Influence of Microalloying Elements on Recrystallization Texture of Warm-Rolled Interstitial Free Steels

被引:14
作者
Capdevila, C. [1 ]
Amigo, V. [2 ]
Caballero, F. G. [1 ]
de Andres, C. Garcia [1 ]
Salvador, M. D. [2 ]
机构
[1] CSIC, CENIM, Madrid 28040, Spain
[2] Univ Politecn Valencia, Inst Tecnol Mat, Valencia 46022, Spain
关键词
interstitial free (IF) steels; ferrite; recrystallization; texture; LOW-CARBON STEEL; HIGH-STRENGTH STEELS; PRECIPITATION; AUSTENITE; BEHAVIOR;
D O I
10.2320/matertrans.MG200909
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The addition of microalloying elements such as Ti and Nb to increase the strength of deep drawing quality steels for automotive sheet products might affect the microstructure formed during the annealing after warm rolling in several ways. Firstly, the precipitates can exert a Zener's pinning on growing recrystallized grain, which leads to a sluggish recrystallization kinetics. Secondly, the amount of microalloying elements control the amount of C, N, S, and P in solid solution, which indirectly affects the recrystallization texture obtained after annealing. In this sense, the work carried out with three different interstitial free (IF) and interstitial free high-strength (IFHS) steel grades allows us to conclude that the increase of microalloying additions delays recrystallization kinetics. Moreover, the abrupt texture change observed between as-rolled and annealed material indicates that the nucleation mechanism for recrystallization is more related to classical nucleation at deformed grain boundaries than subgrain rotation (continuous nucleation). [doi:10.2320/matertrans.MG200909]
引用
收藏
页码:625 / 634
页数:10
相关论文
共 34 条
[1]  
ABE T, 1983, TETSU TO HAGANE, V69, pS1415
[2]   Microstructural development during warm rolling of an IF steel [J].
Akbari, GH ;
Sellars, CM ;
Whiteman, JA .
ACTA MATERIALIA, 1997, 45 (12) :5047-5058
[3]   Distinctive aspects of the physical metallurgy of warm rolling [J].
Barnett, MR ;
Jonas, JJ .
ISIJ INTERNATIONAL, 1999, 39 (09) :856-873
[4]   Formation of {111}⟨110⟩ and {111}⟨112⟩ textures in cold rolled and annealed IF sheet steel [J].
Barnett, MR ;
Kestens, L .
ISIJ INTERNATIONAL, 1999, 39 (09) :923-929
[5]  
Bunge H., 1982, TEXTURE ANAL MAT SCI, P1, DOI 10.1016/B978-0-408-10642-9.50006-4
[6]   Influence of second phase particles on recrystallisation of cold-rolled low carbon microalloyed steels during isothermal annealing [J].
Capdevila, C ;
De Cock, T ;
García-Mateo, C ;
Caballero, FG ;
de Andrés, CG .
MICROALLOYING FOR NEW STEEL PROCESSES AND APPLICATIONS, 2005, 500-501 :803-810
[7]   Austenite retention in low Al/Si multiphase steels [J].
De Cock, T. ;
Ferrer, J. P. ;
Capdevila, C. ;
Caballero, F. G. ;
Lopez, V. ;
Garcia de Andres, C. .
SCRIPTA MATERIALIA, 2006, 55 (05) :441-443
[8]  
DECOOMAN BC, 2003, INT FOR PROP APPL IF, P249
[9]  
FUNU T, 1990, MAT SCI TECHNOL, V6, P1093
[10]   Comparative study of precipitation behavior and texture formation in cold rolled-batch annealed and cold rolled-continuous annealed interstitial free high strength steels [J].
Ghosh, P. ;
Bhattacharya, B. ;
Ray, R. K. .
SCRIPTA MATERIALIA, 2007, 56 (08) :657-660