On the effect of temperature on the threshold stress intensity factor of delayed hydride cracking in light water reactor fuel cladding

被引:17
|
作者
Holston, Anna-Maria Alvarez [1 ]
Stjarnsater, Johan [1 ]
机构
[1] Studsvik Nucl AB, S-61182 Nykoping, Sweden
关键词
Delayed Hydride Cracking; Fuel Cladding Integrity; Pin Loading Testing; Threshold Stress Intensity Factor; Zry-4; WT-PERCENT NB; HYDROGEN EMBRITTLEMENT; ZIRCONIUM ALLOYS; BEND TESTS; ZIRCALOY-4; SOLUBILITY; BEHAVIOR;
D O I
10.1016/j.net.2017.04.002
中图分类号
TL [原子能技术]; O571 [原子核物理学];
学科分类号
0827 ; 082701 ;
摘要
Delayed hydride cracking (DHC) was first observed in pressure tubes in Canadian CANDU reactors. In light water reactors, DHC was not observed until the late 1990s in high-burnup boiling water reactor (BWR) fuel cladding. In recent years, the focus on DHC has resurfaced in light of the increased interest in the cladding integrity during interim conditions. In principle, all spent fuel in the wet pools has sufficient hydrogen content for DHC to operate below 300 degrees C. It is therefore of importance to establish the critical parameters for DHC to operate. This work studies the threshold stress intensity factor (K-IH) to initiate DHC as a function of temperature in Zry-4 for temperatures between 227 degrees C and 315 degrees C. The experimental technique used in this study was the pin-loading testing technique. To determine the KIH, an unloading method was used where the load was successively reduced in a stepwise manner until no cracking was observed during 24 hours. The results showed that there was moderate temperature behavior at lower temperatures. Around 300 degrees C, there was a sharp increase in KIH indicating the upper temperature limit for DHC. The value for KIH at 227 degrees C was determined to be 2.6 +/- 0.3 MPa root m. (C) 2017 Korean Nuclear Society, Published by Elsevier Korea LLC.
引用
收藏
页码:663 / 667
页数:5
相关论文
共 42 条
  • [21] Effect analysis of stress-intensity-factor-range decreasing rate for obtaining threshold stress-intensity-factor-range
    Li, Bochuan
    Koyama, Motomichi
    Hamada, Shigeru
    Noguchi, Hiroshi
    THEORETICAL AND APPLIED FRACTURE MECHANICS, 2019, 104
  • [22] Threshold stress intensity factor and crack growth rate for stress corrosion cracking of simulated heat affected zone in caustic solution
    Pal, Sarvesh
    Ibrahim, R. N.
    Raman, R. K. Singh
    ENGINEERING FRACTURE MECHANICS, 2011, 78 (01) : 13 - 26
  • [23] Effect of Specimen Thickness on Threshold Stress Intensity Factor (KIH) Associated with DHC in Zr-2.5 Nb Alloy Pressure Tube Material
    Sunil, Saurav
    Bind, A. K.
    Murty, T. N.
    Singh, R. N.
    Avinash, G.
    Singh, I. V.
    MATERIALS PERFORMANCE AND CHARACTERIZATION, 2022, 11 (02) : 301 - 314
  • [24] On temperature-dependent interfacial fracture energy/stress intensity factor and matrix cracking in ceramic composites
    Gao, Fei
    Li, Weiguo
    Zhang, Xuyao
    Yang, Mengqing
    He, Yi
    Dong, Pan
    Ma, Yanli
    Qu, Zhaoliang
    INTERNATIONAL JOURNAL OF APPLIED CERAMIC TECHNOLOGY, 2022, 19 (04) : 2300 - 2310
  • [25] Multiphysics modeling of accident tolerant fuel-cladding U3Si2-FeCrAl performance in a light water reactor
    Liu, Rong
    Zhou, Wenzhong
    Cai, Jiejin
    NUCLEAR ENGINEERING AND DESIGN, 2018, 330 : 106 - 116
  • [26] Effects of temperature and oxidation on threshold stress intensity factor of 12% Cr steel for steam turbine rotor component
    Lee, Jong-Hoon
    Kim, Bum-Joon
    Kim, Moon Ki
    Lim, Byeong-Soo
    JOURNAL OF MECHANICAL SCIENCE AND TECHNOLOGY, 2013, 27 (05) : 1273 - 1277
  • [27] Hydrogen-enhanced oxidation of ferrite phase in stainless steel cladding and the contribution to stress corrosion cracking in deaerated high temperature water
    Cui, Tongming
    Dong, Haiying
    Xu, Xinhe
    Ma, Jiarong
    Lu, Zhanpeng
    Tang, Yuanjie
    Pan, Deng
    Lozano-Perez, Sergio
    Shoji, Tetsuo
    JOURNAL OF NUCLEAR MATERIALS, 2021, 557
  • [28] Effect of temperature on hydrogen embrittlement susceptibility of alloy 718 in Light Water Reactor environment
    Galliano, Florian
    Andrieu, Eric
    Cloue, Jean-Marc
    Odemer, Gregory
    Blanc, Christine
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2017, 42 (33) : 21371 - 21378
  • [29] Threshold stress intensity factor for hydrogen-assisted cracking of CR-MO steel used as stationary storage buffer of a hydrogen refueling station
    Matsumoto, T.
    Kubota, M.
    Matsuolza, S.
    Ginet, P.
    Furtado, J.
    Barbier, F.
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2017, 42 (11) : 7422 - 7428
  • [30] Role of Zn injection on mitigating stress corrosion cracking initiation of Alloy 182 weld metal in simulated light water reactor environment
    Chen, Kai
    Mackiewicz, Adrianna
    Seifert, Hans -Peter
    Virtanen, Sannakaisa
    Ritter, Stefan
    CORROSION SCIENCE, 2023, 221