Synthesis of mixed-phase titania films by low-temperature ultrasonic spray pyrolysis

被引:16
|
作者
Nakaruk, A. [1 ]
Kavei, G. [1 ,2 ]
Sorrell, C. C. [1 ]
机构
[1] Univ New S Wales, Sch Mat Sci & Engn, Sydney, NSW 2052, Australia
[2] Mat & Energy Res Ctr, Tehran, Iran
基金
澳大利亚研究理事会;
关键词
Titanium dioxide; Ultrasonic spray pyrolysis; Thin film; Glancing angle X-ray diffraction; TIO2; THICK-FILMS; ANATASE-RUTILE TRANSFORMATION; OPTICAL-PROPERTIES; DEPOSITION; OXIDATION; HYDROGEN;
D O I
10.1016/j.matlet.2010.03.016
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Fully dense TiO2 films with (1) mixed-phase rutile and anatase and (2) anatase (sole phase) were deposited on fused quartz substrates by ultrasonic spray pyrolysis at nominally 400 degrees C. The presence and absence of insulation around the entrainment pathway traversing 20 cm above the substrate/hot plate were investigated (174 degrees C vs 122 degrees C). The thick films were assessed in terms of mineralogies (qualitative and quantitative), microstructures (topography, thickness and grain size), and visible light transmission (optical and microstructural considerations). With insulation, opaque mixed anatase (similar to 30 vol.%; <50 nm) and rutile (similar to 70 vol.%; similar to 1 mu m) were observed; without insulation, only transparent anatase (<50 nm) was observed. (C) 2010 Elsevier B.V. All rights reserved.
引用
收藏
页码:1365 / 1368
页数:4
相关论文
共 50 条
  • [1] Anatase-rutile transformation through high-temperature annealing of titania films produced by ultrasonic spray pyrolysis
    Nakaruk, A.
    Ragazzon, D.
    Sorrell, C. C.
    THIN SOLID FILMS, 2010, 518 (14) : 3735 - 3742
  • [2] TiO2 films prepared by ultrasonic spray pyrolysis
    Nakaruk, A.
    Reece, P. J.
    Ragazzon, D.
    Sorrell, C. C.
    MATERIALS SCIENCE AND TECHNOLOGY, 2010, 26 (04) : 469 - 472
  • [3] Anatase thin films by ultrasonic spray pyrolysis
    Nakaruk, A.
    Ragazzon, D.
    Sorrell, C. C.
    JOURNAL OF ANALYTICAL AND APPLIED PYROLYSIS, 2010, 88 (01) : 98 - 101
  • [4] Deposition rate of anatase films by ultrasonic spray pyrolysis
    Ragazzon, D.
    Nakaruk, A.
    Sorrell, C. C.
    ADVANCES IN APPLIED CERAMICS, 2010, 109 (04) : 196 - 199
  • [5] Low-Temperature Growth of ZnO Films by Spray Pyrolysis
    Yoshino, Kenji
    Takemoto, Yujin
    Oshima, Minoru
    Toyota, Kouji
    Inaba, Koichiro
    Haga, Ken-ichi
    Tokudome, Koichi
    JAPANESE JOURNAL OF APPLIED PHYSICS, 2011, 50 (04)
  • [6] Low substrate temperature synthesis of carbon nanowalls by ultrasonic spray pyrolysis
    Zhang, Jianhui
    Khatri, Ishwor
    Kishi, Naoki
    Mominuzzaman, Sharif M.
    Soga, Tetsuo
    Jimbo, Takashi
    THIN SOLID FILMS, 2011, 519 (13) : 4162 - 4165
  • [7] Mixed-phase nanocrystalline TiO2 photocatalysts produced by flame spray pyrolysis
    Bettini, Luca Giacomo
    Dozzi, Maria Vittoria
    Della Foglia, Flavio
    Chiarello, Gian Luca
    Selli, Elena
    Lenardi, Cristina
    Piseri, Paolo
    Milani, Paolo
    APPLIED CATALYSIS B-ENVIRONMENTAL, 2015, 178 : 226 - 232
  • [8] Synthesis of TiO2 thin films by a new low-temperature solid-phase pyrolysis technique
    Volkova, M. G.
    Bayan, E. M.
    Petrov, V. V.
    Gulyaeva, I. A.
    Chernyshev, A., V
    FUNCTIONAL MATERIALS LETTERS, 2022, 15 (05)
  • [9] Low-temperature deposition of CuAl2O4 thin film photocatalyst by ultrasonic spray pyrolysis
    Suhariadi, Iping
    Rahmawan, Yudi
    Muyassiroh, Diva A. M.
    Barrinaya, Muhammad A.
    Fatriansyah, Jaka F.
    MATERIALS LETTERS, 2022, 311
  • [10] Low temperature growth of highly crystallized ZnO:Al films by ultrasonic spray pyrolysis from acetylacetone salt
    Xu, Jiwen
    Wang, Hua
    Yang, Ling
    Jiang, Minghong
    Wei, Shuai
    Zhang, Tingting
    MATERIALS SCIENCE AND ENGINEERING B-ADVANCED FUNCTIONAL SOLID-STATE MATERIALS, 2010, 167 (03): : 182 - 186