Hydrogen and helium trapping in tungsten under simultaneous irradiations

被引:109
|
作者
Lee, H. T.
Haasz, A. A.
Davis, J. W.
Macaulay-Newcombe, R. G.
Whyte, D. G.
Wright, G. M.
机构
[1] Univ Toronto, Inst Aerosp Studies, Toronto, ON M3H 5T6, Canada
[2] Univ Wisconsin, Madison, WI 53706 USA
基金
加拿大自然科学与工程研究理事会;
关键词
tungsten; deuterium inventory; helium; thermal desorption; ion-surface interactions;
D O I
10.1016/j.jnucmat.2007.01.111
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Hydrogen and helium trapping in polycrystalline tungsten under simultaneous He+-H+ and He+-D+ irradiation was measured by thermal desorption spectroscopy. At 300 K: He retention and release are affected very little by the presence of H, closely following He+-only irradiations; He is trapped within similar to 30 nm of the surface. D retention is similar to D+-only levels but the presence of He enhances D trapping in the near surface, while limiting D diffusion into the bulk; D is trapped within similar to 30-35 nm of the surface possibly at interstitial sites surrounding He-vacancy defects. At 700 K: He retention and release are again similar to He+-only cases; He is trapped within similar to 30 nm of the surface while no D is observed. (c) 2007 Elsevier B.V. All rights reserved.
引用
收藏
页码:898 / 903
页数:6
相关论文
共 50 条
  • [41] Effect of hydrogen pre-implantation on formation and growth of bubbles in tungsten under helium ion irradiation
    Luo, Fengfeng
    Wang, Jiawei
    Zhang, Linwei
    Guo, Liping
    Zhang, Weiping
    Shen, Zhenyu
    Wang, Chunlan
    NUCLEAR INSTRUMENTS & METHODS IN PHYSICS RESEARCH SECTION B-BEAM INTERACTIONS WITH MATERIALS AND ATOMS, 2019, 450 : 224 - 228
  • [42] Hydrogen trapping energetics at BCC iron-helium interfaces
    Bergstrom, Z. J.
    Yang, L.
    Wirth, B. D.
    JOURNAL OF NUCLEAR MATERIALS, 2022, 572
  • [43] Study of hydrogen isotopes behavior in tungsten by a multi trapping macroscopic rate equation model
    Hodille, E. A.
    Ferro, Y.
    Fernandez, N.
    Becquart, C. S.
    Angot, T.
    Layet, J. M.
    Bisson, R.
    Grisolia, C.
    PHYSICA SCRIPTA, 2016, T167
  • [44] Cavity formation in a SiC/SiC composite under simultaneous irradiation of hydrogen, helium and silicon ions
    Miwa, S
    Hasegawa, A
    Taguchi, T
    Igawa, N
    Abe, K
    MATERIALS TRANSACTIONS, 2005, 46 (03) : 536 - 542
  • [45] Stress-induced hydrogen self-trapping in tungsten
    Smirnov, R. D.
    Krasheninnikov, S. I.
    NUCLEAR FUSION, 2018, 58 (12)
  • [46] Hydrogen bubble formation and evolution in tungsten under different hydrogen irradiation conditions
    Hu, Wenhui
    Luo, Fengfeng
    Shen, Zhenyu
    Guo, Liping
    Zheng, Zhongcheng
    Wen, Yongming
    Ren, Yaoyao
    FUSION ENGINEERING AND DESIGN, 2015, 90 : 23 - 28
  • [47] Effect of surface quality on hydrogen/helium irradiation behavior in tungsten
    Chen, Hongyu
    Xu, Qiu
    Wang, Jiahuan
    Li, Peng
    Yuan, Julong
    Lyu, Binghai
    Wang, Jinhu
    Tokunaga, Kazutoshi
    Yao, Gang
    Luo, Laima
    Wu, Yucheng
    NUCLEAR ENGINEERING AND TECHNOLOGY, 2022, 54 (06) : 1947 - 1953
  • [48] Synergistic influence of dislocations and helium cluster on hydrogen atom in tungsten
    Xu, Bai-Chuan
    Li, Ya-Wen
    Mai, Yilang
    Li, Ziqi
    Wu, Wei
    Li, Xiao-Chun
    Pan, Xin-Dong
    Sun, Fei
    Zhou, Hai-Shan
    Luo, Guang-Nan
    JOURNAL OF NUCLEAR MATERIALS, 2024, 596
  • [49] Ion beam analysis of helium and its irradiation effect on hydrogen trapping in W single crystals
    Nagata, S
    Tsuchiya, B
    Sugawara, T
    Ohtsu, N
    Shikama, T
    NUCLEAR INSTRUMENTS & METHODS IN PHYSICS RESEARCH SECTION B-BEAM INTERACTIONS WITH MATERIALS AND ATOMS, 2002, 190 : 652 - 656
  • [50] Synergistic effects by simultaneous bombardment of tungsten with hydrogen and carbon
    Krieger, K
    Roth, J
    JOURNAL OF NUCLEAR MATERIALS, 2001, 290 : 107 - 111