Marine Fouling Release Silicone/Carbon Nanotube Nanocomposite Coatings: On the Importance of the Nanotube Dispersion State

被引:47
作者
Beigbeder, Alexandre [1 ]
Mincheva, Rosica [1 ]
Pettitt, Michala E. [2 ]
Callow, Maureen E. [2 ]
Callow, James A. [2 ,3 ]
Claes, Michael
Dubois, Philippe [1 ]
机构
[1] Univ Mons, Acad Univ Wallonie Bruxelles, Lab Polymer & Composite Mat, CIRMAP, B-7000 Mons, Belgium
[2] Univ Birmingham, Sch Biosci, Birmingham B15 2TT, W Midlands, England
[3] Nanocyl SA, B-5060 Sambreville, Belgium
关键词
Nanocomposites; PDMS; Carbon Nanotubes; Antifouling; Fouling Release; Alga; CARBON NANOTUBE; SILICATE NANOCOMPOSITES; POLYMERIZATION;
D O I
10.1166/jnn.2010.2185
中图分类号
O6 [化学];
学科分类号
0703 ;
摘要
The present work reports on the influence of the dispersion quality of multiwall carbon nanotubes (MWCNTs) in a silicone matrix on the marine fouling-release performance of the resulting nanocomposite coatings. A first set of coatings filled with different nanofiller contents was prepared by the dilution of a silicone/MWCNTs masterbatch within a hydrosilylation-curing polydimethylsiloxane resin. The fouling-release properties of the nanocomposite coatings were studied through laboratory assays with the marine alga (seaweed) Ova, a common fouling species. As reported previously (see Ref. [19]), the addition of a small (0.05%) amount of carbon nanotubes substantially improves the fouling-release properties of the silicone matrix. This paper shows that this improvement is dependent on the amount of filler, with a maximum obtained with 0.1 wt% of multiwall carbon nanotubes (MWCNTs). The method of dispersion of carbon nanotubes in the silicone matrix is also shown to significantly (p = 0.05) influence the fouling-release properties of the coatings. Dispersing 0.1% MWCNTs using the masterbatch approach yielded coatings with circa 40% improved fouling-release properties over those where MWCNTs were dispersed directly in the polymeric matrix. This improvement is directly related to the state of nanofiller dispersion within the cross-linked silicone coating.
引用
收藏
页码:2972 / 2978
页数:7
相关论文
共 25 条
[1]   Polymer-layered silicate nanocomposites: Preparation, properties and uses of a new class of materials [J].
Alexandre, Michael ;
Dubois, Philippe .
Materials Science and Engineering: R: Reports, 2000, 28 (1-2) :1-63
[2]  
BEIGBEDER A, 2008, Patent No. 2008046166
[3]  
BEIGBEDER A, 2009, 5 ECNP INT C NAN MUL
[4]  
Beigbeder A., 2009, J. Nanostruct. Polym. Nanocompos, V5, P37
[5]   Preparation and characterisation of silicone-based coatings filled with carbon nanotubes and natural sepiolite and their application as marine fouling-release coatings [J].
Beigbeder, Alexandre ;
Degee, Philippe ;
Conlan, Sheelagh L. ;
Mutton, Robert J. ;
Clare, Anthony S. ;
Pettitt, Michala E. ;
Callow, Maureen E. ;
Callow, James A. ;
Dubois, Philippe .
BIOFOULING, 2008, 24 (04) :291-302
[6]   CH-π interactions as the driving force for silicone-based nanocomposites with exceptional properties [J].
Beigbeder, Alexandre ;
Linares, Mathielt ;
Devalckenaere, Myriam ;
Degee, Philippe ;
Claes, Michael ;
Beljonne, David ;
Lazzaroni, Roberto ;
Dubois, Philippe .
ADVANCED MATERIALS, 2008, 20 (05) :1003-+
[7]   Multiwall carbon nanotube elastomeric composites: A review [J].
Bokobza, Liliane .
POLYMER, 2007, 48 (17) :4907-4920
[8]   Mechanical, electrical and spectroscopic investigations of carbon nanotube-reinforced elastomers [J].
Bokobza, Liliane .
VIBRATIONAL SPECTROSCOPY, 2009, 51 (01) :52-59
[9]   From carbon nanotube coatings to high-performance polymer nanocomposites [J].
Bredeau, Stephane ;
Peeterbroeck, Sophie ;
Bonduel, Daniel ;
Alexandre, Michael ;
Dubois, Philippe .
POLYMER INTERNATIONAL, 2008, 57 (04) :547-553
[10]   Ethylene-norbornene copolymerization by carbon nanotube-supported metallocene catalysis: Generation of high-performance polyolefinic, nanocomposites [J].
Bredeau, Stephane ;
Boggioni, Laura ;
Bertini, Fabio ;
Tritto, Incoronata ;
Monteverde, Fabien ;
Alexandre, Michael ;
Dubois, Philippe .
MACROMOLECULAR RAPID COMMUNICATIONS, 2007, 28 (07) :822-827