Microstructure and creep properties of Sn-Ag-Cu lead-free solders bearing minor amounts of the rare earth cerium

被引:20
|
作者
Zhang, Liang [1 ]
Xue, Song-bai [1 ]
Gao, Li-li [1 ]
Chen, Yan [2 ]
Yu, Sheng-lin [1 ,3 ]
Sheng, Zhong [1 ]
Zeng, Guang [1 ]
机构
[1] Nanjing Univ Aeronaut & Astronaut, Coll Mat Sci & Technol, Nanjing 210016, Peoples R China
[2] Harbin Welding Inst, Harbin, Peoples R China
[3] China Elect Technol Grp Corp, Res Inst 14, Nanjing, Peoples R China
关键词
Solders; Alloys; Mechanical properties of materials; Thermodynamics; Creep; Chemical elements and inorganic compounds; MECHANICAL-PROPERTIES; INTERMETALLIC COMPOUNDS; INDENTATION CREEP; ALLOYS; NI; COMPOUND; BEHAVIOR; GROWTH; SOLDERABILITY; JOINTS;
D O I
10.1108/09540911011036262
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Purpose - The purpose of this paper is to investigate the effects of minor addition of the rare earth (RE) element cerium, Cc, on the microstructures and creep properties of Sn-Ag-Cu solder alloys. Design/methodology/approach - The pure Sn, Sn-Cu alloy, Sn-Ag alloy and Cu-Ce alloy were used as raw materials. Sn-Ag-Cu alloys with different contents of RE Cc were chosen to compare with Sn-Ag-Cu. The raw materials of Sn, Sn-Cu alloy, Sn-Ag alloy, Cu-Ce alloy were melted in a ceramic crucible, and were melted at 550 degrees C +/- 1 degrees C for 40 minutes. To homogenize the solder alloy, mechanical stirring was performed every ten minutes using a glass rod. During the melting, KG + LiCl (1.11), were used over the surface of liquid solder to prevent oxidation. The melted solder was chill cast into a rod. Findings - It is found that the microstructure exhibits smaller grains and the A0n/CU6Sn5 intermetallic compound (IMC) phases are modified in matrix with the addition of Cc. In particular, the addition of 0.03 wt.% Cc to the Sn-Ag-Cu solder can refine the microstructures and decrease the thickness of the IMC layers of Sn-Ag-Cu solder alloys. Meanwhile, thermodynamic analysis showed that these phenomena could be attributed to the reduction of the driving force for Cu-Sn IMC formation due to the addition of Cc. Results calculated using the thermodynamic method are close to the above experimental data. Thus, the optimum content of Cc in Sn-Ag-Cu solder alloys should be about 0.030 percent. Additionally, the effect of Cc on the creep rupture life of Sn-Ag-Cu soldered joints was studied. It was found that the creep rupture life may be increased up to 7.5 times more than that of the original Sn-Ag-Cu alloy, when Cc accounts for 0.030 percent. Originality/value - This paper usefully investigates the effects of the RE cerium (Cc), on the microstructures and creep properties of Sn-Ag-Cu solder alloys, optimizing the quantity of Cc in the Sn-Ag-Cu solder alloy through a thermodynamic method and by creep-rupture life testing.
引用
收藏
页码:30 / 36
页数:7
相关论文
共 50 条
  • [11] Properties enhancement of low Ag-content Sn-Ag-Cu lead-free solders containing small amount of Zn
    El-Daly, A. A.
    Hammad, A. E.
    Al-Ganainy, G. S.
    Ragab, M.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2014, 614 : 20 - 28
  • [12] Combined effects of Ag content and cooling rate on microstructure and mechanical behavior of Sn-Ag-Cu solders
    Pereira, Pedro Deghaid
    Spinelli, Jose Eduardo
    Garcia, Amauri
    MATERIALS & DESIGN, 2013, 45 : 377 - 383
  • [13] Temperature Dependence of Creep and Hardness of Sn-Ag-Cu Lead-Free Solder
    Y.D. Han
    H.Y. Jing
    S.M.L. Nai
    L.Y. Xu
    C.M. Tan
    J. Wei
    Journal of Electronic Materials, 2010, 39 : 223 - 229
  • [14] Interface behavior and performance of Sn-Ag-Cu lead-free solder bearing Tb
    Yuan, Zeyu
    He, Yujie
    Wu, Ruize
    Xu, Ming
    Zhang, Jun
    Zhu, Yunqing
    Wang, Qiaoli
    Xie, Weibin
    Chen, Huiming
    JOURNAL OF MATERIALS SCIENCE-MATERIALS IN ELECTRONICS, 2022, 33 (26) : 20769 - 20777
  • [15] Lead-free solders with rare earth additions
    Guo, Fu
    Zhao, Mengke
    Xia, Zhidong
    Lei, Yongping
    Li, Xiaoyan
    Shi, Yaowu
    JOM, 2009, 61 (06) : 39 - 44
  • [16] Viscoplastic creep and microstructure evolution of Sn-based lead-free solders at low strain
    Zhang, Q. K.
    Hu, F. Q.
    Song, Z. L.
    Zhang, Z. F.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2017, 701 : 187 - 195
  • [17] Mechanisms of beta-Sn nucleation and microstructure evolution in Sn-Ag-Cu solders containing titanium
    Ma, Z. L.
    Shang, H.
    Daszki, A. A.
    Belyakov, S. A.
    Gourlay, C. M.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2019, 777 : 1357 - 1366
  • [18] Effect of Sn nanoparticle additions on thermal properties of Sn-Ag-Cu lead-free solder paste
    Wernicki, Evan
    Gu, Zhiyong
    THERMOCHIMICA ACTA, 2020, 690
  • [19] The study of mechanical properties of Sn-Ag-Cu lead-free solders with different Ag contents and Ni doping under different strain rates and temperatures
    Che, F. X.
    Zhu, W. H.
    Poh, Edith S. W.
    Zhang, X. W.
    Zhang, X. R.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2010, 507 (01) : 215 - 224
  • [20] A study of the microstructure, thermal properties and wetting kinetics of Sn-3Ag-xZn lead-free solders
    Li, Yulong
    Yu, Xiao
    Sekulic, Dusan P.
    Hu, Xiaowu
    Yan, Ming
    Hu, Ronghua
    APPLIED PHYSICS A-MATERIALS SCIENCE & PROCESSING, 2016, 122 (06):