Moving cracks form white etching areas during rolling contact fatigue in bearings

被引:57
作者
Morsdorf, L. [1 ]
Mayweg, D. [1 ]
Li, Y. [1 ,2 ]
Diederichs, A. [3 ]
Raabe, D. [1 ]
Herbig, M. [1 ]
机构
[1] Max Planck Inst Eisenforsch GmbH, Max Planck Str 1, D-40237 Dusseldorf, Germany
[2] Ruhr Univ Bochum, ZGH, Univ Str 150, D-44780 Bochum, Germany
[3] Rhein Westfal TH Aachen, Gemeinschaftslab Elektronenmikroskopie, D-52056 Aachen, Germany
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2020年 / 771卷
关键词
White etching cracks; AISI; 52100; 100Cr6; Rolling contact fatigue; Failure mechanism; 100CR6; BEARING; MICROSTRUCTURAL CHANGES; NONMETALLIC INCLUSIONS; FORMATION MECHANISMS; FRACTURE NUCLEATION; MATTER; LAYERS; EVOLUTION; SURFACE; WEAR;
D O I
10.1016/j.msea.2019.138659
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
White etching cracks (WECs) and the associated white etching areas (WEAs) are responsible for failure of widely spread engineering applications such as bearings and railways. Although the phenomenon is known for more than 100 years, the underlying mechanisms are still a matter of debate. In this work, we thoroughly investigate a 100Cr6 wind turbine gearbox bearing after failure in service operation. Based on our findings from detailed microstructure characterization on multiple length scales we formulate a new consistent explanation for the formation of WEAs during rolling contact fatigue. We propose a mechanism of moving WECs - not only in terms of conventional crack propagation but also as a movement of the crack normal to its plane. During cyclic loading the crack continuously changes its position and leaves behind a severely plastically deformed area consisting of ferritic nano-grains, i.e. the WEAs. The atomic-scale delocalization of the crack plane in a single loading cycle adds up to micron-sized WEAs during repetitive loading/unloading. After the initial formation of a fatigue crack around inclusions, crack face rubbing occurs during compressive loading cycles. This leads to the formation of WEA by local severe plastic deformation. It also leads to partial cohesion of the abutting crack faces and material transport between them. As a result, the WEC opens at a slightly shifted position with respect to its former location during unloading.
引用
收藏
页数:13
相关论文
共 56 条
[1]  
[Anonymous], MATERIALS
[2]  
[Anonymous], ASME J TRIBOL
[3]  
[Anonymous], 1912, J W SCOTT IRON STEEL
[4]  
[Anonymous], ANTR K AACH
[5]  
[Anonymous], 14 EUR WORKSH MOD DE
[6]  
BAY N, 1983, WELD J, V62, pS137
[7]   Critical Assessment 13: Elimination of white etching matter in bearing steels [J].
Bhadeshia, H. K. D. H. ;
Solano-Alvarez, W. .
MATERIALS SCIENCE AND TECHNOLOGY, 2015, 31 (09) :1011-1015
[8]   Multiscale characterization of White Etching Cracks (WEC) in a 100Cr6 bearing from a thrust bearing test rig [J].
Danielsen, H. K. ;
Guzman, F. Gutierrez ;
Dahl, K. V. ;
Li, Y. J. ;
Wu, J. ;
Jacobs, G. ;
Burghardt, G. ;
Faester, S. ;
Alimadadi, H. ;
Goto, S. ;
Raabe, D. ;
Petrov, R. .
WEAR, 2017, 370 :73-82
[9]   Electron microscopy analysis of structural changes within white etching areas [J].
Diederichs, A. M. ;
Schwedt, A. ;
Mayer, J. ;
Dreifert, T. .
MATERIALS SCIENCE AND TECHNOLOGY, 2016, 32 (16) :1683-1693
[10]   An updated review: white etching cracks (WECs) and axial cracks in wind turbine gearbox bearings [J].
Evans, M. -H. .
MATERIALS SCIENCE AND TECHNOLOGY, 2016, 32 (11) :1133-1169