Sagging Mechanisms of Three-Layer Aluminum Clad Foils used in the Heat Exchanger in the Brazing Process

被引:2
作者
Tang, Chao-lan [1 ]
Xu, Qiu-ping [1 ]
Guo, Xiao-feng [1 ]
Chen, Xin [2 ,3 ]
Liu, Can-wei [2 ,3 ]
Li, Long [2 ,3 ]
Zhou, De-jing [2 ,3 ]
机构
[1] Guangdong Univ Technol, Sch Electromech Engn, Guangzhou 510006, Guangdong, Peoples R China
[2] Jiangsu Key Lab Clad Mat, Wuxi 214145, Peoples R China
[3] Yin Bang Clad Mat Co Ltd, Wuxi 214145, Peoples R China
关键词
aluminum brazing clad foils; erosion; final rolling reduction; recovery; sagging resistance; DEFORMED ALUMINUM; BRAZEABILITY; ALLOYS; SHEETS; RESISTANCE; BEHAVIOR; STRESS;
D O I
10.1007/s11665-018-3548-7
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The sagging mechanisms of a three-layer aluminum clad foils (AA4343/AA3003Mod/AA4343) with final rolling reduction of 20-50% during brazing were studied. The results show that the sagging behavior of the aluminum brazed foils during the brazing cycle can be divided into four stages: Stage I is the slight sagging stage, during which sagging deformation can almost be ignored; Stage II is referred to as the accelerative sagging stage, and the sagging behavior is mainly ascribed to recovery. In stage II, the greater the reduction ratio is, the earlier the recovery ends, and the smaller the value of the sagging distance is. Stage III is the slow sagging stage, and sliding deformation along the grain boundaries is responsible for the slow sagging rate. Stage IV is the erosion stage. During stage IV, the coarsely recrystallized grains can inhibit erosion and are helpful in obtaining excellent sagging resistance, while the foils with finely recrystallized grains or non-recrystallized structure show severe erosion and limited sagging resistance.
引用
收藏
页码:4846 / 4854
页数:9
相关论文
共 5 条
[1]   Sagging Mechanisms of Three-Layer Aluminum Clad Foils used in the Heat Exchanger in the Brazing Process [J].
Chao-lan Tang ;
Qiu-ping Xu ;
Xiao-feng Guo ;
Xin Chen ;
Can-wei Liu ;
Long Li ;
De-jing Zhou .
Journal of Materials Engineering and Performance, 2018, 27 :4846-4854
[2]   Sagging mechanisms in the brazing of aluminum heat exchangers [J].
Qin, Jining ;
Kang, Suk-Bong ;
Cho, Jae-Hyung .
SCRIPTA MATERIALIA, 2013, 68 (12) :941-944
[3]   Effects of annealing process on sagging resistance of cold-rolled three-layer Al alloy clad sheets [J].
Zhao, Yuan-yuan ;
Zhang, Zhen-yan ;
Jin, Li ;
Dong, Jie .
TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2016, 26 (10) :2542-2551
[4]   Fabrication and brazeability of a three-layer 4343/3003/4343 aluminum clad sheet by rolling [J].
Yoon, JS ;
Lee, SH ;
Kim, MS .
JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2001, 111 (1-3) :85-89
[5]   Deformation and heat treatment ability of three-layer 6009/7050/6009 Al alloy clad slab prepared by direct-chill casting [J].
Yan, Guang-yuan ;
Mao, Feng ;
Cao, Zhi-qiang ;
Li, Ting-ju ;
Wang, Tong-min .
TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2018, 28 (01) :9-19