摘要
Zirconium diboride (ZrB2) based ultra-high temperature ceramics either unmodified or with SiC particulate additions of 10, 20, or 30 volume percent were prepared by conventional hot pressing. The ZrB2-SiC compositions had improved four-point bend strength compared to the ZrB2 prepared in our laboratory as well as other reported ZrB2 or ZrB2-SiC materials. Strength and toughness increased as the amount of SiC increased. Measured strengths ranged from similar to550 MPa for ZrB2 to over 1000 MPa for ZrB2-30% SiC. Likewise, toughness increased from 3.5 MPa to more than 5 MPa over the same composition range. The addition of SiC also improved oxidation resistance compared to pure ZrB2. Co-extrusion processing was used to produce ZrB2-based ultra-high temperature ceramics with a fibrous monolithic structure. Samples had dense ZrB2-30 vol% SiC cells approximately 100 Am in diameter surrounded by porous ZrB2 cell boundaries approximately 20 mum thick. ZrB2-based fibrous monoliths had four point bend strength of similar to450 MPa, about half of a conventional ZrB2-SiC ceramic with the cell composition. Preliminary analysis of fracture behavior found that ZrB2-based fibrous monoliths did not exhibit graceful failure because the difference in strength between the cell and cell boundary of the current materials was not sufficient. (C) 2004 Kluwer Academic Publishers.
引用
收藏
页码:5951 / 5957
页数:7
相关论文
共 19 条
[1]  
[Anonymous], 1994, Phase Equilibria Diagrams-Phase Diagrams for Ceramists
[2]  
*ASTM, C28 ASTM
[3]   Crack deflection in ceramic laminates using porous interlayers [J].
Blanks, KS ;
Kristoffersson, A ;
Carlström, E ;
Clegg, WJ .
JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 1998, 18 (13) :1945-1951
[4]   High-strength zirconium diboride-based ceramics [J].
Chamberlain, AL ;
Fahrenholtz, WG ;
Hilmas, GE ;
Ellerby, DT .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2004, 87 (06) :1170-1172
[5]  
Clougherty EV, 1970, RES DEV REFRACTORY 2
[6]  
CUTLER RA, 1991, CERAMICS GLASSES, P787
[7]   Boron carbide-zirconium boride in situ composites by the reactive pressureless sintering of boron carbide-zirconia mixtures [J].
Goldstein, A ;
Geffen, Y ;
Goldenberg, A .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2001, 84 (03) :642-644
[8]  
HILMAS GE, 1994, CERAMIC T, V51, P609
[9]  
KAJI N, 1992, TAIKABUTSU OVERSEAS, V44, P387
[10]   Effect of Fe and Cr addition on the sintering behavior of ZrB2 produced by self-propagating high-temperature synthesis [J].
Mishra, SK ;
Das, SK ;
Ray, AK ;
Ramachandrarao, P .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2002, 85 (11) :2846-2848