Optimizing the thiosulfate leaching of gold from printed circuit boards of discarded mobile phone

被引:91
作者
Vinh Hung Ha [1 ]
Lee, Jae-chun [2 ,3 ]
Huynh, Trung Hai [1 ]
Jeong, Jinki [2 ,3 ]
Pandey, B. D. [4 ]
机构
[1] Hanoi Univ Sci & Technol, Sch Environm Sci & Technol, Hanoi, Vietnam
[2] Korea Inst Geosci & Mineral Resources, Mineral Resources Res Div, Taejon 305350, South Korea
[3] Korea Univ Sci & Technol, Taejon 305350, South Korea
[4] Natl Met Lab, CSIR, Met Extract & Forming Div, Jamshedpur 831007, Bihar, India
关键词
Gold; Thiosulfate leaching; Optimization; PCBs; E-waste; RESPONSE-SURFACE METHODOLOGY; RECOVERY; OXIDATION; METALS; COPPER; WASTE; OPTIMIZATION; SPECIATION; KINETICS; AMMONIA;
D O I
10.1016/j.hydromet.2014.07.007
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
An environmentally benign process involving thiosulfate leaching was developed in order to recover gold from the printed circuit boards (PCBs) of discarded mobile phone. The effect of concentration of the reagents such as thiosulfate, copper(II) and ammonia on the leaching of gold was investigated in the temperature range 20-50 degrees C. Parameters were optimized through modeling of the leaching process using response surface methodology (RSM) based on central composite design (CCD). The optimum conditions for leaching of gold from PCBs were identified to be 72.71 mM thiosulfate, 10.0 mM copper(II) and 0.266 M ammonia. The initial rate of gold leaching was found to be 2.395 x 10(-5) mol.m(-2).s(-1) under the optimum conditions. As regards the kinetics of gold leaching, the pseudo-second order kinetic model with chemical control was found to be applicable in the low concentration range (40-60 mM thiosulfate, 5-7 mM copper(II) and 0.22-0.247 M ammonia), compared to that of pseudo-first order kinetic model at mid concentration range of the reactants viz., 60-70 mM thiosulfate, 7-9 mM copper(II) and 0.247-0.263 M ammonia. The apparent activation energy of the reaction in the temperature range 20-50 degrees C was found to be 78.6 kJ.mol(-1). The samples were characterized before and after leaching using scanning electron microscopy (SEM) which corroborated the chemical controlled leaching mechanism. (C) 2014 Elsevier B.V. All rights reserved.
引用
收藏
页码:118 / 126
页数:9
相关论文
共 26 条
[1]   Thermodynamic analysis of gold leaching by ammoniacal thiosulfate using Eh/pH and speciation diagrams [J].
Aylmore, MG ;
Muir, DM .
MINERALS & METALLURGICAL PROCESSING, 2001, 18 (04) :221-227
[2]   MULTI-FACTOR EXPERIMENTAL-DESIGNS FOR EXPLORING RESPONSE SURFACES [J].
BOX, GEP ;
HUNTER, JS .
ANNALS OF MATHEMATICAL STATISTICS, 1957, 28 (01) :195-241
[3]   Copper catalysed oxidation of thiosulfate by oxygen in gold leach golutions [J].
Breuer, PL ;
Jeffrey, MI .
MINERALS ENGINEERING, 2003, 16 (01) :21-30
[4]   Thiosulfate leaching kinetics of gold in the presence of copper and ammonia [J].
Breuer, PL ;
Jeffrey, MI .
MINERALS ENGINEERING, 2000, 13 (10-11) :1071-1081
[5]   Application of response surface methodology for optimization of the synthesis of synthetic rutile from titania slag [J].
Chen, Guo ;
Chen, Jin ;
Srinivasakannan, C. ;
Peng, Jinhui .
APPLIED SURFACE SCIENCE, 2012, 258 (07) :3068-3073
[6]   The impact of thiosulfate oxidation products on the oxidation of gold in ammonia thiosulfate solutions [J].
Chu, CK ;
Breuer, PL ;
Jeffrey, MI .
MINERALS ENGINEERING, 2003, 16 (03) :265-271
[7]   Metallurgical recovery of metals from electronic waste: A review [J].
Cui, Jirang ;
Zhang, Lifeng .
JOURNAL OF HAZARDOUS MATERIALS, 2008, 158 (2-3) :228-256
[8]   Thiosulphate leaching of gold in the presence of ethylenediaminetetraacetic acid (EDTA) [J].
Feng, D. ;
van Deventer, J. S. J. .
MINERALS ENGINEERING, 2010, 23 (02) :143-150
[9]   Recovery of gold and silver from spent mobile phones by means of acidothiourea leaching followed by adsorption using biosorbent prepared from persimmon tannin [J].
Gurung, Manju ;
Adhikari, Birendra Babu ;
Kawakita, Hidetaka ;
Ohto, Keisuke ;
Inoue, Katsutoshi ;
Alam, Shafiq .
HYDROMETALLURGY, 2013, 133 :84-93
[10]  
Ha V.H., 2011, SCI TECHNOL TU A, V82A, P37