Effect of oxygen inhibition on composite repair strength over time

被引:56
作者
Dall'Oca, Susanna
Papacchini, Federica
Goracci, Cecilia
Cury, Alvaro H.
Suh, Byoung I.
Tay, Franklin R.
Polimeni, Antonella
Ferrari, Marco
机构
[1] Univ Siena, Dept Dent Mat, Policlin Le Scotte, I-53100 Siena, Italy
[2] Bisco Inc, Schaumburg, IL USA
[3] Med Coll Georgia, Sch Dent, Dept Oral Biol & Maxillofacial Pathol, Augusta, GA 30912 USA
[4] Univ Roma La Sapienza, Dept Pediat Dent, Rome, Italy
关键词
light-cured resin composite; composite repair; oxygen-inhibited layer; time; microtensile bond strength;
D O I
10.1002/jbm.b.30689
中图分类号
R318 [生物医学工程];
学科分类号
0831 ;
摘要
The study was aimed at examining whether an oxygen inhibition layer is required for bonding a repairing to a pre-existing composite, and to determine the time required for free radicals within a composite substrate to decay to the extent that the composite repair strength drops significantly. Ten slabs of Gradia Direct Anterior (GC Corp.) were divided into (1) control group: an interfacial oxygen inhibition layer was created by applying and light-curing two layers of bonding resin (D/E Resin, Bisco) to the slabs surface in atmospheric air; (2) experimental group: the absence of an interfacial oxygen inhibition layer was obtained by light-curing the second bonding resin layer in a nitrogen atmosphere. After I and 2 h, 1, 14, and 30 days of air storage, a composite repair was layered over the bonding resin. Microtensile bond strengths were measured and statistically analyzed. The curing atmosphere was not a significant factor for bond strength (p = 0.82), and time and curing atmosphere-time interaction were significant (p < 0.001). The 30 day-strengths were the lowest (P < 0.05). An oxygen-inhibited layer is not initially required for bonding to resin composite, and it takes more than 14 days before the bond strength between a pre-existing and a fresh composite drops. (C) 2006 Wiley Periodicals, Inc.
引用
收藏
页码:493 / 498
页数:6
相关论文
共 28 条
[21]  
2-L
[22]  
Pashley D H, 1999, J Adhes Dent, V1, P299
[23]  
Perdigao Jorge, 2002, J Esthet Restor Dent, V14, P31, DOI 10.1111/j.1708-8240.2002.tb00145.x
[24]   THE EFFECT OF OXYGEN INHIBITION ON AN UNFILLED FILLED COMPOSITE SYSTEM [J].
RUEGGEBERG, FA ;
MARGESON, DH .
JOURNAL OF DENTAL RESEARCH, 1990, 69 (10) :1652-1658
[25]  
Suh Byoung In, 2004, J Esthet Restor Dent, V16, P316, DOI 10.1111/j.1708-8240.2004.tb00060.x
[26]  
SUN BJ, 2003, J DENT RES, V82
[27]   Interfacial layer characterization in dental composite [J].
Truffier-Boutry, D ;
Place, E ;
Devaux, J ;
Leloup, G .
JOURNAL OF ORAL REHABILITATION, 2003, 30 (01) :74-77
[28]   Effect of resin hydrophilicity and water storage on resin strength [J].
Yiu, CKY ;
King, NM ;
Pashley, DH ;
Suh, BI ;
Carvalho, RM ;
Carrilho, MRO ;
Tay, FR .
BIOMATERIALS, 2004, 25 (26) :5789-5796