Gas-Phase Synthesis of Silicon-Rich Silicon Nitride Nanoparticles for High Performance Lithium-Ion Batteries

被引:14
作者
Kilian, Stefan O. [1 ]
Wiggers, Hartmut [1 ,2 ]
机构
[1] Univ Duisburg Essen, Inst Combust & Gas Dynam React Fluids, Carl Benz Str 199, D-47057 Duisburg, Germany
[2] Univ Duisburg Essen, Ctr Nanointegrat Duisburg Essen CENIDE, D-47057 Duisburg, Germany
关键词
high performance lithium– ion battery; nanoparticle synthesis; silicon anode; silicon nitride;
D O I
10.1002/ppsc.202100007
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The practical application of silicon-based anodes is severely hindered by continuous capacity fade during cycling. A very promising way to stabilize silicon in lithium-ion battery (LIB) anodes is the utilization of nanostructured silicon-rich silicon nitride (SiNx), a conversion-type anode material. Here, SiNx with structure sizes in the sub-micrometer range have been synthesized in a hot-wall reactor by pyrolysis of monosilane and ammonia. This work focusses on understanding process parameter-particle property correlations. Further, a model for the growth of SiNx nanoparticles in this hot-wall-reactor design is proposed. This synthesis concept is of specific interest regarding simplicity, flexibility, and scalability: A way utilizing any mixtures of precursor gases to build multi-functional nanoparticles that can be directly used for LIBs instead of focusing on modification of nanostructures after they have been formed. Lab-scale production rates as high as 30 g h(-1) can be easily achieved and further scaled. SiN0.7 nanoparticles provide a first cycle coulombic efficiency of 54%, a specific discharge capacity of 1367 mAh g(-1), and a capacity retention over 80% after 300 cycles at 0.5 C (j = 0.68 mA cm(-2)). These results imply that silicon-rich silicon nitrides are promising candidates for high-performance LIBs with very high durability.
引用
收藏
页数:10
相关论文
共 60 条
[1]   Review of selected electrode-solution interactions which determine the performance of Li and Li ion batteries [J].
Aurbach, D .
JOURNAL OF POWER SOURCES, 2000, 89 (02) :206-218
[2]  
B. I. S. Research, 2020, GLOBAL NEXT GENERATI
[3]   Colossal reversible volume changes in lithium alloys [J].
Beaulieu, LY ;
Eberman, KW ;
Turner, RL ;
Krause, LJ ;
Dahn, JR .
ELECTROCHEMICAL AND SOLID STATE LETTERS, 2001, 4 (09) :A137-A140
[4]  
BECERRA R, 2007, SILICON CHEM, V3, P131
[5]   Cost Projection of State of the Art Lithium-Ion Batteries for Electric Vehicles Up to 2030 [J].
Berckmans, Gert ;
Messagie, Maarten ;
Smekens, Jelle ;
Omar, Noshin ;
Vanhaverbeke, Lieselot ;
Van Mierlo, Joeri .
ENERGIES, 2017, 10 (09)
[6]   Will advanced lithium-alloy anodes have a chance in lithium-ion batteries? [J].
Besenhard, JO ;
Yang, J ;
Winter, M .
JOURNAL OF POWER SOURCES, 1997, 68 (01) :87-90
[7]   Nanomaterials for rechargeable lithium batteries [J].
Bruce, Peter G. ;
Scrosati, Bruno ;
Tarascon, Jean-Marie .
ANGEWANDTE CHEMIE-INTERNATIONAL EDITION, 2008, 47 (16) :2930-2946
[8]   Surface chemistry and morphology of the solid electrolyte interphase on silicon nanowire lithium-ion battery anodes [J].
Chan, Candace K. ;
Ruffo, Riccardo ;
Hong, Seung Sae ;
Cui, Yi .
JOURNAL OF POWER SOURCES, 2009, 189 (02) :1132-1140
[9]   Recent advancement of SiOx, based anodes for lithium-ion batteries [J].
Chen, Tao ;
Wu, Ji ;
Zhang, Qinglin ;
Su, Xin .
JOURNAL OF POWER SOURCES, 2017, 363 :126-144
[10]   Rapid, low-temperature synthesis of nc-Si in high-density, non-equilibrium plasmas: enabling nanocrystallinity at very low hydrogen dilution [J].
Cheng, Qijin ;
Xu, Shuyan ;
Ostrikov, Kostya .
JOURNAL OF MATERIALS CHEMISTRY, 2009, 19 (29) :5134-5140