On the effect of temperature on the threshold stress intensity factor of delayed hydride cracking in light water reactor fuel cladding

被引:17
|
作者
Holston, Anna-Maria Alvarez [1 ]
Stjarnsater, Johan [1 ]
机构
[1] Studsvik Nucl AB, S-61182 Nykoping, Sweden
关键词
Delayed Hydride Cracking; Fuel Cladding Integrity; Pin Loading Testing; Threshold Stress Intensity Factor; Zry-4; WT-PERCENT NB; HYDROGEN EMBRITTLEMENT; ZIRCONIUM ALLOYS; BEND TESTS; ZIRCALOY-4; SOLUBILITY; BEHAVIOR;
D O I
10.1016/j.net.2017.04.002
中图分类号
TL [原子能技术]; O571 [原子核物理学];
学科分类号
0827 ; 082701 ;
摘要
Delayed hydride cracking (DHC) was first observed in pressure tubes in Canadian CANDU reactors. In light water reactors, DHC was not observed until the late 1990s in high-burnup boiling water reactor (BWR) fuel cladding. In recent years, the focus on DHC has resurfaced in light of the increased interest in the cladding integrity during interim conditions. In principle, all spent fuel in the wet pools has sufficient hydrogen content for DHC to operate below 300 degrees C. It is therefore of importance to establish the critical parameters for DHC to operate. This work studies the threshold stress intensity factor (K-IH) to initiate DHC as a function of temperature in Zry-4 for temperatures between 227 degrees C and 315 degrees C. The experimental technique used in this study was the pin-loading testing technique. To determine the KIH, an unloading method was used where the load was successively reduced in a stepwise manner until no cracking was observed during 24 hours. The results showed that there was moderate temperature behavior at lower temperatures. Around 300 degrees C, there was a sharp increase in KIH indicating the upper temperature limit for DHC. The value for KIH at 227 degrees C was determined to be 2.6 +/- 0.3 MPa root m. (C) 2017 Korean Nuclear Society, Published by Elsevier Korea LLC.
引用
收藏
页码:663 / 667
页数:5
相关论文
共 42 条
  • [1] Threshold stress intensity factor of delayed hydride cracking in irradiated and unirradiated zircaloy-4 cladding
    Hong, Jong-Dae
    Park, Myungchul
    Holston, Anna-Maria Alvarez
    Stjarnsater, Johan
    Kook, Donghak
    JOURNAL OF NUCLEAR MATERIALS, 2021, 543
  • [2] Theoretical models of threshold stress intensity factor and critical hydride length for delayed hydride cracking considering thermal stresses
    Zhang, Jingyu
    Zhu, Jiacheng
    Ding, Shurong
    Chen, Liang
    Li, Wenjie
    Pang, Hua
    NUCLEAR ENGINEERING AND TECHNOLOGY, 2018, 50 (07) : 1138 - 1147
  • [3] Threshold stress intensity factor for delayed hydride cracking of a recrystallized N18 alloy plate along the rolling direction
    Sun, Chao
    Ying, Shi H.
    Tan, Jun
    Peng, Qian
    Dai, Xun
    PROCEEDINGS OF THE 18TH INTERNATIONAL CONFERENCE ON NUCLEAR ENGINEERING 2010, VOL 5, 2011, : 79 - +
  • [4] Threshold stress intensity factor for delayed hydride cracking in Zr-2.5%Nb pressure tube alloy
    Singh, R. N.
    Stahle, P.
    Chakravartty, J. K.
    Shmakov, A. A.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2009, 523 (1-2): : 112 - 117
  • [5] Theory model combined with XFEM of threshold stress intensity factor and critical hydride length for delay hydride cracking
    Chen, Wenjun
    Kou, Huaqin
    Chen, Liang
    Wang, Fang
    Zeng, Xiangguo
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2019, 44 (54) : 29047 - 29056
  • [6] ENGINEERING RELATION FOR DEPENDENCE OF THRESHOLD STRESS INTENSITY FACTOR FOR DELAYED HYDRIDE CRACKING ON CRACK ORIENTATION
    Scarth, Douglas A.
    Shek, Gordon K.
    Xu, Steven X.
    PROCEEDINGS OF THE ASME PRESSURE VESSELS AND PIPING CONFERENCE - 2008, VOL 6, PT A AND B, 2009, : 29 - 42
  • [7] A THEORETICAL MODEL OF THE STRESS INTENSITY FACTOR THRESHOLD OF DHC FOR FUEL CLADDING TUBE
    Chen, Liang
    Liu, Lili
    Song, Xiaoming
    Pang, Hua
    PROCEEDINGS OF THE 26TH INTERNATIONAL CONFERENCE ON NUCLEAR ENGINEERING, 2018, VOL 3, 2018,
  • [8] DELAYED HYDRIDE CRACKING IN ZIRCALOY FUEL CLADDING - AN IAEA COORDINATED RESEARCH PROGRAMME
    Coleman, C.
    Grigoriev, V.
    Inozemtsev, V.
    Markelov, V.
    Roth, M.
    Makarevicius, V.
    Kim, Y. S.
    Ali, Kanwar Liagat
    Chakravartty, J. K.
    Mizrahi, R.
    Lalgudi, R.
    NUCLEAR ENGINEERING AND TECHNOLOGY, 2009, 41 (02) : 171 - 178
  • [9] An assessment of delayed hydride cracking in zirconium alloy cladding tubes under stress transients
    Chan, K. S.
    INTERNATIONAL MATERIALS REVIEWS, 2013, 58 (06) : 349 - 373
  • [10] EFFECTS OF TEMPERATURE AND THERMAL CYCLING ON THE THRESHOLD STRESS INTENSITY FACTOR FOR DELAYED HYDRIDE CRACKING IN ZR-2.5 NB PRESSURE TUBES
    Shek, Gordon K.
    Cui, Jun
    PROCEEDINGS OF THE ASME PRESSURE VESSELS AND PIPING CONFERENCE, VOL 6, PTS A AND B, 2010, : 107 - 116