Effects of Temperature and Applied Potential on the Stress Corrosion Cracking of X80 Steel in a Xinzhou Simulated Soil Solution

被引:5
作者
Cheng, Yuan [1 ]
Liu, Peng [1 ]
Yang, Mengmeng [1 ]
机构
[1] Univ Sci & Technol Beijing, Natl Ctr Mat Serv Safety, Beijing 100083, Peoples R China
关键词
stress corrosion cracking (SCC); pipeline steel; soil environment; X70 PIPELINE STEEL; STRAIN-RATE; MECHANISTIC ASPECT; PITTING CORROSION; HYDROGEN; INITIATION; BEHAVIOR; GAS; DISSOLUTION; GROWTH;
D O I
10.3390/ma15072560
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
In this research, the stress corrosion cracking (SCC) behavior of X80 pipeline steel in a Xinzhou soil environment at different temperatures and applied potentials was studied with a slow strain rate test (SSRT), potentiodynamic polarization curve measurements, and scanning electron microscopy (SEM). When a higher anodic potential was applied, anodic dissolution occurred at the crack tip and on the crack wall. The cracking mechanism of X80 steel in Xinzhou soil solution is anodic dissolution (AD). At positive cathodic potentials, X80 steel is under an anodic polarization state at the crack tip and under a cathodic polarization state at the crack wall. The SCC of X80 steel is affected by the combined effects of anodic dissolution (AD) and hydrogen embrittlement (HE). At more negative cathodic potentials, both crack tips and crack walls are under cathodic polarization. The SCC of X80 steel is dominated by hydrogen embrittlement (HE). SCC susceptibility has the same variation trend with potentials at different temperatures. The susceptibility to SCC increases notably as the temperature increases at weak cathodic potentials and open circuit potential due to the effect of temperature on the corrosion potential and the diffusion of atoms.
引用
收藏
页数:13
相关论文
共 60 条
[1]   Corrosion and cracking behavior in an API X-80 steel exposed to sour gas environments [J].
Albarran, JL ;
Aguilar, A ;
Martinez, L ;
Lopez, HF .
CORROSION, 2002, 58 (09) :783-792
[2]   A new understanding of intergranular stress corrosion cracking resistance of pipeline steel through grain boundary character and crystallographic texture studies [J].
Arafin, M. A. ;
Szpunar, J. A. .
CORROSION SCIENCE, 2009, 51 (01) :119-128
[3]   Role of microstructures on stress corrosion cracking of pipeline steels in carbonate-bicarbonate solution [J].
Asahi, H ;
Kushida, T ;
Kimura, M ;
Fukai, H ;
Okano, S .
CORROSION, 1999, 55 (07) :644-652
[4]   Hydrogen permeation and hydrogen content under cathodic charging in HSLA 80 and HSLA 100 steels [J].
Banerjee, K ;
Chatterjee, UK .
SCRIPTA MATERIALIA, 2001, 44 (02) :213-216
[5]   2013 Frank Newman Speller Award Lecture: Integrity Management of Natural Gas and Petroleum Pipelines Subject to Stress Corrosion Cracking [J].
Beavers, John A. .
CORROSION, 2014, 70 (01) :3-18
[6]   Effect of hydrogen peroxide on crack growth rate in X70 pipeline steel in weak acid solution [J].
Bogdanov, Roman ;
Marshakov, Andrey ;
Ignatenko, Vasiliy ;
Ryakhovskikh, Ilya ;
Bachurina, Diana .
CORROSION ENGINEERING SCIENCE AND TECHNOLOGY, 2017, 52 (04) :294-301
[7]   Research and Cracking Implications from an Assessment of Two Variants of Near-Neutral pH Crack Colonies in Liquid Pipelines [J].
Bouaeshi, W. ;
Ironside, S. ;
Eadie, R. .
CORROSION, 2007, 63 (07) :648-660
[8]   Hydrogen assisted cracking driven by cathodic protection operated at near -1200 mV CSE - an onshore natural gas pipeline failure [J].
Cazenave, Pablo ;
Jimenez, Katina ;
Gao, Ming ;
Moneta, Andrea ;
Hryciuk, Pedro .
JOURNAL OF PIPELINE SCIENCE AND ENGINEERING, 2021, 1 (01) :100-121
[9]   An Overview of Near-Neutral pH Stress Corrosion Cracking in Pipelines and Mitigation Strategies for Its Initiation and Growth [J].
Chen, Weixing .
CORROSION, 2016, 72 (07) :962-977
[10]   Microstructure dependence of stress corrosion cracking initiation in X-65 pipeline steel exposed to a near-neutral pH soil environment [J].
Chu, R ;
Chen, W ;
Wang, SH ;
King, F ;
Jack, TR ;
Fessler, RR .
CORROSION, 2004, 60 (03) :275-283