Microstructure and mechanical properties of Ti3SiC2/Ti3SiC2 diffusion bonded joints using Ti foil as an interlayer

被引:21
|
作者
Wang, Y. [1 ]
Wu, X. F. [1 ]
Yang, Z. W. [1 ]
Xia, Y. H. [1 ]
Wang, D. P. [1 ]
机构
[1] Tianjin Univ, Tianjin Key Lab Adv Joining Technol, Sch Mat Sci & Engn, Tianjin 300350, Peoples R China
基金
中国国家自然科学基金;
关键词
Diffusion bonded joint; Ti3SiC2; ceramic; Microstructure; Mechanical property; INTERFACIAL MICROSTRUCTURE; M(N+1)AX(N) PHASES; TI3SIC2; ALLOY; AL; GROWTH; EVOLUTION; TI3ALC2; NB; ZR;
D O I
10.1016/j.ceramint.2019.07.079
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Diffusion bonded joints of Ti3SiC2 ceramic without or with a Ti foil were fabricated. The effects of temperature, holding time and Ti foil thickness on the microstructural evolution and mechanical properties of Ti3SiC2/Ti/Ti3SiC2 joints were systematically investigated. Compared with the case of direct diffusion joints, the Ti3SiC2/Ti/Ti3SiC2 joint was obtained at 1000 degrees C and the bonding temperature reduced by 150 degrees C. The typical microstructure of the Ti3SiC2/Ti/Ti3SiC2 joints obtained at 1100 degrees C with a 60-mu m thick Ti foil for 60 min consisted of Ti3SiC2/Ti(5)Si(3)c/TiSi/Ti5Si4/TiAl2/TiAl/ Ti3Al/alpha-Ti/Ti3Al/TiAl/TiAl2/Ti5Si4/TiSi/Ti5Si3Cx/Ti3SiC2 layers in that order. The formation sequence of the diffusion layer at the joint was TiAl2 -> TiSi -> Ti5Si3 -> Ti5Si4 -> TiAl -> Ti3Al. Upon changing the bonding temperature from 1000 to 1150 degrees C, the thickness of the Ti foil from 0 to 120 mu m and the holding time from 30 to 120 min, the shear strength first increased and then decreased. The shear strength of the Ti3SiC2/Ti/Ti3SiC2 joint at 1100 degrees C for 60 min under 20 MPa reached 174 +/- 4 MPa, which was 1.87 times that of the direct diffusion joint under the same experimental conditions. The results of Vickers microhardness measurements showed that the Ti5Si4 and TiSi compounds exhibited the highest microhardness of 853 43HV. The fractures caused by Ti(5S)i(4) and TiSi propagated into the Ti5Si3Cx, Ti3SiC2 and Ti-Al diffusion layers.
引用
收藏
页码:20900 / 20909
页数:10
相关论文
共 50 条
  • [21] Preparation of Ti3SiC2
    P. V. Istomin
    A. V. Nadutkin
    Yu. I. Ryabkov
    B. A. Goldin
    Inorganic Materials, 2006, 42 : 250 - 255
  • [22] Polymorphism of Ti3SiC2
    Yu, R
    Zhan, Q
    He, LL
    Zhou, YC
    Ye, HQ
    JOURNAL OF MATERIALS RESEARCH, 2002, 17 (05) : 948 - 950
  • [23] Structure of Ti3SiC2
    Rawn, CJ
    Payzant, EA
    Hubbard, CR
    Barsoum, MW
    El-Raghy, T
    EUROPEAN POWDER DIFFRACTION, PTS 1 AND 2, 2000, 321-3 : 889 - 892
  • [24] Ti3SiC2 and ice
    Barsoum, MW
    Radovic, M
    Finkel, P
    El-Raghy, T
    APPLIED PHYSICS LETTERS, 2001, 79 (04) : 479 - 481
  • [25] Effect of Processing Condition on the Microstructure and Mechanical Properties of Ti3SiC2/SiC Composites
    Yin, Hongfeng
    Lu, Linlin
    ECO-MATERIALS PROCESSING AND DESIGN XI, 2010, 658 : 352 - 355
  • [26] Preparation of Ti3SiC2
    Istomin, PV
    Nadutkin, AV
    Ryabkov, YI
    Goldin, BA
    INORGANIC MATERIALS, 2006, 42 (03) : 250 - 255
  • [27] CVD of Ti3SiC2
    Pickering, E
    Lackey, WJ
    Crain, S
    CHEMICAL VAPOR DEPOSITION, 2000, 6 (06) : 289 - 295
  • [28] CVD of Ti3SiC2
    Pickering, E.
    Lackey, W.J.
    Crain, S.
    Advanced Materials, 2000, 12 (22) : 289 - 295
  • [29] Fabrication and Properties of Ti3SiC2/SiC Composites
    YIN Hongfeng
    China'sRefractories, 2008, (01) : 10 - 13
  • [30] Fabrication of SiCf/Ti3SiC2 by the electrophoresis of highly dispersed Ti3SiC2 powder
    Kwon, Heejin
    Zhou, Xiaobing
    Yoon, Dang-Hyok
    CERAMICS INTERNATIONAL, 2020, 46 (11) : 18168 - 18174