aluminium-silicon piston alloy
    Haque, MM
    Sharif, A
    [J]. JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2001, 118 (1-3) : 69 - 73
  • [10] HURAN M, 1996, WEAR, V194, P54