Effects of oxide addition on the microstructure and mechanical properties of lamellar SiC scaffolds and Al-Si-Mg/SiC composites prepared by freeze casting and pressureless infiltration
被引:49
作者:
论文数: 引用数:
h-index:
机构:
Shaga, Alateng
[1
]
Shen, Ping
论文数: 0引用数: 0
h-index: 0
机构:
Jilin Univ, Key Lab Automobile Mat, Dept Mat Sci & Engn, Minist Educ, 5988 Renmin St, Changchun 130025, Peoples R ChinaJilin Univ, Key Lab Automobile Mat, Dept Mat Sci & Engn, Minist Educ, 5988 Renmin St, Changchun 130025, Peoples R China
Shen, Ping
[1
]
Guo, Rui-Fen
论文数: 0引用数: 0
h-index: 0
机构:
Jilin Univ, Key Lab Automobile Mat, Dept Mat Sci & Engn, Minist Educ, 5988 Renmin St, Changchun 130025, Peoples R ChinaJilin Univ, Key Lab Automobile Mat, Dept Mat Sci & Engn, Minist Educ, 5988 Renmin St, Changchun 130025, Peoples R China
Guo, Rui-Fen
[1
]
Jiang, Qi-Chuan
论文数: 0引用数: 0
h-index: 0
机构:
Jilin Univ, Key Lab Automobile Mat, Dept Mat Sci & Engn, Minist Educ, 5988 Renmin St, Changchun 130025, Peoples R ChinaJilin Univ, Key Lab Automobile Mat, Dept Mat Sci & Engn, Minist Educ, 5988 Renmin St, Changchun 130025, Peoples R China
Jiang, Qi-Chuan
[1
]
机构:
[1] Jilin Univ, Key Lab Automobile Mat, Dept Mat Sci & Engn, Minist Educ, 5988 Renmin St, Changchun 130025, Peoples R China
Silicate-bonded porous SiC scaffolds with lamellar structures were prepared by freeze casting and liquid phase sintering. It was found that the viscosity and solidification velocity of SiC water-based slurries with 30 vol% solid loading decreased with increasing Al2O3-MgO (AM) addition. As the AM content increased from 10 to 30 wt%, the lamellae of the sintered scaffolds became denser and the porosity decreased from 69 +/- 0.5% to 62 +/- 0.5%, while the compressive strength improved from 25 +/- 2 to 51 +/- 2 MPa. The dynamics of pressureless infiltration for an Al-12 Si-10 Mg alloy on the SiC porous scaffold was measured and the composites with lamellar-interpenetrated structures were successfully produced. Both the compressive strength and the elastic modulus of the composites increased with increasing AM content. The maximum strength reached 952 +/- 24 MPa and the highest elastic modulus about 156 GPa, respectively, in a longitudinal direction, increasing about 32% and 11% as compared with those of the composites without AM. (C) 2016 Elsevier Ltd and Techna Group S.r.l. All rights reserved.