Effects of critical defects on stress corrosion cracking of Al-Zn-Mg-Cu-Zr alloy

被引:26
|
作者
Sun, Yuanwei [1 ]
Pan, Qinglin [2 ]
Lin, Sen [3 ]
Zhao, Xiangjin [1 ]
Liu, Zhongli [1 ]
Li, Weijian [1 ]
Wang, Guiquan [1 ]
机构
[1] Yantai Univ, Sch Nucl Equipment & Engn, Yantai 264000, Peoples R China
[2] Cent South Univ, Sch Mat Sci & Engn, Changsha 410083, Peoples R China
[3] CRRC Qingdao Sifang Co Ltd, Qingdao 266000, Peoples R China
关键词
Al-Zn-Mg-Cu-Zr alloy; Critical defects; Stress corrosion cracking propagation; Cu content; Al7Cu2Fe particle; HYDROGEN EMBRITTLEMENT; ANODIC-DISSOLUTION; ALUMINUM-ALLOYS; HEAT-TREATMENTS; BEHAVIOR; MICROSTRUCTURE; PARTICLES; AIRCRAFT; MICROCHEMISTRY; RESISTANCE;
D O I
10.1016/j.jmrt.2021.03.070
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The effects of critical defects on stress corrosion cracking (SCC) of Al-7.82Zn-1.99Mg-2.41Cu-0.12Zr alloy under under-ageing (UA), peak-ageing (PA) double-ageing (DA) and retrogression and reageing (RRA) were investigated. It is found that anodic dissolution of grain boundary precipitates (GBPs) for UA sample generates critical defects due to low Cu content of GBPs, whereas the dissolution of Al, Mg and Zn elements within the grain interior is responsible for the formation of critical defects for PA, DA and RRA samples. The high distribution continuity of GBPs promotes the continuous propagation of stress corrosion crack along grain boundary, leading to intergranular SCC for UA sample. Coarsened GBPs which are distributed discontinuously could hinder anodic dissolution along the grain boundary. As a result, the cracks propagate along the grain interior, causing transgranular SCC for DA sample. And large size and low density of matrix precipitates (MPTs) decease SCC susceptibility. Al7Cu2Fe particles promote the dissolution of the surrounding matrix, inducing local stress concentration, and thus leading to the generation of stress corrosion cracks. (C) 2021 The Authors. Published by Elsevier B.V.
引用
收藏
页码:1303 / 1318
页数:16
相关论文
共 50 条
  • [31] STRESS CORROSION CRACKING OF AN AL-ZN-MG-CU ALLOY/ CORROSAOSOB TENSAO DE UMA LIGA AL-ZN-MG-CU.
    CARDOSO, ALVARO AZEVEDO
    1982, V 38 (N 297): : 469 - 472
  • [32] Effects of Deformation Modes on Texture Evolution during Hot Working of Al-Zn-Mg-Cu-Zr Alloy
    赵晓东
    LU Ruilong
    LIN Jinbao
    陈慧琴
    JournalofWuhanUniversityofTechnology(MaterialsScience), 2016, 31 (03) : 616 - 623
  • [33] Effects of Deformation Modes on Texture Evolution during Hot Working of Al-Zn-Mg-Cu-Zr Alloy
    Zhao Xiaodong
    Lu Ruilong
    Lin Jinbao
    Chen Huiqin
    JOURNAL OF WUHAN UNIVERSITY OF TECHNOLOGY-MATERIALS SCIENCE EDITION, 2016, 31 (03): : 616 - 623
  • [34] Effects of minor Er and Y addition to Al-Zn-Mg-Cu-Zr alloy on microstructures and mechanical properties
    Li, Guo-Feng
    Zhang, Xin-Ming
    Zhu, Hang-Fei
    Cailiao Gongcheng/Journal of Materials Engineering, 2010, (05): : 78 - 82
  • [35] Effects of deformation modes on texture evolution during hot working of Al-Zn-Mg-Cu-Zr alloy
    Xiaodong Zhao
    Ruilong Lu
    Jinbao Lin
    Huiqin Chen
    Journal of Wuhan University of Technology-Mater. Sci. Ed., 2016, 31 : 616 - 623
  • [36] The Effect of Planar Solidification on Mechanical Properties of Al-Zn-Mg-Cu-Zr Alloy Plate
    Hosch, T.
    Chu, M. G.
    Feyen, G.
    Rioja, R. J.
    Cassada, W. A.
    PROCEEDINGS OF THE 13TH INTERNATIONAL CONFERENCE ON ALUMINUM ALLOYS (ICAA13), 2012, : 1377 - 1382
  • [37] Portevin-Le Chatelier effect in Al-Zn-Mg-Cu-Zr aluminum alloy
    陈军洲
    甄良
    樊立伟
    杨守杰
    戴圣龙
    邵文柱
    TransactionsofNonferrousMetalsSocietyofChina, 2009, 19 (05) : 1071 - 1075
  • [38] Influence of quench on ageing response and mechanical properties of Al-Zn-Mg-Cu-Zr alloy
    Fan, XG
    Jiang, DM
    Meng, QC
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2005, 15 : 18 - 22
  • [39] Microstructure and properties of Al-Zn-Mg-Cu-Zr alloy prepared by spray deposition method
    School of Materials Science and Engineering, Central South University, Changsha
    410083, China
    不详
    410083, China
    Zhongguo Youse Jinshu Xuebao, 7 (1773-1780):
  • [40] Precipitation Behavior and Quenching Sensitivity of a Spray Deposited Al-Zn-Mg-Cu-Zr Alloy
    Sheng, Xiaofei
    Lei, Qian
    Xiao, Zhu
    Wang, Mingpu
    MATERIALS, 2017, 10 (09)