Improved oxidation performance of TiAl alloy by a novel Al-Si composite coating

被引:18
|
作者
Wang, Qi [1 ,3 ]
Wu, Wei-Yao [2 ]
Jiang, Mei-Yan [2 ]
Cao, Fa-He [1 ]
Wu, Hai-Xin [1 ,3 ]
Sun, Dong-Bai [1 ,3 ]
Yu, Hong-Ying [1 ]
Wu, Lian-Kui [1 ,2 ]
机构
[1] Sun Yat Sen Univ, Sch Mat, Guangzhou 510275, Peoples R China
[2] Zhejiang Univ Technol, Coll Mat Sci & Engn, Hangzhou 310014, Peoples R China
[3] Sun Yat Sen Univ, South China Sea Inst, Guangzhou 510275, Peoples R China
来源
SURFACE & COATINGS TECHNOLOGY | 2020年 / 381卷 / 381期
基金
中国国家自然科学基金;
关键词
TiAl; Magnetron sputtering; Aluminizing coating; SiO2; coating; High temperature oxidation; HIGH-TEMPERATURE OXIDATION; THERMAL BARRIER COATINGS; TITANIUM-ALLOYS; ISOTHERMAL OXIDATION; BEHAVIOR; RESISTANCE; FILM; TI-50AL; PROTECTION; ELEMENTS;
D O I
10.1016/j.surfcoat.2019.125126
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
A novel Al-Si composite coating was fabricated on gamma-TiAl by the combination of magnetron sputtered Al coating and subsequently electrodeposited SiO2 coating. The oxidation performance of the specimens was evaluated in static air at 900 degrees C. Results shown that the Al Si composite coating can act as an efficient oxygen migration barrier and provide good oxidation resistance. During the oxidation process, an Al2O3 enriched layer formed beneath the composite coating. The interfacial reaction between the composite coating and alloy resulted in the generation of Al2O3 and Ti5Si3.
引用
收藏
页数:13
相关论文
共 50 条
  • [31] Way to fabricate an Al-Si coating on the surface of a Ti alloy and its high-temperature oxidation resistance
    Key Laboratory for Automobile Materials, Department of Materials Science and Engineering, Jilin University, Changchun 130025, China
    Beijing Keji Daxue Xuebao/Journal of University of Science and Technology Beijing, 2007, 29 (02): : 157 - 161
  • [32] High temperature oxidation morphology of Al-Si coating on K438 high-temperature alloy
    Yang, Shi-Wei
    Zhang, Fan-Yun
    Li, Li
    Jiang, Shu-Li
    Harbin Gongcheng Daxue Xuebao/Journal of Harbin Engineering University, 2005, 26 (01): : 101 - 104
  • [33] Oxidation Behavior of γ-TiAl Alloy with NiCrAlY/Al Duplex Coating at 950 °C
    Xu Yi
    Miao Qiang
    Liang Wenping
    Wang Ling
    Yu Xiushui
    Jiang Qiong
    Ren Beilei
    RARE METAL MATERIALS AND ENGINEERING, 2014, 43 (06) : 1407 - 1411
  • [34] Effects of Si phase refinement on the plasma electrolytic oxidation of eutectic Al-Si alloy
    Li, Kang
    Li, Wenfang
    Zhang, Guoge
    Zhu, Wen
    Zheng, Fenghua
    Zhang, Dongqiao
    Wang, Min
    JOURNAL OF ALLOYS AND COMPOUNDS, 2019, 790 : 650 - 656
  • [35] LASER MICRO-COATING OF STAINLESS STEEL ON AN AL-SI CAST ALLOY
    Kraus, Pavel
    Hren, Iryna
    Naprstkova, Natasa
    Michna, Stefan
    Michnova, Lenka
    Aboltins, Aivars
    19TH INTERNATIONAL SCIENTIFIC CONFERENCE ENGINEERING FOR RURAL DEVELOPMENT, 2020, : 503 - 508
  • [36] Oxidation resistance of TiAl3-Al composite coating on orthorhombic Ti2AlNb based alloy
    Kong, Lingyan
    Qi, Jianzhong
    Lu, Bin
    Yang, Rui
    Cui, Xinyu
    Li, Tiefan
    Xiong, Tianying
    SURFACE & COATINGS TECHNOLOGY, 2010, 204 (14): : 2262 - 2267
  • [37] High performance tribological coatings on a secondary cast Al-Si alloy generated by Plasma Electrolytic Oxidation
    Fernandez-Lopez, P.
    Alves, S. A.
    Lopez-Ortega, A.
    San Jose-Lombera, J. T.
    Bayon, R.
    CERAMICS INTERNATIONAL, 2021, 47 (22) : 31238 - 31250
  • [38] Amorphous structure in a laser clad Ni-Cr-Al coating on Al-Si alloy
    梁工英
    苏俊义
    黄俊达
    胡仲豪
    Transactions of Nonferrous Metals Society of China, 2000, (02) : 220 - 223
  • [39] Segregation phenomena of laser alloyed Ni-Cr-Al coating on Al-Si alloy
    Liang, GY
    Li, CL
    Su, JY
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1997, 224 (1-2): : 173 - 176
  • [40] OXIDATION RESISTANCE OF TIAL IMPROVED BY A COCRAL COATING
    TANIGUCHI, S
    SHIBATA, T
    ASANUMA, N
    LUO, H
    WANG, FH
    WU, WT
    JOURNAL DE PHYSIQUE IV, 1993, 3 (C9): : 403 - 410