Microstructure and creep properties of Sn-Ag-Cu lead-free solders bearing minor amounts of the rare earth cerium

被引:20
|
作者
Zhang, Liang [1 ]
Xue, Song-bai [1 ]
Gao, Li-li [1 ]
Chen, Yan [2 ]
Yu, Sheng-lin [1 ,3 ]
Sheng, Zhong [1 ]
Zeng, Guang [1 ]
机构
[1] Nanjing Univ Aeronaut & Astronaut, Coll Mat Sci & Technol, Nanjing 210016, Peoples R China
[2] Harbin Welding Inst, Harbin, Peoples R China
[3] China Elect Technol Grp Corp, Res Inst 14, Nanjing, Peoples R China
关键词
Solders; Alloys; Mechanical properties of materials; Thermodynamics; Creep; Chemical elements and inorganic compounds; MECHANICAL-PROPERTIES; INTERMETALLIC COMPOUNDS; INDENTATION CREEP; ALLOYS; NI; COMPOUND; BEHAVIOR; GROWTH; SOLDERABILITY; JOINTS;
D O I
10.1108/09540911011036262
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Purpose - The purpose of this paper is to investigate the effects of minor addition of the rare earth (RE) element cerium, Cc, on the microstructures and creep properties of Sn-Ag-Cu solder alloys. Design/methodology/approach - The pure Sn, Sn-Cu alloy, Sn-Ag alloy and Cu-Ce alloy were used as raw materials. Sn-Ag-Cu alloys with different contents of RE Cc were chosen to compare with Sn-Ag-Cu. The raw materials of Sn, Sn-Cu alloy, Sn-Ag alloy, Cu-Ce alloy were melted in a ceramic crucible, and were melted at 550 degrees C +/- 1 degrees C for 40 minutes. To homogenize the solder alloy, mechanical stirring was performed every ten minutes using a glass rod. During the melting, KG + LiCl (1.11), were used over the surface of liquid solder to prevent oxidation. The melted solder was chill cast into a rod. Findings - It is found that the microstructure exhibits smaller grains and the A0n/CU6Sn5 intermetallic compound (IMC) phases are modified in matrix with the addition of Cc. In particular, the addition of 0.03 wt.% Cc to the Sn-Ag-Cu solder can refine the microstructures and decrease the thickness of the IMC layers of Sn-Ag-Cu solder alloys. Meanwhile, thermodynamic analysis showed that these phenomena could be attributed to the reduction of the driving force for Cu-Sn IMC formation due to the addition of Cc. Results calculated using the thermodynamic method are close to the above experimental data. Thus, the optimum content of Cc in Sn-Ag-Cu solder alloys should be about 0.030 percent. Additionally, the effect of Cc on the creep rupture life of Sn-Ag-Cu soldered joints was studied. It was found that the creep rupture life may be increased up to 7.5 times more than that of the original Sn-Ag-Cu alloy, when Cc accounts for 0.030 percent. Originality/value - This paper usefully investigates the effects of the RE cerium (Cc), on the microstructures and creep properties of Sn-Ag-Cu solder alloys, optimizing the quantity of Cc in the Sn-Ag-Cu solder alloy through a thermodynamic method and by creep-rupture life testing.
引用
收藏
页码:30 / 36
页数:7
相关论文
共 50 条
  • [31] Effect of graphene nanosheets reinforcement on the performance of Sn-Ag-Cu lead-free solder
    Liu, X. D.
    Han, Y. D.
    Jing, H. Y.
    Wei, J.
    Xu, L. Y.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2013, 562 : 25 - 32
  • [32] Evolution of thermal property and creep resistance of Ni and Zn-doped Sn-2.0Ag-0.5Cu lead-free solders
    El-Daly, A. A.
    El-Taher, A. M.
    MATERIALS & DESIGN, 2013, 51 : 789 - 796
  • [33] Nanoindentation Creep Behavior of Nanocomposite Sn-Ag-Cu Solders
    Roshanghias, A.
    Kokabi, A. H.
    Miyashita, Y.
    Mutoh, Y.
    Ihara, I.
    Fatt, R. G. Guan
    Madaah-Hosseini, H. R.
    JOURNAL OF ELECTRONIC MATERIALS, 2012, 41 (08) : 2057 - 2064
  • [34] Creep Behavior of Lead-Free Sn-Ag-Cu + Ni-Ge Solder Alloys
    N. Hidaka
    H. Watanabe
    M. Yoshiba
    Journal of Electronic Materials, 2009, 38 : 670 - 677
  • [35] Microstructure evolution and mechanical properties of Sn0.7Cu0.7Bi lead-free solders produced by directional solidification
    Hu, Xiaowu
    Li, Ke
    Min, Zhixian
    JOURNAL OF ALLOYS AND COMPOUNDS, 2013, 566 : 239 - 245
  • [36] Prediction of activities of all components in Sn-Ag-Cu and Sn-Ag-Cu-Zn lead-free solders using modified molecular interaction volume model
    You, Yanjun
    Kong, Lingxin
    Xu, Junjie
    Xu, Baoqiang
    Liu, Ganggang
    Yang, Bin
    RESULTS IN CHEMISTRY, 2021, 3
  • [37] Creep properties and microstructure of the Sn-Ag-Cu-Ni-Ge lead-free solder alloy
    Hidaka, Noboru
    Nagano, Megumi
    Shimoda, Masayoshi
    Watanabe, Hirohiko
    Ono, Masahiro
    ADVANCES IN ELECTRONIC PACKAGING 2005, PTS A-C, 2005, : 1805 - 1810
  • [38] Study on melt properties, microstructure, tensile properties of low Ag content Sn-Ag-Zn Lead-free solders
    Luo, Tingbi
    Chen, Zhuo
    Hu, Anmin
    Li, Ming
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2012, 556 : 885 - 890
  • [39] Effects of Ag contents in Sn-xAg lead-free solders on microstructure, corrosion behavior and interfacial reaction with Cu substrate
    Tunthawiroon, Phacharaphon
    Kanlayasiri, Kannachai
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2019, 29 (08) : 1696 - 1704
  • [40] Study of mechanical properties of Ag nanoparticle-modified graphene/Sn-Ag-Cu solders by nanoindentation
    Han, Y. D.
    Gao, Y.
    Zhang, S. T.
    Jing, H. Y.
    Wei, J.
    Zhao, L.
    Xu, L. Y.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2019, 761