Effect of Li content on microstructure and mechanical property of Mg-xLi-3(Al-Si) alloys

被引:29
作者
Zhang, Cheng [1 ,2 ]
Wu, Liang [1 ,2 ]
Zhao, Zi-long [3 ]
Xie, Zhi-hui [4 ]
Huang, Guang-sheng [1 ,2 ,5 ]
Liu, Lei [1 ,2 ]
Jiang, Bin [1 ,2 ,5 ]
Atrens, Andrej [6 ]
Pan, Fu-sheng [1 ,2 ,5 ]
机构
[1] Chongqing Univ, Coll Mat Sci & Engn, State Key Lab Mech Transmiss, Chongqing 400044, Peoples R China
[2] Chongqing Univ, Natl Engn Res Ctr Magnesium Alloys, Chongqing 400044, Peoples R China
[3] Chongqing Univ, Coll Civil Engn, Chongqing 400045, Peoples R China
[4] China West Normal Univ, Coll Chem & Chem Engn, Synth & Pollut Control Key Lab Sichuan Prov, Nanchong 637002, Peoples R China
[5] Chongqing Acad Sci & Technol, Chongqing Res Ctr Adv Mat, Chongqing 401123, Peoples R China
[6] Univ Queensland, Sch Mech & Min Engn, Brisbane, Qld 4072, Australia
基金
中国博士后科学基金; 中国国家自然科学基金;
关键词
Mg-Li alloy; Al-Si eutectic; second phase; tensile strength; elongation; LAYERED DOUBLE HYDROXIDE; ICOSAHEDRAL PHASE; MG ALLOY; CRYSTALLOGRAPHIC TEXTURE; SI ADDITIONS; CORROSION; AL; EVOLUTION; BEHAVIOR; MG-8LI;
D O I
10.1016/S1003-6326(19)65158-7
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Mg-4Li-3(Al-Si), Mg-8Li-3(Al-Si) and Mg-12Li-3(Al-Si) alloys based on the alpha-Mg, alpha-Mg+beta-Li, beta-Li phases, respectively, were produced to investigate the effect of alloying with Al-Si eutectic on the microstructure and mechanical properties of the three alloys. Alloying with the Al-Si eutectic of Mg-xLi (x=4, 8 and 12 wt.%) alloys caused the formation of different types of Al-Li precipitates: Al3Li, AlLi and Li3Al2, respectively. Also, considerable quantities of Mg2Si phase particles were found in the three alloys. The results of tensile tests showed that the Mg-4Li-3(Al-Si) alloy exhibited the highest ultimate tensile strength (UTS) of 249 MPa but the lowest elongation of 6.3%. The Mg-12Li-3(Al-Si) alloy had the highest elongation of 26% but the lowest UTS of 173 MPa. The different mechanical properties were attributed to the different crystal structures of the three alloys and the precipitate with different type, morphology and distribution.
引用
收藏
页码:2506 / 2513
页数:8
相关论文
共 36 条
[11]   Silicon Strengthened CrAlVN Coatings [J].
Li, Qiang ;
Qiu, Yue-xiu ;
Li, Bo ;
Zhao, Dong-liang ;
Sun, De-en ;
Li, De-hui .
JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL, 2015, 22 (12) :1118-1125
[12]   Formation Behavior of 14H Long Period Stacking Ordered Structure in Mg-Y-Zn Cast Alloys with Different α-Mg Fractions [J].
Liu, Huan ;
Xue, Feng ;
Bai, Jing ;
Ma, Aibin ;
Jiang, Jinghua .
JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2016, 32 (12) :1267-1273
[13]   Microstructure evolution of Mg-14% Li-1% Al alloy during the process of equal channel angular pressing [J].
Liu, T. ;
Wu, S. D. ;
Li, S. X. ;
Li, P. J. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2007, 460 :499-503
[14]   Revealing the Maximum Strength in Nanotwinned Copper [J].
Lu, L. ;
Chen, X. ;
Huang, X. ;
Lu, K. .
SCIENCE, 2009, 323 (5914) :607-610
[15]   3D reconstruction of plasma electrolytic oxidation coatings on Mg alloy via synchrotron radiation tomography [J].
Lu, Xiaopeng ;
Blawert, Carsten ;
Tolnai, Domonkos ;
Subroto, Tungky ;
Kainer, Karl Ulrich ;
Zhang, Tao ;
Wang, Fuhui ;
Zheludkevich, Mikhail L. .
CORROSION SCIENCE, 2018, 139 :395-402
[16]   Effect of Li content on the indentation creep characteristics of cast Mg-Li-Zn alloys [J].
Mahmudi, R. ;
Shalbafi, M. ;
Karami, M. ;
Geranmayeh, A. R. .
MATERIALS & DESIGN, 2015, 75 :184-190
[17]   Development of lightweight Mg-Li-Al alloys with high specific strength [J].
Park, Gyu Hyeon ;
Kim, Jeong Tae ;
Park, Hae Jin ;
Kim, Young Seok ;
Jeong, Hae Joon ;
Lee, Naesung ;
Seo, Yongho ;
Suh, Jin-Yoo ;
Son, Hyeon-Taek ;
Wang, Wei-Min ;
Park, Jin Man ;
Kim, Ki Buen .
JOURNAL OF ALLOYS AND COMPOUNDS, 2016, 680 :116-120
[18]   Effects of adding Al-Si eutectic alloy and hot rolling on microstructures and mechanical behavior of Mg-8Li alloys [J].
Shi, Quanxin ;
Bian, Liping ;
Liang, Wei ;
Chen, Zhiqiang ;
Yang, Fuqian ;
Wang, Yide .
JOURNAL OF ALLOYS AND COMPOUNDS, 2015, 631 :129-132
[19]   Influence of extruding temperature and heat treatment process on microstructure and mechanical properties of three structures containing Mg-Li alloy bars [J].
Tang, Yan ;
Le, Qichi ;
Misra, R. D. K. ;
Su, Guanqiao ;
Cui, Jianzhong .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2018, 712 :266-280
[20]   Microstructure and properties of Mg-8Li-1Al-1Ce alloy [J].
Wang, Tao ;
Zhang, Milin ;
Wu, Ruizhi .
MATERIALS LETTERS, 2008, 62 (12-13) :1846-1848