Preparation of silica aerogel from TEOS

被引:92
作者
Tamon, H [1 ]
Kitamura, T [1 ]
Okazaki, M [1 ]
机构
[1] Kyoto Univ, Dept Chem Engn, Kyoto 60601, Japan
关键词
silica aerogel; sol-gel polymerization; tetraethylorthosilicate (TEOS); supercritical drying; light transmission; mesoporous structure;
D O I
10.1006/jcis.1997.5269
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Silica alcogels were synthesized by the sol-gel polymerization of tetraethylorthosilicate (TEOS). In the synthesis, HCl and NH3 were used as hydrolysis and condensation catalysts. The gelation time became short and the visible light transmittance increased with increasing the amount of HCl or lengthening the hydrolysis time. The alcogels were dried under supercritical conditions with carbon dioxide, and silica aerogels were obtained. As a result of characterization by visible light transmission and N-2 adsorption, the aerogels are mesoporous materials with high surface areas. The experimental results suggest that the aerogel properties are not influenced by the drying conditions such as extraction temperature, extraction time, depressurizing temperature, and depressurizing rate. On the other hand, the properties are changed under the conditions of sol-gel polymerization. In the preparation of highly transparent aerogels with high surface areas and large pore volumes, it is necessary to synthesize highly transparent alcogels. It is found that the visible light transmittance of alcogels is an index for preparing aerogols from TEOS. (C) 1998 Academie Press.
引用
收藏
页码:353 / 359
页数:7