Tribological performance of laser peened Ti-6Al-4V

被引:79
作者
Kumar, Dharmesh [1 ]
Akhtar, Syed Nadeem [2 ]
Patel, Anup Kumar [3 ]
Ramkumar, J. [2 ]
Balani, Kantesh [3 ]
机构
[1] Indian Inst Technol, Mat Sci Programme, Kanpur 208016, Uttar Pradesh, India
[2] Indian Inst Technol, Kanpur 208016, Uttar Pradesh, India
[3] Indian Inst Technol, Kanpur 208016, Uttar Pradesh, India
关键词
Fretting; Other materials (Ti-6Al-4V); Laser processing; Profilometry; Residual stress; Stick-slip; ALLOYS; ABLATION;
D O I
10.1016/j.wear.2014.11.016
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
Ti-6Al-4V is a well-known metallic biomaterial used for implants, but its use is limited by its inferior hardness and tribological resistance in vivo. Laser peening (LP) is one potential means to enhance its tribological properties. LP induces surface residual compressive stresses due to plastic deformation caused by the propagation of a shock wave. Further, performing laser peening under water can enhance a material's hardness and wear resistance because it confines shock waves to the surface of the material. In the current research, the influence of an excimer laser (Kr-F, 248 nm) with varying fluence on the fretting behavior of Ti-6Al-4V was carried out. An optimized laser fluence of 100 J/cm(2) resulted in an increase in hardness by 28% in air and 35% in water confining media, respectively, when compared to that of an untreated Ti-6Al-4V substrate. It was observed that the residual compressive stresses from LP increased from 540 MPa in air to 604 MPa in water. Fretting wear against bearing steel type AISI E52100 shows a major wear reduction on LP Ti-6Al-4V samples as wear volume decreased from 1.211 x 10(-3) mm(3) to either 0.139 x 10(-3) mm(3) or to 0.106 x 10(-3) mm(3) in samples peened in air and water, respectively. Frictional hysteresis data show that the dissipation energy loss for Ti-6Al-4V substrate from 11.412 x 10(-4) J is decreased to 3.284 x 10(-4) J for LP sample at 20 N load. Moreover, a considerable fall in contact diameter is observed from the non-processed surface (0.29 x 10(-3) mu m) to the LP sample (0.176 x 10(-3) mu m). Friction log plots indicate that wear mechanisms are mostly adhesion, abrasion and delamination. Enhanced tribological performance of LP Ti-6Al-4V was observed using LP in a water medium, and indicates potential improvements when the alloy is used in joint replacements. (C) 2014 Elsevier B.V. All rights reserved.
引用
收藏
页码:203 / 217
页数:15
相关论文
共 50 条
[41]   Effect of impact angle on hot corrosion resistance of abrasive water jet peened Ti-6Al-4V alloy [J].
Chakkravarthy, V. ;
Manojkumar, P. ;
Jerome, S. ;
Evlashin, S. A. ;
Narayanan, Jinoop Arackal ;
Mendagaliev, R. V. ;
Sidorenko, A. O. ;
Narayan, R. L. .
SURFACE & COATINGS TECHNOLOGY, 2024, 494
[42]   Investigation of tribological and metallurgical effects on Ti-6Al-4V laminates made by LSEM for Ti/GFRP stacked composite [J].
Kumar, Pushpinder ;
Joshi, Ravinder Singh ;
Singla, Rohit Kumar .
WEAR, 2023, 524
[43]   Crack analysis in Ti-6Al-4V alloy produced by selective laser melting [J].
Hui-Yan Zhang ;
Yan-Hui Liu ;
Zhi-Wei Li ;
An-Hui Xiong ;
Ke Li ;
Jia-Yun Fu .
Tungsten, 2021, 3 (03) :361-367
[44]   Crack analysis in Ti-6Al-4V alloy produced by selective laser melting [J].
Hui-Yan Zhang ;
Yan-Hui Liu ;
Zhi-Wei Li ;
An-Hui Xiong ;
Ke Li ;
Jia-Yun Fu .
Tungsten, 2021, 3 :361-367
[45]   Tool life and wear mechanisms in laser assisted milling Ti-6Al-4V [J].
Bermingham, M. J. ;
Sim, W. M. ;
Kent, D. ;
Gardiner, S. ;
Dargusch, M. S. .
WEAR, 2015, 322 :151-163
[46]   Effect of Substrate Thickness and Preheating on the Distortion of Laser Deposited Ti-6Al-4V [J].
Corbin, David J. ;
Nassar, Abdalla R. ;
Reutzel, Edward W. ;
Beese, Allison M. ;
Michaleris, Pan .
JOURNAL OF MANUFACTURING SCIENCE AND ENGINEERING-TRANSACTIONS OF THE ASME, 2018, 140 (06)
[47]   Laser diffusion nitriding of Ti-6Al-4V for improving hardness and wear resistance [J].
Man, H. C. ;
Bai, M. ;
Cheng, F. T. .
APPLIED SURFACE SCIENCE, 2011, 258 (01) :436-441
[48]   Microstructure characterization of Ti-6Al-4V titanium laser weld and its deformation [J].
Xu Pei-quan .
TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2012, 22 (09) :2118-2123
[49]   Improvement of fatigue life of Ti-6Al-4V alloy by laser shock peening [J].
Zhang, X. C. ;
Zhang, Y. K. ;
Lu, J. Z. ;
Xuan, F. Z. ;
Wang, Z. D. ;
Tu, S. T. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2010, 527 (15) :3411-3415
[50]   Wetting and Spreading of AgCuTi on Selective Laser-Melted Ti-6Al-4V [J].
Hao, Lujing ;
Liu, Jiankun ;
Li, Yulong .
MATERIALS, 2021, 14 (17)