Mechanism of a single layer 193 nm dissolution inhibition resist

被引:5
|
作者
Yan, ZL [1 ]
Houlihan, FM [1 ]
Reichmanis, E [1 ]
Nalamasu, O [1 ]
Reiser, A [1 ]
Dabbagh, G [1 ]
Hutton, RS [1 ]
Osei, D [1 ]
Sousa, J [1 ]
Bolan, KJ [1 ]
机构
[1] Polytech Univ, Inst Imaging Sci, Brooklyn, NY 11201 USA
关键词
193; nm; dissolution inhibitor; cycloolefin polymer;
D O I
10.1117/12.388275
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
We have found that the progress of developer base into films of terpolymers of norbornene (NB)-maleic anhydride (MA) and acrylic acid (AA) is a percolation process with a critical site concentration of x(c) = 0.084 which suggests that every acrylic acid site in the terpolymer of norbomene-maleic anhydride-acrylic acid can make 12 monomer units of the polymer water compatible. In practice these systems are being used with various tert-butyl esters of cholic acid as dissolution inhibitors. The cholates differ very much in their dissolution inhibition factors (lowest t-butyl cholate (1.3) to highest t-butyl lithocholate glutarate dimer(7.4). The change in these factors corrected for molarity follow the hydrophobic character of the dissolution as measured by log(p). A quick screening method has also been established to evaluate dissolution inhibitors based on our observation that the cloud point (the volume % acetone in a water/acetone which gives persistent cloudiness) parallels the dissolution inhibiting power as measured by the dissolution inhibition factor. For dissolution promotion, optimal results are obtained with t-butyl 1,3,5-cyclohexanetricarboxylate (f=-6.3) and poorest results with t-butyl lithocholate (f=-2.8); this appears to track with the number of carboxyl groups and the hydrophobicity of the carboxylic acids. The R-max found for resist formulations tracks well with these findings. Another factor in determining the ultimate achievable contrast is the degree of acidolytic deprotection achieved by the material. It appears that acidolyticaly cleaveable carboxylate esters with a higher concentration of electron withdrawing groups such as t-butyl 1,3,5-cyclohexanetricasboxylate are more effective.
引用
收藏
页码:127 / 135
页数:3
相关论文
共 50 条
  • [21] Resist challenges for 193nm lithography.
    Bowden, MJ
    ABSTRACTS OF PAPERS OF THE AMERICAN CHEMICAL SOCIETY, 1999, 217 : U427 - U427
  • [22] Resist component leaching in 193 nm immersion lithography
    Dammel, RR
    Pawlowski, G
    Romano, A
    Houlihan, FM
    Kim, WK
    Sakamuri, R
    Abdallah, D
    Advances in Resist Technology and Processing XXII, Pt 1 and 2, 2005, 5753 : 95 - 101
  • [23] High index resist for 193 nm immersion lithography
    Matsumoto, Kazuya
    Costner, Elizabeth A.
    Nishimura, Isao
    Ueda, Mitsuru
    Willson, C. Grant
    MACROMOLECULES, 2008, 41 (15) : 5674 - 5680
  • [24] Bilayer resist approach for 193-nm lithography
    Schaedeli, U
    Tinguely, E
    Blakeney, AJ
    Falcigno, P
    Kunz, RR
    ADVANCES IN RESIST TECHNOLOGY AND PROCESSING XIII, 1996, 2724 : 344 - 354
  • [25] Evolution of a 193nm bilayer resist for manufacturing
    Kwong, R
    Khojasteh, M
    Lawson, P
    Hughes, T
    Varanasi, PR
    Brunsvold, B
    Allen, R
    Brock, P
    Sooriyakumaran, R
    Truong, H
    ADVANCES IN RESIST TECHNOLOGY AND PROCESSING XIX, PTS 1 AND 2, 2002, 4690 : 403 - 409
  • [26] Analyzing and characterizing 193nm resist shrinkage
    Su, B
    Eytan, G
    Padmanaban, M
    Romano, A
    SOLID STATE TECHNOLOGY, 2001, 44 (05) : 52 - +
  • [27] Comparison of resist collapse properties for deep ultraviolet and 193 nm resist platforms
    Cao, HB
    Nealey, PF
    Domke, WD
    JOURNAL OF VACUUM SCIENCE & TECHNOLOGY B, 2000, 18 (06): : 3303 - 3307
  • [28] Dissolution behavior of chemically amplified resist polymers for 248-, 193-, and 157-nm lithography
    Ito, H
    IBM JOURNAL OF RESEARCH AND DEVELOPMENT, 2001, 45 (05) : 683 - 695
  • [29] Dissolution behavior of chemically amplified resist polymers for 248-, 193-, and 157-nm lithography
    Ito, H.
    1600, IBM Corporation (45):
  • [30] Novel single-layer photoresist containing cycloolefins for 193 nm
    Park, JH
    Seo, DC
    Kim, KD
    Park, SY
    Kim, SJ
    Lee, W
    Jung, JC
    Bok, CK
    Baik, KH
    ADVANCES IN RESIST TECHNOLOGY AND PROCESSING XV, PTS 1 AND 2, 1998, 3333 : 454 - 462