The Relationship between Microstructure and Fracture Behavior of TiAl/Ti2AlNb SPDB Joint with High Temperature Titanium Alloy Interlayers

被引:2
|
作者
Liao, Minxing [1 ]
Tian, Hao [1 ]
Zhao, Lei [2 ]
Zhang, Boxian [3 ]
He, Jianchao [1 ]
机构
[1] Harbin Inst Technol, Inst Special Environm Phys Sci, Shenzhen 518055, Peoples R China
[2] Cent Iron & Steel Res Inst, Dept Funct Mat Res, Beijing 100081, Peoples R China
[3] AVIC Mfg Technol Inst, Aeronaut Key Lab Welding & Joining Technol, Beijing 100024, Peoples R China
基金
中国国家自然科学基金;
关键词
spark plasma diffusion bonding; TiAl; microstructure; mechanical properties; fracture; GAMMA-TIAL ALLOYS; MECHANICAL-PROPERTIES; PURE TI; DEFORMATION; EVOLUTION; PHASE; FOIL; NB;
D O I
10.3390/ma15144849
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
In this paper, spark plasma diffusion bonding technology was employed to join TiAl and Ti2AlNb with high temperature titanium alloy interlayer at 950 degrees C/10kN/60 min, then following furnace cooling at cooling rate up to 100 degrees C/min. After welding, the joint was aging heat-treated at 800 degrees C for 24 h. The microstructure and the elements diffusion of the TiAl/Ti2AlNb joint was analyzed by field emission scanning electron microscopy (FESEM) with EDS. Moreover, the tensile properties of the joint were tested at room temperature, 650 degrees C, and 750 degrees C. The results show that the spark plasma diffusion bonding formed a high quality TiAl/Ti2AlNb joint without microcracks or microvoids, while also effectively protecting the base metal. Significant differences in the microstructure of the joint appeared from TiAl side to Ti2AlNb side: TiAl BM (Base Metal) -> DP(Duplex) and NG (Near-Gamma) -> alpha(2)-phase matrix with needle-like alpha-phase -> bulk alpha(2)-phase -> needle-like alpha-phase -> metastable beta-phase -> Ti2AlNb BM. After heat treatment at 800 degrees C for 24 h, the microstructure of the TiAl side and the interlayer region did not change, but the density and size of the needle-like alpha-phase in region 3 increased slightly. The microstructure of Ti2AlNb near the weld changed obviously, and a large number of fine O phases are precipitated from the metastable beta phase matrix after heat treatment. Except for the Ti2AlN near-interface region, the effect of heat treatment on the microstructure of the joint is not significant. The microhardness of the joint is in the shape of a mountain peak. The maximum microhardness at the interface is above 500 HV, and it is significantly reduced to 400 HV after heat treatment. The fracture of the joint occurred at the interface at room temperature, 650 degrees C, and 750 degrees C. with the tensile strength 450 MPa, 540 MPa, and 471 Mpa, respectively, and mainly showing brittle fracture.
引用
收藏
页数:14
相关论文
共 50 条
  • [1] Effect of processing parameters on the microstructure and mechanical properties of TiAl/Ti2AlNb laminated composites
    Li, Donghai
    Wang, Binbin
    Luo, Liangshun
    Li, Xuewen
    Xu, Yanjin
    Li, BinQiang
    Hawezy, Diween
    Wang, Liang
    Su, Yanqing
    Guo, Jingjie
    Fu, Hengzhi
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2022, 109 : 228 - 244
  • [2] Study of microstructure and mechanical properties of Ti2AlNb/TiAl LFW joint
    Zhang, Da
    Jiang, Fangyuan
    Xiong, Jiangtao
    Liu, Jiatao
    Li, Jinglong
    Guo, Wei
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2025, 934
  • [3] Microstructure evolution and mechanical properties of diffusion bonding high Nb containing TiAl alloy to Ti2AlNb alloy
    Zhu, Lei
    Li, Jinshan
    Tang, Bin
    Liu, Yan
    Zhang, Mengqi
    Li, Lei
    Kou, Hongchao
    VACUUM, 2019, 164 : 140 - 148
  • [4] Microstructure of γ-TiAl and Ti2AlNb linear friction welding joint
    Du, Suigeng
    Hu, Hongyi
    Ding, Ke
    Hangkong Xuebao/Acta Aeronautica et Astronautica Sinica, 2024, 45 (13):
  • [5] Microstructure and phase evolution in γ-TiAl/Ti2AlNb dual alloy fabricated by direct metal deposition
    Wu, Yu
    Cheng, Xu
    Zhang, Shuquan
    Liu, Dong
    Wang, Huaming
    INTERMETALLICS, 2019, 106 : 26 - 35
  • [6] Enhanced strength and fracture characteristics of the TiAl/Ti2AlNb laminated composite
    Li, Donghai
    Wang, Binbin
    Luo, Liangshun
    Li, Xuewen
    Yu, Jianxin
    Li, Binqiang
    Wang, Liang
    Su, Yanqing
    Guo, Jingjie
    Fu, Hengzhi
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2022, 835
  • [7] Improvement of room temperature ductility for Mo and Fe modified Ti2AlNb alloy
    Emura, Satoshi
    Tsuzaki, Kaneaki
    Tsuchiya, Koichi
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2010, 528 (01): : 355 - 362
  • [8] Relationship between microstructure and mechanical properties of TiAl/Ti2AlNb joint brazed using Ti-27Co eutectic filler metal
    Cao, Jian
    Dai, Xiangyu
    Liu, Jiaqi
    Si, Xiaoqing
    Feng, Jicai
    MATERIALS & DESIGN, 2017, 121 : 176 - 184
  • [9] Regulating the interfacial microstructure in TiAl/Ti2AlNb vacuum diffusion bonded joints for superior mechanical performance
    Huang, Libing
    Dong, Honggang
    Li, Jiachen
    Li, Chao
    Li, Peng
    Zhao, Dongsheng
    Shi, Shuyan
    Liu, Xiaoying
    Ma, Xiong
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2023, 887
  • [10] Effect of welding temperature on microstructure and mechanical properties of TiAl/Ti2AlNb spark plasma diffusion welded joint
    Ma, Mingqian
    Chen, Chunhuan
    Chai, Lu
    Lv, Yanlong
    Hou, Jinbao
    Zhang, Boxian
    WELDING IN THE WORLD, 2022, 66 (05) : 985 - 994